# US 2015/0104376 A1 · Method of annealing sapphire

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0104376 A1
- Document ID: US20150104376A1
- Status: Published application
- Kind: A1
- Application number: 14/489,924
- Filed: 2014-09-18
- Published: 2015-04-16
- Earliest claimed: 2013-10-16
- Applicants: GT Crystal Systems, LLC
- Inventors: Scott J. Turchetti; Daniela M. Fredrick
- Web page: https://patentgrep.com/patent/US20150104376A1

## CPC

- H05K 5/03: Covers
- C30B 29/20: Aluminium oxides
- C30B 33/02: Heat treatment (C30B33/04, C30B33/06 take precedence)
- H04M 1/0266: {for a display module assembly}
- H04M 1/185: {Improving the shock resistance of the housing, e.g. by increasing the rigidity}
- H05K: PRINTED CIRCUITS; CASINGS OR CONSTRUCTIONAL DETAILS OF ELECTRIC APPARATUS; MANUFACTURE OF ASSEMBLAGES OF ELECTRICAL COMPONENTS
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR
- H04M: TELEPHONIC COMMUNICATION (circuits for controlling other apparatus via a telephone cable and not involving telephone switching apparatus G08)

## Abstract

A method of annealing at least one sapphire lamina is disclosed. The method comprises at least two different heating steps and produces an annealed sapphire lamina having improved optical properties that can be used for fabricating a cover plate of an electronic device. The cover plate and electronic device comprising the annealed sapphire lamina are also disclosed.

## Claims

### Claim 1

A method of producing a cover plate of an electronic device comprising the steps of:
i) providing at least one sapphire lamina;
ii) heating the sapphire lamina at a first temperature and under vacuum at a first pressure;
iii) heating the sapphire lamina at a second temperature and in an inert gas at a second pressure, wherein the second temperature is greater than the first temperature and the second pressure is greater than the first pressure;
iv) cooling the sapphire lamina to room temperature to produce an annealed sapphire lamina; and
v) fabricating the cover plate comprising the annealed sapphire lamina.

### Claim 2 (depends on 1)

The method of claim 1, wherein the sapphire lamina has a thickness of from about 0.1 mm to about 2 mm.

### Claim 3 (depends on 2)

The method of claim 2, wherein the thickness of the sapphire lamina is from about 0.2 mm to about 1 mm.

### Claim 4 (depends on 1)

The method of claim 1, wherein the first temperature is from about 900°C. to about 2000°C.

### Claim 5 (depends on 1)

The method of claim 1, wherein the first temperature is from about 1400° C. to about 1800°C.

### Claim 6 (depends on 1)

The method of claim 1, wherein the first temperature is from about 1500° C. to about 1700°C.

### Claim 7 (depends on 1)

The method of claim 1, wherein the second temperature is from about 1000° C. to about 2050° C.

### Claim 8 (depends on 1)

The method of claim 1, wherein the second temperature is from about 1500° C. to about 2000°C.

### Claim 9 (depends on 1)

The method of claim 1, wherein the second temperature is from about 1600° C. to about 1800°C.

### Claim 10 (depends on 1)

The method of claim 1, wherein the first pressure is less than about 1 torr.

### Claim 11 (depends on 1)

The method of claim 1, wherein the first pressure is from about 10−1 torr to about 10−7 torr.

### Claim 12 (depends on 1)

The method of claim 1, wherein the second pressure is between the first pressure and atmospheric pressure.

### Claim 13 (depends on 1)

The method of claim 1, wherein the second pressure is atmospheric pressure.

### Claim 14 (depends on 1)

The method of claim 1, wherein the inert gas comprises argon or helium.

### Claim 15 (depends on 14)

The method of claim 14, wherein the inert gas is argon.

### Claim 16 (depends on 1)

The method of claim 1, wherein the sapphire lamina is heated at the first temperature and under vacuum at the first pressure and subsequently heated at the second temperature and in the gaseous atmosphere at the second pressure.

### Claim 17 (depends on 1)

The method of claim 1, wherein the sapphire lamina is heated at the first temperature and under vacuum at the first pressure, cooled to a temperature below the first temperature, and subsequently heated at the second temperature and in the gaseous atmosphere at the second pressure.

### Claim 18 (depends on 17)

The method of claim 17, wherein the sapphire lamina is cooled to room temperature.

### Claim 19 (depends on 1)

The method of claim 1, wherein the method further comprises the step of heating the sapphire lamina at a third temperature and in a gaseous atmosphere comprising hydrogen at a third pressure, wherein the third temperature is below the second temperature and the third pressure is above the first pressure.

### Claim 20 (depends on 19)

The method of claim 19, wherein the hydrogen comprises water.

### Claim 21 (depends on 19)

The method of claim 19, wherein the gaseous atmosphere comprises hydrogen and an inert gas.

### Claim 22 (depends on 19)

The method of claim 19, wherein the sapphire lamina is heated in the gaseous atmosphere comprising hydrogen prior to the step of heating the sapphire lamina at the second temperature and in the inert gas at the second pressure.

### Claim 23 (depends on 19)

The method of claim 19, wherein the sapphire lamina is heated in the gaseous atmosphere comprising hydrogen prior to the step of heating the sapphire lamina at the first temperature and under vacuum at the first pressure.

### Claim 24 (depends on 1)

The method of claim 1, wherein the sapphire lamina is provided in an annealing furnace.

### Claim 25 (depends on 1)

The method of claim 1, wherein a plurality of sapphire lamina are provided.

### Claim 26 (depends on 1)

The method of claim 1, wherein the cover plate is the sapphire lamina.

### Claim 27 (depends on 1)

The method of claim 1, wherein the cover plate is two or more layers, and the sapphire lamina is an exterior layer of the cover plate.

### Claim 28 (depends on 27)

The method of claim 27, wherein the cover plate further comprises a transparent layer affixed to the sapphire layer.

### Claim 29 (depends on 28)

The method of claim 28, wherein the transparent layer has a front surface, and wherein the sapphire layer is affixed to the front surface.

### Claim 30 (depends on 29)

The method of claim 29, wherein the subsurface layer comprises glass.

### Claim 31 (depends on 29)

The method of claim 29, wherein the subsurface layer comprises a polymeric material.

### Claim 32 (depends on 1)

The method of claim 1, wherein the electronic device comprises at least one display element having a display surface and wherein the cover plate is affixed to the display surface.

### Claim 33 (depends on 1)

The method of claim 1, wherein the electronic device comprises at least one display element having a display surface and wherein the cover plate is a protective layer removably positioned on top of the display surface.

### Claim 34 (depends on 1)

The method of claim 1, wherein the electronic device is an electronic media player, a mobile telephone, a personal data assistant, a pager, a tablet, a laptop computer, or an electronic notebook

### Claim 35

A cover plate for an electronic device prepared by a method comprising the steps of:
i) providing at least one sapphire lamina;
ii) heating the sapphire lamina at a first temperature and under vacuum at a first pressure;
iii) heating the sapphire lamina at a second temperature and in an inert gaseous atmosphere at a second pressure, wherein the second temperature is greater than the first temperature and the second pressure is greater than the first pressure;
iv) cooling the sapphire lamina to room temperature to produce an annealed sapphire lamina; and
v) fabricating the cover plate comprising the annealed sapphire lamina.

### Claim 36

An electronic device comprising a cover plate prepared by a method comprising the steps of:
i) providing at least one sapphire lamina;
ii) heating the sapphire lamina at a first temperature and under vacuum at a first pressure;
iii) heating the sapphire lamina at a second temperature and in an inert gaseous atmosphere at a second pressure, wherein the second temperature is greater than the first temperature and the second pressure is greater than the first pressure;
iv) cooling the sapphire lamina to room temperature to produce an annealed sapphire lamina; and
v) fabricating the cover plate comprising the annealed sapphire lamina.