# US 2015/0104372 A1 · Single-Step, Solvent-Free, Catalyst-Free Preparation of Holey Carbon Allotropes

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0104372 A1
- Document ID: US20150104372A1
- Status: Published application
- Kind: A1
- Application number: 14/513,813
- Filed: 2014-10-14
- Published: 2015-04-16
- Earliest claimed: 2013-10-11
- Assignees: The United States of America as represented by the Administrator of the National Aeronautics and Space Administration
- Applicants: U.S.A. as represented by the Administrator of the National Aeronautics and Space Administration
- Inventors: Yi Lin; Jae-Woo Kim; John W. Connell; Michael R. Funk; Caroline J. Campbell
- Web page: https://patentgrep.com/patent/US20150104372A1

## CPC

- C01B 32/168: After-treatment
- C01B 32/156: After-treatment
- C01B 32/194: After-treatment
- C01B 32/21: After-treatment
- C01B 32/225: Expansion; Exfoliation
- C01P 2006/16: Pore diameter
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS

## Abstract

Methods for forming holey carbon allotropes and graphene nanomeshes are provided by the various embodiments. The various embodiments may be applicable to a variety of carbon allotropes, such as graphene, graphene oxide, reduced graphene oxide, thermal exfoliated graphene, graphene nanoribbons, graphite, exfoliated graphite, expanded graphite, carbon nanotubes (e.g., single-walled carbon nanotubes, double-walled carbon nanotubes, few-walled carbon nanotubes, multi-walled carbon nanotubes, etc.), carbon nanofibers, carbon fibers, carbon black, amorphous carbon, fullerenes, etc. The methods may produce holey carbon allotropes without the use of solvents, catalysts, flammable gas, additional chemical agents, or electrolysis to produce the pores (e.g., holes, etc.) in the carbon allotropes. In an embodiment, a carbon allotrope may be heated at a working window temperature for a working period of time to create holes in the carbon allotrope.

## Claims

### Claim 1

A method of forming a holey carbon allotrope, comprising:
providing a carbon allotrope; and
heating the provided carbon allotrope at a working window temperature for a working period of time to create pores in the provided carbon allotrope.

### Claim 2 (depends on 1)

The method of claim 1, wherein:
the working window temperature is from about 100° C. to about 800° C.; and
the working period of time is from about 1 minute to about 24 hours.

### Claim 3 (depends on 2)

The method of claim 2, wherein the created pores have a radius size of about 1 nanometer to about 100 nanometers.

### Claim 4 (depends on 3)

The method of claim 3, wherein heating the provided carbon allotrope at the working window temperature for the working period of time to create pores in the provided carbon allotrope is performed without the addition of solvents, catalysts, flammable gasses, additional chemical agents, or electrolysis.

### Claim 5 (depends on 4)

The method of claim 4, wherein heating the provided carbon allotrope is performed by thermal heating, mechanical heating, microwave heating, infrared heating, laser beam heating, mechanochemical heating, electrochemical heating, electron bombardment, ion bombardment, electromagnetic heating, or any combination of the foregoing.

### Claim 6 (depends on 4)

The method of claim 4, wherein the working window temperature is from about 150° C. to about 500° C.

### Claim 7 (depends on 6)

The method of claim 6, wherein the working window temperature is from about 300° C. to about 500° C.

### Claim 8 (depends on 4)

The method of claim 4, wherein:
the working window temperature is about 400° C. or more; and
the working period of time is about 1 hour.

### Claim 9 (depends on 8)

The method of claim 8, wherein the working window temperature is about 450° C.

### Claim 10 (depends on 4)

The method of claim 4, wherein:
the working window temperature is about 400° C. or more; and
the working period of time is about 3 hours.

### Claim 11 (depends on 10)

The method of claim 10, wherein the working window temperature is about 450° C.

### Claim 12 (depends on 4)

The method of claim 4, wherein:
the working window temperature is about 350° C. or more; and
the working period of time is about 10 hours.

### Claim 13 (depends on 12)

The method of claim 12, wherein the working window temperature is about 400° C.

### Claim 14 (depends on 4)

The method of claim 4, wherein:
the working window temperature is about 500° C. or more; and
the working period of time is about 20 minutes.

### Claim 15 (depends on 14)

The method of claim 14, wherein the working window temperature is about 500° C.

### Claim 16 (depends on 4)

The method of claim 4, wherein the provided carbon allotrope is at least one selected from the group consisting of graphene, graphene oxide, reduced graphene oxide, thermal exfoliated graphene, graphene nanoribbons, graphite, exfoliated graphite, expanded graphite, single-walled carbon nanotubes, double-walled carbon nanotubes, few-walled carbon nanotubes, multi-walled carbon nanotubes, carbon nanofibers, carbon fibers, carbon black, amorphous carbon, and fullerenes.

### Claim 17 (depends on 4)

The method of claim 4, wherein a form of the provided carbon allotrope is at least one selected from the group consisting of a sheet, a mat, a roving, a yarn, a thread, and a filament.

### Claim 18 (depends on 17)

The method of claim 17, wherein constituents of the form of the provided carbon allotrope are at least partially aligned in a same direction.

### Claim 19 (depends on 4)

A holey carbon allotrope formed by the method of claim 4.

### Claim 20 (depends on 17)

An electrode formed from the holey carbon allotrope of claim 17.