# US 2015/0104369 A1 · Polysilicon transportation device and a reactor system and method of polycrystalline silicon production therewith

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0104369 A1
- Document ID: US20150104369A1
- Status: Published application
- Kind: A1
- Application number: 14/052,559
- Filed: 2013-10-11
- Published: 2015-04-16
- Earliest claimed: 2013-10-11
- Applicants: REC Silicon Inc
- Inventors: Robert J. Geertsen
- Web page: https://patentgrep.com/patent/US20150104369A1

## CPC

- C01B 33/027: by decomposition or reduction of gaseous or vaporised silicon compounds other than silica or silica-containing material
- Y10T 137/0318: Processes
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

A method and system for reduction or mitigation of metal contamination of polycrystalline silicon are disclosed. A conveyance device comprising a flexible synthetic resin tube having an inner surface at least partially coated with an inner layer comprising elastomeric microcellular polyurethane is disclosed for use in fluidized bed reactor operations associated with manufacture and product handling procedures for ultra pure granular polysilicon. Use of the conduit to effect passage of the polysilicon mitigates foreign metal contact contamination from sources otherwise typically present in such manufacturing units.

## Claims

### Claim 1

A method of reducing or eliminating metal contact contamination of granular silicon during its conveyance or transportation, the method comprising:
conveying granular silicon through a conduit comprising a synthetic resin tube having an inner surface at least partially coated with a protective layer comprising a microcellular elastomeric polyurethane.

### Claim 2 (depends on 1)

The method of claim 1 wherein the synthetic resin tube is a flexible tube.

### Claim 3 (depends on 1)

The method of claim 1 wherein the microcellular elastomeric polyurethane has a bulk density of at least 800 kg/m3 and a Shore Hardness of at least 65 A.

### Claim 4 (depends on 3)

The method of claim 3 wherein the microcellular elastomeric polyurethane has a Shore Hardness of from 65 A to 85 A and a bulk density of from 800 to 1150 kg/m3.

### Claim 5 (depends on 1)

The method of claim 1 wherein the protective layer has an average thickness of at least 0.1 millimetres and up to 10 millimetres.

### Claim 6 (depends on 2)

The method of claim 2 wherein the flexible tube further comprises an outer layer comprising a soft synthetic resin united with the protective layer, and a reinforcement member buried in or attached to the outer layer.

### Claim 7 (depends on 6)

The method of claim 6 wherein the microcellular elastomeric polyurethane of the protective layer has a Shore Hardness of at least 65 A, the outer protective layer comprises a soft vinyl chloride resin, and the reinforcement member is a helically wound reinforcement member that comprises a hard synthetic resin.

### Claim 8 (depends on 1)

The method of claim 1 wherein the synthetic resin tube is a component associated with a fluidized bed reactor installation for granular polysilicon production, but excluding a fluidized reactor bed chamber of the fluidized bed reactor installation.

### Claim 9

A fluidized bed reactor unit for production of polycrystalline silicon, comprising:
a vessel defining a reactor chamber; and
at least one flexible synthetic resin tube, external to the reactor chamber, having an inner surface that defines a passageway that is in communication with the reactor chamber, the inner surface being at least partially coated with a protective layer comprising a microcellular elastomeric polyurethane.

### Claim 10 (depends on 9)

The fluidized bed reactor unit of claim 9 wherein the microcellular elastomeric polyurethane has a bulk density of at least 800 kg/m3 and a Shore Hardness of at least 65 A.

### Claim 11 (depends on 10)

The fluidized bed reactor unit of claim 10 wherein the protective layer has an average thickness of at least 0.1 millimetres and up to 10 millimetres.

### Claim 12 (depends on 9)

The fluidized bed reactor unit of claim 9 wherein the flexible tube further comprises an outer layer comprising a soft synthetic resin united with the protective layer, and a reinforcement member buried in or attached to the outer layer.

### Claim 13 (depends on 12)

The method of claim 12 wherein the microcellular elastomeric polyurethane of the protective layer has a Shore Hardness of at least 65 A, the outer layer comprises a soft vinyl chloride resin, and the reinforcement member is a helically wound reinforcement member that comprises a hard synthetic resin.

### Claim 14

A process for the production of granular polycrystalline silicon, comprising:
effecting pyrolysis of a silicon-containing gas using a fluidized bed reactor comprising a feed or discharge conduit comprising a flexible synthetic resin tube having an inner surface at least partially coated with a protective layer comprising a microcellular elastomeric polyurethane;
depositing a polycrystalline silicon layer on a seed particle in the fluidized bed reactor to produce granulate polycrystalline silicon; and
transporting the seed particle prior to entry, transporting granulate polycrystalline silicon after exit from the fluidized bed reactor, or both via the feed or discharge conduit in which the flexible tube inhibits or eliminates metal contact surface contamination of the seed particle, the polycrystalline silicon particle, or both.

### Claim 15 (depends on 14)

The process of claim 14 wherein the microcellular elastomeric polyurethane has a bulk density of at least 800 kg/m3 and a Shore Hardness of at least 65 A.

### Claim 16 (depends on 14)

The process of claim 14 wherein the flexible tube further comprises an outer layer comprising a soft synthetic resin united with the protective layer, and a reinforcement member buried in or attached to the outer layer.

### Claim 17 (depends on 16)

The process of claim 16 wherein the microcellular elastomeric polyurethane of the protective layer has a Shore Hardness of at least 65 A, the outer protective layer comprises a soft vinyl chloride resin, and the reinforcement member is a helically wound reinforcement member that comprises a hard synthetic resin.