# US 2015/0102357 A1 · GaN-containing semiconductor structure

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0102357 A1
- Document ID: US20150102357A1
- Status: Published application
- Kind: A1
- Application number: 14/190,382
- Filed: 2014-02-26
- Published: 2015-04-16
- Earliest claimed: 2013-10-14
- Assignees: National Chiao Tung University
- Applicants: National Chiao Tung University
- Inventors: Yi CHANG; Yuen Yee WONG; Chi Feng HSIEH
- Web page: https://patentgrep.com/patent/US20150102357A1

## CPC

- H10D 62/8503: {Nitride Group III-V materials, e.g. AlN or GaN}
- H10P 14/24: using chemical vapour deposition [CVD]
- H10P 14/2921: {being crystalline insulating materials}
- H10P 14/3216: {Nitrides}
- H10P 14/3251: {consisting of three or more layers}
- H10P 14/3416: {Nitrides}
- H10D 8/60: Schottky-barrier diodes
- H10D 30/47: having two-dimensional [2D] charge carrier gas channels, e.g. nanoribbon FETs or high electron mobility transistors [HEMT]
- H10D 30/471: {High electron mobility transistors [HEMT] or high hole mobility transistors [HHMT]}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A method for forming a GaN-containing semiconductor structure is provided. The method comprises a substrate is provided, a nucleation layer is formed above the substrate, a diffusion blocking layer is formed above the nucleation layer, a strain relief layer is formed above the diffusion blocking layer, and a semiconductor layer is formed above the strain relief layer, in which the diffusion blocking layer is deposited on the nucleation layer such that the diffusion blocking layer can prevent the impurities out-diffusion from the substrate.

## Claims

### Claim 1

A method for forming a GaN-containing semiconductor structure by using metal-organic chemical vapor deposition (MOCVD), comprising:
providing a substrate;
providing a nucleation layer on the substrate by using metal-organic chemical vapor deposition (MOCVD), wherein a forming temperature of the nucleation layer is from 500° C. to 800° C.;
providing a diffusion blocking layer on the nucleation layer;
providing a strain relief layer on the diffusion blocking layer; and
providing a semiconductor layer on the strain relief layer.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the nucleation layer, the diffusion blocking layer, the strain relief layer and the semiconductor layer are achieved by using metal-organic chemical vapor deposition (MOCVD).

### Claim 3

(canceled)

### Claim 4 (depends on 1)

The method according to claim 1, wherein the forming temperature of the diffusion blocking layer is from 950° C. to 1200° C.

### Claim 5 (depends on 1)

The method according to claim 1, wherein the forming temperature of the strain relief layer is from 450° C. to 600° C.

### Claim 6 (depends on 1)

The method according to claim 1, wherein the forming temperature of the semiconductor layer is from 950° C. to 1200° C.

### Claim 7

A GaN-containing semiconductor structure formed by using metal-organic chemical vapor deposition (MOCVD), comprising:
a substrate;
a nucleation layer on the substrate;
a diffusion blocking layer on the nucleation layer, wherein the diffusion blocking layer is selected from the group consisting of a single AlN layer, the single AlN layer with a single AlGaN layer, the single AlN layer with multiple AlGaN layers;
a strain relief layer on the diffusion blocking layer; and
a semiconductor layer on the strain relief layer.

### Claim 8 (depends on 7)

The structure according to claim 7, wherein the nucleation layer is the AlN nucleation layer.

### Claim 9

(canceled)

### Claim 10 (depends on 7)

The structure according to claim 7, wherein the strain relief layer is the GaN, and a thickness is from 30 nm to 100 nm.

### Claim 11 (depends on 2)

The method according to claim 2, wherein the forming temperature of the diffusion blocking layer is from 950° C. to 1200° C.;
the forming temperature of the strain relief layer is from 450° C. to 600° C.; and wherein the forming temperature of the semiconductor layer is from 950° C. to 1200° C.

### Claim 12 (depends on 7)

The structure according to claim 7, wherein the nucleation layer is the AlN nucleation layer and the strain relief layer is the GaN, and a thickness is from 30 nm to 100 nm.