# US 2015/0103639 A1 · Coating of surfaces intended for horology by using catanionic compositions containing phosphonic molecules and amines

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0103639 A1
- Document ID: US20150103639A1
- Status: Published application
- Kind: A1
- Application number: 14/399,616
- Filed: 2013-05-07
- Published: 2015-04-16
- Earliest claimed: 2012-05-10
- Assignees: Association Suisse Pour La Recherche Horlogere
- Applicants: Association Suisse pour la Recherche Horlogere
- Inventors: David Portet; Gregory Le Collinet
- Web page: https://patentgrep.com/patent/US20150103639A1

## CPC

- G04B 37/22: Materials or processes of manufacturing pocket watch or wrist watch cases {(machines or tools for the manufacture of clockwork cases G04D3/0064, G04D3/0097, G04D3/029; decoration or tools therefor G04B45/0076)}
- B05D 1/185: {applying monomolecular layers (B05D1/204 takes precedence)}
- B05D 1/34: Applying different liquids or other fluent materials simultaneously
- B05D 3/002: {Pretreatement}
- B05D 3/007: {After-treatment}
- B05D 7/52: {Two layers}
- B82Y 30/00: Nanotechnology for materials or surface science, e.g. nanocomposites
- B82Y 40/00: Manufacture or treatment of nanostructures
- C10M 105/62: containing hydroxy groups
- C10M 105/74: containing phosphorus
- C10M 177/00: Special methods of preparation of lubricating compositions; Chemical modification by after-treatment of components or of the whole of a lubricating composition, not covered by other classes
- B05D 7/14: to metal, e.g. car bodies (involving a chemical reaction between the metal and the coating C23)
- C10M 2223/06: having phosphorus-to-carbon bonds
- C10M 2223/063: Ammonium or amine salts
- C10N 2030/06: Oiliness; Film-strength; Anti-wear; Resistance to extreme pressure
- C10N 2040/06: Instruments or other precision apparatus, e.g. damping fluids
- C10N 2050/02: dissolved or suspended in a carrier which subsequently evaporates to leave a lubricant coating
- C10N 2080/00: Special pretreatment of the material to be lubricated, e.g. phosphatising or chromatising of a metal
- G04B: MECHANICALLY-DRIVEN CLOCKS OR WATCHES; MECHANICAL PARTS OF CLOCKS OR WATCHES IN GENERAL; TIME PIECES USING THE POSITION OF THE SUN, MOON OR STARS (spring- or weight-driven mechanisms in general F03G; electromechanical clocks or watches G04C; electromechanical clocks with attached or built-in means operating any device at pre-selected times or after predetermined time intervals G04C23/00; clocks or watches with stop devices G04F7/08)
- B05D: PROCESSES FOR APPLYING FLUENT MATERIALS TO SURFACES, IN GENERAL (conveying articles or workpieces through baths of liquid B65G, e.g. B65G49/02)
- B82Y: SPECIFIC USES OR APPLICATIONS OF NANOSTRUCTURES; MEASUREMENT OR ANALYSIS OF NANOSTRUCTURES; MANUFACTURE OR TREATMENT OF NANOSTRUCTURES
- C10M: LUBRICATING COMPOSITIONS (well drilling compositions C09K8/02); USE OF CHEMICAL SUBSTANCES EITHER ALONE OR AS LUBRICATING INGREDIENTS IN A LUBRICATING COMPOSITION (mould release, i.e. separating, agents for metals B22C3/00, for plastics or substances in a plastic state, in general B29C33/56, for glass C03B40/02; textile lubricating compositions D06M11/00, D06M13/00, D06M15/00; immersion oils for microscopy G02B21/33)
- C10N: INDEXING SCHEME ASSOCIATED WITH SUBCLASS C10M RELATING TO LUBRICATING COMPOSITIONS

## Abstract

The present invention describes the use of amine molecules (N) and phosphonic compounds (P) for coating surfaces intended to be used in the field of horology. Since these two types of compounds are alkaline and acid in nature, they form pairs of ions that interact with all types of surfaces, whether these are composed of mineral materials such as glass, metal, non-oxidised materials (inter alia gold, rhodium and their alloys), or also polymeric materials. Taking advantage of the surprising complementary nature of these two types of compounds, the present inventors propose a composition and a coating process that enable functionalisation layers to be formed on any type of material, in particular those used in clock mechanisms.

## Claims

### Claim at position 1

1-18. (canceled)

### Claim 19

A process for coating a surface in a clock mechanism or a device integrated into a watch product with a molecular functionalization layer, the process comprising:
a) optionally preparing said surface by washing in a solvent and/or in an aqueous detergent, then drying,
b) contacting said surface with a first composition comprising an effective quantity of a phosphonic compound until self-assembly of said phosphonic compound to a fine layer on said surface,
c) contacting said surface with a second composition comprising an effective quantity of an amine compound until self-assembly of said amine compound to a fine layer on said surface to form a functionalized surface,
d) removing supernatant from the functionalized surface,
e) rinsing the functionalized surface, and
f) drying the functionalized surface;
wherein said phosphonic compound and said amine compound are different compounds.

### Claim 20 (depends on 19)

The process according to claim 19, wherein b) and c) are carried out in succession.

### Claim 21 (depends on 20)

The process according to claim 20, wherein b) is carried out before c).

### Claim 22 (depends on 19)

The process according to claim 19, wherein the first composition and the second composition are the same composition and b) and c) are combined.

### Claim 23 (depends on 19)

The process according to claim 19, wherein b) to are repeated with the first composition, the second composition or both.

### Claim 24 (depends on 19)

The process according to claim 19, in which said surface comprises more than 50% of:
a metal selected from the group consisting of gold (Au), platinum (Pt), palladium (Pd), silver (Ag), rhodium (Rh), copper (Cu), iron (Fe), titanium (Ti), aluminium (Al), chromium (Cr), tantalum (Ta), aluminas, zirconias, ruby, sapphire, nickel (Ni), ruthenium (Ru), tin (Sn), a combination thereof and an oxide thereof,
an alloy selected from the group consisting of steel, stainless steel, brass, copper-nickel-zinc, bronze, tin-nickel (Sn—Ni), nickel-phosphorus (Ni—P), copper-beryllium (Cu—Be), palladium-nickel (Pd—Ni), copper-cobalt (Cu—Co) or a vanadium (V) alloy, chromium (Cr), manganese (Mn), zinc (Zn), tungsten (W), zirconium (Zr), an amorphous alloy, a combination thereof and an oxide thereof, zirconium oxide (ZrOx), titanium oxide (TiOx), tantalum oxide (TaxOy), and a combination thereof,
a semi-conductor selected from the group consisting of silicon (Si), germanium (Ge), and an oxide thereof, diamond in any form, and a combination thereof, and
a carbide, a nitride of or both of a material selected from the group consisting of boron (B), silicon (Si), tungsten (W), chromium (Cr), titanium (Ti), magnesium (Mg), aluminium (Al) and a combination thereof, and
a substituted or unsubstituted polymer selected from the group consisting of polyamide, polyacrylate, polyacrylamide, polyurethane, polyurea, polyester, polyketone, polyimide, polysulphide, polysulphoxide, polysulphone, polythiophene, polypyridine, polypyrrole, polyether, silicone, polyamide, polysaccharide, fluoropolymer, amide, imides, polypeptide, polyethylene, polyoxymethylene (POM), polystyrene, polypropylene, polyethylene terephthalate (PET), polyether ether ketone (PEEK), nylon, a copolymer thereof and a mixture thereof.

### Claim 25 (depends on 19)

The process according to claim 19, wherein the amine compound is of formula (I-N):
in which:
A is a (CH2)m—X— group, wherein m is an integer from 0-100, and X is a C0-C100 alkyl group that is saturated or unsaturated, perfluorinated or partially fluorinated, wherein the alkyl chain is unsubstituted or substituted with at least one 0 to 10 cycloalkyl or at least one aryl group that is perfluorinated or unperfluorinated; X is selected from the group consisting of a single covalent bond, —(O—CH2—CH2)m′, —(O—CH2—CH2-CH2)m′, —(O—CH2—CH(CH3))m′ and —(O—CH(CH3)—CH2)m′, wherein m′ is an integer from 0-100,
B is either a) or b):
a) a single chemical bond, an O atom, an S atom, S(CO), (CO)S, NR or (CO)NR, NR(CO), wherein R is a hydrogen atom or a C1-C10 alkyl,
b) one of the following formulas:
C is selected from the group consisting of a hydrogen atom, F(CF(CF3)CF2O)n(CF2)2CF3, F(CF2CF(CF3)O)n(CF2)2CF3, F(CF2CF2CF2O)n(CF2)2CF3, and F(CF2CF2O)n(CF2)2CF3 and CpF2p+1, in which n and p are integers from 1-100;
and
R1 and R2 independently of one another represent A-B-C groups as defined above, a hydrogen atom or a linear C1-C6 alkyl short-chain;
and/or in that said phosphonic compound has the following formula (I-P):
in which:
R is a hydrogen atom H, fluorine atom F or an OH group,
R′ is a hydrogen atom H, fluorine atom F or a PO3H2 group,
A is a (CH2)m—X— group, wherein m is an integer from 0-100, and X is a C0-C100 alkyl group that is saturated or unsaturated, perfluorinated or partially fluorinated, wherein the alkyl chain is unsubstituted or substituted with at least one 0 to 10 cycloalkyl or at least one aryl group that is perfluorinated or unperfluorinated; X is selected from the group consisting of a single covalent bond, —(O—CH2—CH2)m′, —(O—CH2—CH2-CH2)m′, —(O—CH2—CH(CH3))m′, and —(O—CH(CH3)—CH2)m′, wherein m′ is an integer from 0-100,
B is either a) or b):
a) a single chemical bond, an O atom, an S atom, S(CO), (CO)S, NZ or (CO)NZ, NZ(CO), wherein Z is a hydrogen atom or a C1-C10 alkyl, or
b) one of the following formulas:
and
C is selected from the group consisting of a hydrogen atom, (CF(CF3)CF2O)n(CF2)2CF3, (CF2CF(CF3)O)n(CF2)2CF3, (CF2CF2CF2O)n(CF2)2CF3, (CF2CF2O)n(CF2)CF3 and CpF2p+1—, in which n and p are integers from 1-100.

### Claim 26 (depends on 25)

The process according to claim 25, wherein m is an integer from 0-30.

### Claim 27 (depends on 25)

The process according to claim 25, wherein m′ is an integer from 0-50.

### Claim 28 (depends on 25)

The process according to claim 25, wherein n and p are integers from 1-50.

### Claim 29 (depends on 19)

The process according to claim 19, wherein said amine compound is a perfluoropolyether amine of the following formula (I′-N):
in which n is an integer f from 1-100, m is an integer 0-100 and x is an integer from 0-10,
and/or said phosphonic compound is a perfluorinated bisphosphonic acid of the following formula (I′-P):
in which n is an integer from 1-100, m is an integer from 0-100 and x is an integer from 0-10.

### Claim 30 (depends on 19)

The process according to claim 19, wherein said amine compound is an amine compound that is a linear alkyl amine of the following formula (I″-N):
in which n is an integer from 1-100;
and/or said phosphonic compound is a phosphonic compound of one of the following formulas (I″-P) and (I′″-P):
in which n is an integer from 1-100.

### Claim 31 (depends on 30)

The process according to claim 30, wherein n is an integer from 5-30.

### Claim 32 (depends on 31)

The process according to claim 31, wherein n is an integer from 8-20.

### Claim 33 (depends on 19)

The process according to claim 19, wherein said phosphonic compound and said amine compound are dissolved in a solvent selected from the group consisting of water, an alcohol, an aldehyde, a ketone, an ether, an alkane, a hydrotreated naphtha mixed with IPA or acetone, and a combination thereof.

### Claim 34

A process for increasing the hydrophobicity and/or lipophobicity of a surface in a clock mechanism or in a device integrated into a watch product, said process comprising:
a) optionally preparing said surface by washing in a solvent and/or in an aqueous detergent, then drying,
b) contacting said surface with a first composition comprising an effective quantity of a phosphonic compound until self-assembly of said phosphonic compound to a fine layer on said surface,
c) contacting said surface with a second composition comprising an effective quantity of an amine compound until self-assembly of said amine compound to a fine layer on said surface to form a functionalized surface,
d) removing supernatant from the functionalized surface,
e) rinsing the functionalized surface, and
f) drying the functionalized surface;
wherein said phosphonic compound and said amine compound are different compounds.

### Claim 35 (depends on 34)

The process according to claim 34, in which the first composition and the second composition are applied in a sequential manner or simultaneously.

### Claim 36 (depends on 34)

The process according to claim 34, wherein said surface comprises more than 50% of:
a metal selected from the group consisting of gold (Au), platinum (Pt), palladium (Pd), silver (Ag), rhodium (Rh), copper (Cu), iron (Fe), titanium (Ti), aluminium (Al), chromium (Cr), tantalum (Ta), aluminas, zirconias, ruby, sapphire, nickel (Ni), ruthenium (Ru), tin (Sn), a combination thereof and an oxide thereof,
an alloy selected from the group consisting of steel, stainless steel, brass, copper-nickel-zinc, bronze, tin-nickel (Sn—Ni), nickel-phosphorus (Ni—P), copper-beryllium (Cu—Be), palladium-nickel (Pd—Ni), copper-cobalt (Cu—Co) or a vanadium (V) alloy, chromium (Cr), manganese (Mn), zinc (Zn), tungsten (W), zirconium (Zr), an amorphous alloy, a combination thereof and an oxide thereof, zirconium oxide (ZrOx), titanium oxide (TiOx), tantalum oxide (TaxOy) and a combination thereof,
a semi-conductor selected from the group consisting of silicon (Si), germanium (Ge), and an oxide thereof, diamond in any form, and a combination thereof, and
a carbide, a nitride of or both of a material selected from the group consisting of boron (B), silicon (Si), tungsten (W), chromium (Cr), titanium (Ti), magnesium (Mg), aluminium (Al) and a combination thereof, and
a substituted or unsubstituted polymer selected from the group consisting of polyamide, polyacrylate, polyacrylamide, polyurethane, polyurea, polyester, polyketone, polyimide, polysulphide, polysulphoxide, polysulphone, polythiophene, polypyridine, polypyrrole, polyether, silicone, polyamide, polysaccharide, fluoropolymer, amide, imides, polypeptide, polyethylene, polyoxymethylene (POM), polystyrene, polypropylene, polyethylene terephthalate (PET), polyether ether ketone (PEEK), nylon, a copolymer thereof and a mixture thereof.

### Claim 37

A process for limiting the corrosion of a surface in a clock mechanism or in a device integrated into a watch product, said process comprising:
a) optionally preparing said surface by washing in a solvent and/or in an aqueous detergent, then drying,
b) contacting said surface with a first composition comprising an effective quantity of a phosphonic compound until self-assembly of said phosphonic compound to a fine layer on said surface,
c) contacting said surface with a second composition comprising an effective quantity of an amine compound until self-assembly of said amine compound to a fine layer on said surface to form a functionalized surface,
d) removing supernatant from the functionalized surface,
e) rinsing the functionalized surface, and
f) drying the functionalized surface;
wherein said phosphonic compound and said amine compound are different compounds.

### Claim 38

A process for limiting dirt deposition on a surface in a clock mechanism or in a device integrated into a watch product, said process comprising:
a) optionally preparing said surface by washing in a solvent and/or in an aqueous detergent, then drying,
b) contacting said surface with a first composition comprising an effective quantity of a phosphonic compound until self-assembly of said phosphonic compound to a fine layer on said surface,
c) contacting said surface with a second composition comprising an effective quantity of an amine compound until self-assembly of said amine compound to a fine layer on said surface to form a functionalized surface,
d) removing supernatant from the functionalized surface,
e) rinsing the functionalized surface, and
f) drying the functionalized surface;
wherein said phosphonic compound and said amine compound are different compounds.

### Claim 39

A process for limiting microbiological contamination on a surface in a clock mechanism or in a device integrated into a watch product, said process comprising:
a) optionally preparing said surface by washing in a solvent and/or in an aqueous detergent, then drying,
b) contacting said surface with a first composition comprising an effective quantity of a phosphonic compound until self-assembly of said phosphonic compound to a fine layer on said surface,
c) contacting said surface with a second composition comprising an effective quantity of an amine compound until self-assembly of said amine compound to a fine layer on said surface to form a functionalized surface,
d) removing supernatant from the functionalized surface,
e) rinsing the functionalized surface, and
f) drying the functionalized surface;
wherein said phosphonic compound and said amine compound are different compounds.

### Claim 40

A process for lubricating a surface in a clock mechanism or in a device integrated into a watch product, said process comprising:
a) optionally preparing said surface by washing in a solvent and/or in an aqueous detergent, then drying,
b) contacting said surface with a first composition comprising an effective quantity of a phosphonic compound until self-assembly of said phosphonic compound to a fine layer on said surface,
c) contacting said surface with a second composition comprising an effective quantity of an amine compound until self-assembly of said amine compound to a fine layer on said surface to form a functionalized surface,
d) removing supernatant from the functionalized surface,
e) rinsing the functionalized surface, and
f) drying the functionalized surface;
wherein said phosphonic compound and said amine compound are different compounds.

### Claim 41

A process for promoting flows on a surface in a clock mechanism or in a device integrated into a watch product, said process comprising:
a) optionally preparing said surface by washing in a solvent and/or in an aqueous detergent, then drying,
b) contacting said surface with a first composition comprising an effective quantity of a phosphonic compound until self-assembly of said phosphonic compound to a fine layer on said surface,
c) contacting said surface with a second composition comprising an effective quantity of an amine compound until self-assembly of said amine compound to a fine layer on said surface to form a functionalized surface,
d) removing supernatant from the functionalized surface,
e) rinsing the functionalized surface, and
f) drying the functionalized surface;
wherein said phosphonic compound and said amine compound are different compounds.

### Claim 42

A process for confining a lubricant in a predefined zone of a surface in a clock mechanism or in a device integrated into a watch product, said process comprising:
a) optionally preparing said surface by washing in a solvent and/or in an aqueous detergent, then drying,
b) contacting said surface with a first composition comprising an effective quantity of a phosphonic compound until self-assembly of said phosphonic compound to a fine layer on said surface,
c) contacting said surface with a second composition comprising an effective quantity of an amine compound until self-assembly of said amine compound to a fine layer on said surface to form a functionalized surface,
d) removing supernatant from the functionalized surface,
e) rinsing the functionalized surface, and
f) drying the functionalized surface;
wherein said phosphonic compound and said amine compound are different compounds.

### Claim 43

A functionalized surface in a clock mechanism or a device integrated into a watch product, wherein said functionalized surface comprises a covering molecular functionalization layer obtained by a process comprising:
a) optionally preparing said surface by washing in a solvent and/or in an aqueous detergent, then drying,
b) contacting said surface with a first composition comprising an effective quantity of a phosphonic compound until self-assembly of said phosphonic compound to a fine layer on said surface,
c) contacting said surface with a second composition comprising an effective quantity of an amine compound until self-assembly of said amine compound to a fine layer on said surface to form a functionalized surface,
d) removing supernatant from the functionalized surface,
e) rinsing the functionalized surface, and
f) drying the functionalized surface;
wherein said phosphonic compound and said amine compound are different compounds.

### Claim 44 (depends on 43)

The functionalized surface according to claim 43, wherein said surface is a contact surface of an escapement wheel with a plurality of pallet stones of a pallet of a clock escapement device, wherein said surface belongs to the escapement wheel and/or to the plurality of pallet stones.

### Claim 45 (depends on 43)

The functionalized surface according to claim 43, wherein said surface is a contact surface of an arbor and/or of a stone in which said arbor pivots.

### Claim 46

A clock mechanism comprising a functionalized surface, wherein said functionalized surface comprises a covering molecular functionalization layer obtained by a process comprising:
a) optionally preparing said surface by washing in a solvent and/or in an aqueous detergent, then drying,
b) contacting said surface with a first composition comprising an effective quantity of a phosphonic compound until self-assembly of said phosphonic compound to a fine layer on said surface,
c) contacting said surface with a second composition comprising an effective quantity of an amine compound until self-assembly of said amine compound to a fine layer on said surface to form a functionalized surface,
d) removing supernatant from the functionalized surface,
e) rinsing the functionalized surface, and
f) drying the functionalized surface;
wherein said phosphonic compound and said amine compound are different compounds.

### Claim 47

A timepiece comprising a functionalized surface, wherein said functionalized surface comprises a covering molecular functionalization layer obtained by a process comprising:
a) optionally preparing said surface by washing in a solvent and/or in an aqueous detergent, then drying,
b) contacting said surface with a first composition comprising an effective quantity of a phosphonic compound until self-assembly of said phosphonic compound to a fine layer on said surface,
c) contacting said surface with a second composition comprising an effective quantity of an amine compound until self-assembly of said amine compound to a fine layer on said surface to form a functionalized surface,
d) removing supernatant from the functionalized surface,
e) rinsing the functionalized surface, and
f) drying the functionalized surface;
wherein said phosphonic compound and said amine compound are different compounds.