- Assignees: Ocean's King Lighting Science & Technology Co., Ltd.; Shenzhen Ocean's King Lighting Engineering Co., Ltd.
- Inventors: Mingjie Zhou; Rong Wang; Guitang Chen
- Web page: https://patentgrep.com/patent/US20150102260A1

## CPC

- C09K 11/87: containing platina group metals
- C09K 11/02: Use of particular materials as binders, particle coatings or suspension media therefor
- C09K 11/58: containing copper, silver or gold
- C09K 11/7703: {with alkaline earth metals}
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE

## Abstract

A titanate luminescent material has a formula of A1-x,TiO3:Prx@TiO2@My; wherein A is at least one selected from the group consisting of Ca, Sr, and Ba; M is at least one nanoparticles selected from the group consisting of Ag, Au, Pt, Pd, and Cu; 0<x≦0.01; y is the molar ratio between M and Ti in A1-x,TiO3:Prx@TiO2, and 0<y≦1×10−2; @ represents coating; M is a core, TiO2 is an intermediate layer shell, and A1-xTiO3:Prx is an outer layer shell. The titanate luminescent material has a high stability and a better luminescent performance. A preparation method of the titanate luminescent material is also provided.

## Claims

### Claim 1

A titanate luminescent material, having a formula of A1-xTiO3:Prx@TiO2@My;
wherein A is at least one selected from the group consisting of Ca, Sr, and Ba;
M is at least one nanoparticles selected from the group consisting of Ag, Au, Pt, Pd, and Cu;
0<x≦0.01;
y is the molar ratio between M and Ti in A1-xTiO3:Prx@TiO2, and 0<y≦1×10−2;
@ represents coating; M is a core, TiO2 is an intermediate layer shell, and A1-xTiO3:Prx is an outer layer shell.

### Claim 2 (depends on 1)

The titanate luminescent material according to claim 1, wherein 0.001≦x≦0.005.

### Claim 3 (depends on 1)

The titanate luminescent material according to claim 1, wherein 1×10−5≦y≦5×10−3.

### Claim 4

A method of preparing a titanate luminescent material, comprising the following steps:
step one, mixing a metal salt solution and triethanolamine titanium isopropoxide, adding a reducing agent, heating at a temperature of 120° C. to 160° C. with stirring, and obtaining TiO2@M, colloid, rinsing and drying the colloid to prepare TiO2@My solid having a core-shell structure, wherein M is at least one nanoparticles selected from the group consisting of Ag, Au, Pt, Pd, and Cu; y is the molar ratio between M and Ti, and 0<y≦1×10−2;
step two, mixing a source compound of A, a source compound of Pr, and the TiO2@My solid to form a mixture, calcining the mixture at temperature of 800° C. to 1200° C. and for 2 hours to 12 hours, and then heating the mixture at temperature of 1000° C. to 1400° C. for 0.5 hours to 6 hours in a reducing atmosphere, cooling and grinding the mixture to prepare A1-xTiO3:Prx@TiO2@My powder, wherein A is at least one selected from the group consisting of Ca, Sr, and Ba; 0<x≦0.01; @ represents coating; M is a core, TiO2 is an intermediate layer shell, and A1-xTiO3:Pr, is an outer layer shell.

### Claim 5 (depends on 4)

The method according to claim 4, wherein the source compound of A in step two is at least one selected from the group consisting of oxide, carbonate, nitrate, and hydroxide of A.

### Claim 6 (depends on 4)

The method according to claim 4, wherein the source compound of Pr in step two is at least one selected from the group consisting of oxide, carbonate, nitrate, and hydroxide of Pr.

### Claim 7 (depends on 4)

The method according to claim 4, wherein in step one, the reducing agent is dimethyl formamide; and a volume of the reducing agent is 20% to 80% of the sum volume of metal salt solution, triethanolamine titanium isopropoxide, and the reducing agent.

### Claim 8 (depends on 7)

The method according to claim 7, wherein the volume of the reducing agent is 25% to 50% of the sum volume of metal salt solution, triethanolamine titanium isopropoxide, and the reducing agent.

### Claim 9 (depends on 4)

The method according to claim 4, wherein in step one, the TiO2@My colloid is centrifugally precipitated and then rinsed with ethanol.

### Claim 10 (depends on 4)

The method according to claim 4, wherein the reducing atmosphere in step two comprises at least one reducing gas selected from the group consisting of mixed atmosphere of nitrogen and hydrogen, carbon, carbon monoxide, and pure hydrogen.