# US 2015/0102519 A1 · Thin, Smooth Nitrile Rubber Gloves

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0102519 A1
- Document ID: US20150102519A1
- Status: Published application
- Kind: A1
- Application number: 14/573,045
- Filed: 2014-12-17
- Published: 2015-04-16
- Earliest claimed: 2008-08-27
- Assignees: Avent, Inc.
- Applicants: Avent, Inc.
- Inventors: Timothy M. Lipinski; Choong Kheng Tang
- Web page: https://patentgrep.com/patent/US20150102519A1

## CPC

- B29D 99/0067: {Gloves}
- A41D 19/0062: {made of one layer of material}
- A61B 42/00: Surgical gloves; Finger-stalls specially adapted for surgery; Devices for handling or treatment thereof
- B29C 33/58: Applying the releasing agents
- B29C 41/14: Dipping a core {(B29C41/10 takes precedence)}
- C08J 5/02: Direct processing of dispersions, e.g. latex, to articles
- C08L 9/04: Latex
- C08L 13/02: Latex
- B29K 2055/00: Use of specific polymers obtained by polymerisation reactions only involving carbon-to-carbon unsaturated bonds, not provided for in a single one of main groups {B29K2023/00 - B29K2049/00, e.g. having a vinyl group}, as moulding material
- B29K 2105/0085: {Copolymers}
- B29K 2995/0073: smooth
- C08J 2309/04: Latex
- Y10T 428/1352: Polymer or resin containing [i.e., natural or synthetic]
- B29D: PRODUCING PARTICULAR ARTICLES FROM PLASTICS OR FROM SUBSTANCES IN A PLASTIC STATE (making granules B29B9/00; making preforms B29B11/00)
- A41D: OUTERWEAR; PROTECTIVE GARMENTS; ACCESSORIES
- A61B: DIAGNOSIS; SURGERY; IDENTIFICATION (usefulness limited to only animals A61D)
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- B29K: INDEXING SCHEME ASSOCIATED WITH SUBCLASSES B29B, B29C OR B29D, RELATING TO MOULDING MATERIALS OR TO MATERIALS FOR {MOULDS, } REINFORCEMENTS, FILLERS OR PREFORMED PARTS, e.g. INSERTS
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

A nitrile-rubber medical exam glove composed of a glove body which is a flexible layer of nitrile-butadiene rubber. The glove body has a chlorinated first surface forming a donning side of the glove body and an un-chlorinated second surface forming a grip side of the glove body. The elastomeric glove also includes a substantially uniform distribution of a release agent distributed over the un-chlorinated second surface of the glove body. The elastomeric glove has: (a) an average thickness of between about 0.03 to 0.12 mm in a palm region of the glove body as measured in accordance with ASTM D3767, procedure A; (b) an un-chlorinated second surface of the glove body characterized by a Surface Root Mean Square Roughness of from about 3.00 Î¼m to about 6.55 Î¼m; and (c) a failure rate of less than about 1 percent when the elastomeric glove is subjected to pinhole leak testing generally in accordance with ASTM D5151-06.

## Claims

### Claim at position 1

1-14. (canceled)

### Claim 15

A process for making an elastomeric glove, the process comprising:
coating a surface of a mold with a coagulant solution and a release agent, the coagulation solution having a calcium ion concentration of between about 3 percent and about 5 percent based on the weight of calcium ions in the coagulant solution;
partially drying the mold coated with the coagulant solution and release agent; immersing the partially dried mold into an nitrile-butadiene rubber latex emulsion having a latex solids content of between about 12 percent and about 20 percent, by weight, for a dwell time of between about 7 seconds and 15 seconds to form a layer of coagulated nitrile-butadiene rubber latex on the mold surface;
removing the mold from the nitrile-butadiene rubber latex emulsion;
immersing the mold containing the coagulated nitrile-butadiene rubber latex into an aqueous bath to remove excess calcium ions and then drying the coagulated nitrile-butadiene rubber latex to form a glove body on the mold;
removing the glove body from the mold by inverting the glove body such that an exterior surface of the glove body forms an interior surface of the elastomeric glove and an interior surface of the glove body forms an exterior surface of the elastomeric glove.

### Claim 16 (depends on 15)

The process according to claim 15, wherein the ratio of coagulant ions on the mold and latex solids content are approximately 1:4.

### Claim 17 (depends on 15)

The process according to claim 15, wherein the partially dried mold is immersed into a nitrile-butadiene rubber latex emulsion having a latex solids content of between about 14 percent and about 20 percent, by weight.

### Claim 18 (depends on 15)

The process according to claim 15, wherein the partially dried mold is immersed into an nitrile-butadiene rubber latex emulsion for a dwell time of between about 8 seconds and 12 seconds to form a layer of coagulated nitrile-butadiene rubber latex on the mold surface.

### Claim 19 (depends on 15)

The process according to claim 15, wherein the partially dried mold is immersed into an nitrile-butadiene rubber latex emulsion in which the elastomeric nitrile-butadiene rubber comprises a terpolymer of acrylonitrile, butadiene, and carboxylic acid in which the acrylonitrile polymer content is about 15 percent, by weight, to about 42 percent, by weight, the carboxylic acid content is between about 1 percent, by weight and about 10 percent by weight, and the remaining portion of the terpolymer composition is butadiene.

### Claim 20 (depends on 15)

The process according to claim 15, further comprising immersing the mold containing the glove body into a chlorinating bath to chlorinate the exterior surface of the glove body on the mold prior to removing the glove body from the mold.

### Claim 21 (depends on 15)

The process according to claim 15, wherein the release agent is substantially uniformly distributed over the exterior surface of the elastomeric glove, wherein the release agent is waxy.

### Claim 22 (depends on 15)

The process according to claim 15, wherein the exterior surface of the elastomeric glove has a Surface Root Mean Square Roughness (Sq) of from about 3.00 μm to about 6.55 μm.

### Claim 23 (depends on 15)

The process according to claim 15, wherein the exterior surface of the elastomeric glove has a Surface Root Mean Square Roughness (Sq) of from about 3.00 μm to about 5.30 μm.

### Claim 24 (depends on 15)

The process according to claim 15, wherein the elastomeric glove has a failure rate of less than about 1 percent when the elastomeric glove is subjected to pinhole teak testing generally in accordance with ASTM D5151-06.

### Claim 25 (depends on 15)

The process according to claim 15, wherein the elastomeric glove has a failure rate of less than about 0.5 percent when the elastomeric glove is subjected to pinhole leak testing generally in accordance with ASTM D5151-06.

### Claim 26 (depends on 15)