# US 2015/0102087 A1 · Method and device for improving the quality of the weld seam in friction stir welding

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0102087 A1
- Document ID: US20150102087A1
- Status: Published application
- Kind: A1
- Application number: 14/403,372
- Filed: 2013-05-29
- Published: 2015-04-16
- Earliest claimed: 2012-05-31
- Assignees: Grenzebach Maschinenbau GmbH
- Applicants: GrenzebachMaschinenbau GmbH
- Inventors: Johann Foerg; Martin Demharter; Andreas Reitenauer
- Web page: https://patentgrep.com/patent/US20150102087A1

## CPC

- B23K 20/1225: {Particular aspects of welding with a non-consumable tool}
- B23K 20/123: {Controlling or monitoring the welding process}
- B23K 20/125: {Rotary tool drive mechanism}
- B23K 20/1255: {Tools therefor, e.g. characterised by the shape of the probe}
- B23K: SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM

## Abstract

A method and a device for improving the quality of the weld seam in friction stir welding is provided. The process of friction stir welding is effected by means of a friction welding tip, in which a spiral conveyor screw is provided in the spindle bearing. The longitudinal axis of the spindle bearing is inclined at an angle to the vertical. The sliding surface of the rotating spindle consists of a flat sliding surface and, for the welding of curved seams, in each case of a sliding surface inclined at an acute angle to the sliding surface, the friction welding tip is designed in the shape of a truncated cone. The lateral surface of the truncated cone is formed by six trapezoidal planar parts, of which three planar parts each uniformly distributed at the circumference lie at an angle of 120 degrees with respect to one another and account for a proportion greater than ⅙ at the circumference.

## Claims

### Claim 1

A device for improving the quality of a weld seam in friction stir welding comprising:
a) a receiving plate with a drive head and a spindle bearing for receiving a friction welding tip, wherein a transporting screw, which is machined in a spiral form in the spindle bearing, and transports away applied material that is not required, enters into openings leading obliquely outward,
b) wherein the longitudinal axis of the spindle bearing is inclined with respect to the vertical at an angle of 2.8 to 3.2 degrees,
c) wherein the sliding surface of the rotary spindle consists of a planar sliding surface and, particularly for the welding of curved seams, of a respective sliding surface which is itself curved, adjoins on two opposite sides and is inclined at an acute angle to the sliding surface, and
d) wherein the friction welding tip has the form of a truncated cone on which the top surface is raised in the middle, and wherein the lateral surface of the truncated cone is formed by six trapezoidal segments, of which three segments are respectively distributed uniformly on the circumference, lie at an angle of 120 degrees with respect to one another and account for a proportion greater than ⅙ of the circular circumference.

### Claim 2 (depends on 1)

The device as claimed in claim 1, wherein
the inclination of the longitudinal axis of the spindle bearing, the inclination of the surfaces and the pressing pressure of the sliding surface are dimensioned in such a way that they are optimized for the welding of a thin metal sheet with a curved border at the sides to a shaped body designed in the form of a dish and bordered in the same way at the edges.

### Claim 3 (depends on 1)

The device as claimed in claim 1, wherein the pressing pressure of the sliding surfaces can be set, and the respective setting is measured and displayed.

### Claim 4 (depends on 1)

The device as claimed in claim 1, wherein the pressing pressure can be set and for which the pressing pressure is monitored are used for fixing the components to be welded.

### Claim 5 (depends on 1)

The device as claimed in claim 1, wherein the result of the welding process is monitored optically.

### Claim 6

A method for improving the quality of the weld seam in friction stir welding comprising the following steps:
a) the process of friction stir welding is effected by means of a friction welding tip, in which a transporting screw, which is machined in a spiral form in the spindle bearing, transports away applied material that is not required,
b) inclining the longitudinal axis of the spindle bearing with respect to the vertical at an angle of 2.8 to 3.2 degrees,
c) wherein the sliding surface of the rotary spindle consists of a planar sliding surface and, for the welding of curved seams, of a respective sliding surface which is itself curved, adjoining on two opposite sides and inclining at an acute angle to the sliding surface, and
d) the friction welding tip is designed in the form of a truncated cone on which the top surface is raised in the middle, wherein the lateral surface of the truncated cone is formed by six trapezoidal segments, of which three segments are respectively distributed uniformly on the circumference, lie at an angle of 120 degrees with respect to one another and account for a proportion greater than ⅙ of the circular circumference.

### Claim 7 (depends on 6)

The method as claimed in claim 6, comprising the step of setting the pressing pressure of the sliding surfaces, measuring and displaying the respective setting, and consequently controlling the welding process.

### Claim 8 (depends on 6)

The method as claimed in claim 6, comprising the step of optically monitoring the result of the welding process.

### Claim 9 (depends on 6)

A computer program with a program code for carrying out the method of claim 6, when the program is run in a computer.

### Claim 10 (depends on 6)

A machine-readable carrier with the program code of a computer program for carrying out the method as claimed in claim 6, when the program is run in a computer.