# US 2015/0102455 A1 · Method of fabricating dual trench isolated selective epitaxial diode array

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0102455 A1
- Document ID: US20150102455A1
- Status: Published application
- Kind: A1
- Application number: 14/203,500
- Filed: 2014-03-10
- Published: 2015-04-16
- Earliest claimed: 2013-10-11
- Assignees: Semiconductor Manufacturing International (Shanghai) Corporation
- Applicants: Semiconductor Manufacturing International (Shanghai) Corporation
- Inventors: CHAO ZHANG
- Web page: https://patentgrep.com/patent/US20150102455A1

## CPC

- H10B 63/20: {comprising selection components having two electrodes, e.g. diodes}
- H10B 63/80: {Arrangements comprising multiple bistable or multi-stable switching components of the same type on a plane parallel to the substrate, e.g. cross-point arrays}
- H10D 62/115: {Dielectric isolations, e.g. air gaps}
- H10D 84/0165: {the components including complementary IGFETs, e.g. CMOS devices}
- H10D 84/038: {using silicon technology, e.g. SiGe}
- H10D 84/221: {of only diodes}
- H10D 84/811: {Combinations of field-effect devices and one or more diodes, capacitors or resistors}
- H10D 84/85: Complementary IGFETs, e.g. CMOS
- H10N 70/011: {Manufacture or treatment of multistable switching devices}
- H10W 10/014: {using trench refilling with dielectric materials, e.g. shallow trench isolations}
- H10W 10/041: {of isolation regions comprising polycrystalline semiconductor materials}
- H10W 10/17: formed using trench refilling with dielectric materials, e.g. shallow trench isolations
- H10W 10/40: Isolation regions comprising polycrystalline semiconductor materials
- H10B: ELECTRONIC MEMORY DEVICES
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10N: ELECTRIC SOLID-STATE DEVICES NOT OTHERWISE PROVIDED FOR
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

Methods and devices associated with phase change memory include diodes operating as selector switches having a large driving current and high switching speed. A method of forming a semiconductor device includes providing a semiconductor substrate, defining a diode array region and a peripheral region on the semiconductor substrate, forming an N+ buried layer in the diode array region by performing an ion implantation process and an annealing process. The method also includes forming a semiconductor epitaxial layer on the N+ buried layer, forming deep trench isolations through the epitaxial layer and the N+ buried layer into a portion of the substrate in the first direction, and forming shallow trench isolations in the diode array region and in the peripheral region in the second direction. The shallow trench isolation has a depth equal to or greater than a thickness of the epitaxial layer.

## Claims

### Claim 1

A method of manufacturing a semiconductor device, the method comprising:
providing a p-type semiconductor substrate;
defining a diode array region and a peripheral device region on the p-type semiconductor substrate;
forming a N+ buried layer in the diode array region by performing an ion implantation process and an annealing process;
forming a semiconductor epitaxial layer on the N+ buried layer;
forming a deep trench isolation through the epitaxial layer and the N+ buried layer into a portion of the substrate in a first direction;
forming a shallow trench isolation in the diode array region in a second direction and a shallow trench isolation in the peripheral region in the second direction, the shallow trench isolation having a depth equal to or greater than a thickness of the epitaxial layer;
forming a well region and a gate electrode of a CMOS device in the peripheral region;
forming a source and a drain of the CMOS device;
forming a P+ layer in the epitaxial layer; and
forming N+ contact regions in the diode array region and in the peripheral device region.

### Claim 2 (depends on 1)

The method of claim 1, wherein defining a diode array region and a peripheral device region on the semiconductor substrate comprising:
forming a groove having sidewalls and a bottom in the semiconductor substrate as the diode array region and a region outside the groove as the peripheral device region.

### Claim 3 (depends on 2)

The method of claim 2, wherein the groove has a depth in a range between 100 nm and 600 nm, and the sidewalls intercept the bottom at an angle between 80 and 90 degrees.

### Claim 4 (depends on 1)

The method of claim 1, wherein performing an ion implantation process and an annealing process comprises:
forming a lightly doped P-type material on a portion of the diode array region;
forming a heavily doped N-type material on the portion of the diode array region; and
activating the lightly doped P-type material and the heavily doped N-type material by annealing to from the N+ layer.

### Claim 5 (depends on 4)

The method of claim 4, wherein the lightly doped P-type material comprises B, BF2, or any combinations thereof; and the heavily doped N-type material comprises As, P, Sb, or any combinations thereof; and
the annealing is at a temperature between 950° C. and 1150° C. and with a time duration between 10 seconds and 7200 seconds.

### Claim 6 (depends on 1)

The method of claim 1, wherein forming a semiconductor epitaxial layer comprises a deposition process at a temperature in a range between 950° C. and 1100° C. and with dimethyl dichlorosilane as a reaction gas.

### Claim 7 (depends on 1)

The method of claim 1, wherein forming a semiconductor epitaxial layer comprises a deposition process at a temperature in a range between 500° C. and 900° C. and with silane or dimethyl dichlorosilane as a reaction gas.

### Claim 8 (depends on 1)

The method of claim 1, wherein the deep trench isolation comprises undoped polysilicon layer and an oxide layer on the undoped polysilicon layer.

### Claim 9 (depends on 1)

The method of claim 1, forming a deep trench isolation comprises:
concurrently surrounding the diode array region with the deep trench isolation to isolate the diode array region from the peripheral region.

### Claim 10 (depends on 1)

The method of claim 1, wherein the shallow trench isolation in the diode array region and the shallow trench isolation in the peripheral are concurrently formed.

### Claim 11 (depends on 1)

The method of claim 1, further comprising, after forming the shallow trench isolation and prior to forming the P+ layer in the epitaxial layer:
forming an N-type layer disposed between the N+ buried layer at a bottom and the P+ layer at a top.

### Claim 12 (depends on 11)

The method of claim 11, wherein the N-type layer is formed by implanting an N− dopant into the epitaxial layer or by diffusing the N+ buried layer.

### Claim 13 (depends on 11)

The method of claim 11, wherein the source and the drain of the CMOS device is formed concurrently with forming a P+ in the epitaxial layer or the source and the drain of the CMOS device is formed concurrently with forming a N+ buried layer in the diode array region.

### Claim 14 (depends on 1)

The method of claim 1, wherein the P+ layer is a shallow junction.

### Claim 15 (depends on 1)

The method of claim 1, further comprising:
forming a bit line and a word line;
connecting the bit line with the P+ layer; and
connecting the word line with the N+ buried layer.

### Claim at position 16

16-20. (canceled)