# US 2015/0102267 A1 · METHOD FOR PREPARING GRAPHENE-BASED LiFePO4/C COMPOSITE MATERIAL

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0102267 A1
- Document ID: US20150102267A1
- Status: Published application
- Kind: A1
- Application number: 14/401,489
- Filed: 2013-05-09
- Published: 2015-04-16
- Earliest claimed: 2012-05-14
- Assignees: Guoguang Electric Company Limited
- Applicants: Guoguang Electric Company Limited
- Inventors: Guorong Hu; Yanbing Cao; Kaipeng Wu; Zhongdong Peng; Ke Du
- Web page: https://patentgrep.com/patent/US20150102267A1

## CPC

- H01B 1/06: mainly consisting of other non-metallic substances
- C01B 25/375: {of iron}
- C01B 25/45: containing plural metal, or metal and ammonium
- C01B 32/184: Preparation
- C01B 32/23: Oxidation
- H01M 4/04: Processes of manufacture in general
- H01M 4/136: Electrodes based on inorganic compounds other than oxides or hydroxides, e.g. sulfides, selenides, tellurides, halogenides or LiCoFy
- H01M 4/1397: of electrodes based on inorganic compounds other than oxides or hydroxides, e.g. sulfides, selenides, tellurides, halogenides or LiCoFy
- H01M 4/5825: {Oxygenated metallic salts or polyanionic structures, e.g. borates, phosphates, silicates, olivines}
- H01M 4/625: {Carbon or graphite}
- Y02E 60/10: Energy storage using batteries
- H01B: CABLES; CONDUCTORS; INSULATORS; SELECTION OF MATERIALS FOR THEIR CONDUCTIVE, INSULATING OR DIELECTRIC PROPERTIES (selection for magnetic properties H01F1/00; waveguides H01P {; printed circuits H05K})
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

The present invention relates to a method for preparing a graphene-based LiFePO4/C composite material, to solve the problem of poor conductivity and rate performance of lithium iron phosphate cathode material. The main features of the present invention include the steps of: 1) preparing an iron salt solution having graphene oxide dispersed therein; 2) preparing a ferric phosphate/graphene oxide precursor; 3) preparing the graphene-based LiFePO4/C composite material. The beneficial effects of the method is that the process is simple, easy to control and the resulted graphene-based LiFePO4/C composite material has high specific capacity, good recycle performance and excellent rate capability is particularly suitable to the field of the power battery application.

## Claims

### Claim 1

A method for preparing a graphene-based LiFePO4/C composite material, comprising:
dissolving a graphene oxide and an iron salt in a deionized water, a mass ratio of the graphene oxide over an iron element in the iron salt being 0.1˜0.3:1;
dispersing the graphene oxide by ultrasonic to obtain an iron salt solution having the graphene oxide dispersed therein;
mixing the iron salt solution with a phosphate solution to obtain a reaction mixture, in which a molar ratio of Fe:P 1:1˜1.2;
adjusting a pH value of the reaction mixture to 2 to 4;
controlling a temperature of the reaction mixture to allow the reaction mixture to react at 60° C. to 80° C. to obtain an emulsion;
filtering the emulsion to obtain a ferric phosphate/graphene oxide precursor;
blending the ferric phosphate/graphene oxide precursor with a lithium salt at a Li:Fe molar ratio of 1˜1.05:1 to form a first mixture;
adding a carbon source to the first mixture to form a second mixture; and
sintering the second mixture under a reducing atmosphere condition at 600° C. to 700° C., to obtain the graphene-based LiFePO4/C composite material.

### Claim 2 (depends on 1)

The method according to claim 1, wherein an iron ion concentration in the iron salt solution is 0.5 to 2 mol/L.

### Claim 3 (depends on 1)

The method according to claim 1, wherein dispersing the graphene oxide by ultrasonic includes dispersing the graphene oxide by ultrasonic for 2 to 5 hours.

### Claim 4 (depends on 1)

The method according to claim 1, wherein:
controlling the temperature of the reaction mixture to allow the reaction mixture to react includes allowing the reaction mixture to react for 3 to 6 hours; and
sintering includes sintering for 5 to 10 hours.

### Claim 5 (depends on 1)

The method according to claim 1, wherein dissolving the iron salt solution in the deionized water includes dissolving at least one of a ferric sulphate, a ferric chloride, or a ferric nitrate in the deionized water.

### Claim 6 (depends on 1)

The method according to claim 1, wherein mixing the iron salt solution with the phosphate is solution includes mixing the iron salt solution with a solution of at least one of a phosphoric acid, an ammonium biphosphate, an ammonium monoacid phosphate, an ammonium phosphate, a sodium biphosphate, a sodium monoacid phosphate, or a sodium phosphate.

### Claim 7 (depends on 1)

The method according to claim 1, wherein adjusting the PH value of the reaction mixture includes adjusting the PH value of the reaction mixture using an alkaline solution having a concentration of 0.5 to 5 mol/L, the alkaline solution including a solution of a sodium hydroxide, a sodium carbonate, or an ammonia.

### Claim 8 (depends on 1)

The method according to claim 1, wherein blending the ferric phosphate/graphene oxide precursor with the lithium salt includes blending the ferric phosphate/graphene oxide precursor with at least one of a lithium carbonate, a lithium hydroxide, or a lithium acetate.

### Claim 9 (depends on 1)

The method according to claim 1, wherein adding the carbon source includes adding at least one of a glucose, a sucrose, a fructose, a lactose, a citric acid, a starch, a polyvinyl alcohol, a polypropylene, or a phenolic resin, having an amount equaling to 5 to 20% of a theoretical mass of a lithium iron phosphate.

### Claim 10 (depends on 1)

The method according to claim 1, wherein sintering under the reducing atmosphere condition includes sintering in a mixed gas having a volume ratio of Ar:H2=90:10 to 95:5 or of N2:H2=90:10 to 95:5.

### Claim 11 (depends on 1)

The method according to claim 1, further comprising:
washing and drying the emulsion after filtering the emulsion.

### Claim 12 (depends on 1)

The method according to claim 1, further comprising:
performing a ball milling on the second mixture.

### Claim 13 (depends on 1)

The method according to claim 1, wherein dissolving the iron salt in the deionized water includes:
dissolving a ferrous salt in the deionized water, the ferrous salt including at least one of a ferrous sulfate, a ferrous chloride, or a ferrous nitrate; and
oxidizing the ferrous salt using an excess H2O2.