# US 2015/0102033 A1 · Container with high density molecular weight polyethylene moisture barrier layer

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0102033 A1
- Document ID: US20150102033A1
- Status: Published application
- Kind: A1
- Application number: 14/175,583
- Filed: 2014-02-07
- Published: 2015-04-16
- Earliest claimed: 2013-10-11
- Assignees: Silgan Plastics LLC
- Applicants: Silgan Plastics LLC
- Inventors: Susan Banovic
- Web page: https://patentgrep.com/patent/US20150102033A1

## CPC

- B65D 1/0215: {multilayered (B65D81/3837 takes precedence)}
- B29C 49/22: using multilayered preforms or parisons
- B29C 49/78: Measuring, controlling or regulating
- B65D 1/0246: {Closure retaining means, e.g. beads, screw-threads}
- B29C 2949/3088: Bonding
- B29K 2023/06: {PE, i.e. polyethylene}
- B29K 2023/086: {EVOH, i.e. ethylene vinyl alcohol copolymer}
- B29K 2067/003: {PET, i.e. poylethylene terephthalate}
- Y02W 30/80: Packaging reuse or recycling, e.g. of multilayer packaging (bio-packaging Y02W90/10)
- B65D: CONTAINERS FOR STORAGE OR TRANSPORT OF ARTICLES OR MATERIALS, e.g. BAGS, BARRELS, BOTTLES, BOXES, CANS, CARTONS, CRATES, DRUMS, JARS, TANKS, HOPPERS, FORWARDING CONTAINERS; ACCESSORIES, CLOSURES, OR FITTINGS THEREFOR; PACKAGING ELEMENTS; PACKAGES
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- B29K: INDEXING SCHEME ASSOCIATED WITH SUBCLASSES B29B, B29C OR B29D, RELATING TO MOULDING MATERIALS OR TO MATERIALS FOR {MOULDS, } REINFORCEMENTS, FILLERS OR PREFORMED PARTS, e.g. INSERTS
- Y02W: CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO WASTEWATER TREATMENT OR WASTE MANAGEMENT

## Abstract

A molded, low moisture vapor transmission plastic container is provided. The container includes a sidewall including an inner surface, an outer surface, a thickness and a first layer formed from a high density polyethylene resin. The container includes a bottom wall located at a lower end of the sidewall, and the bottom wall includes an inner surface and an outer surface. The inner surfaces of the sidewall and of the bottom wall define an interior contents cavity. The container includes a neck located at an upper end of the sidewall defining an opening into the interior contents cavity. The high density polyethylene resin acts as an effective moisture barrier limiting moisture transmission into or out of the container.

## Claims

### Claim 1

A molded, low moisture vapor transmission plastic container comprising:
a sidewall including an inner surface, an outer surface, a thickness and a first layer formed from a high density polyethylene resin;
a bottom wall located at a lower end of the sidewall, the bottom wall including an inner surface and an outer surface, wherein the inner surfaces of the sidewall and of the bottom wall define an interior contents cavity; and
a neck located at an upper end of the sidewall defining an opening into the interior contents cavity;
wherein the high density polyethylene resin of the first layer has a resin density of about 0.966 grams/cc and a polydispersity index of about 8.72, wherein the first layer has a USP 31 Chapter 671 moisture vapor transmission rate of 1.145 mg/day-liter or less.

### Claim 2 (depends on 1)

The molded, low moisture vapor transmission plastic container of claim 1, wherein the high density polyethylene resin of the first layer is an octene homopolymer.

### Claim 3 (depends on 1)

The molded, low moisture vapor transmission plastic container of claim 1, wherein the container is blow-molded, wherein the sidewall has a thickness of about 40 mils, and further wherein the density of the first layer following blow-molding is about 0.949 grams/cc.

### Claim 4 (depends on 1)

The molded, low moisture vapor transmission plastic container of claim 1, wherein the sidewall includes a second layer of polymer material adjacent to the first layer.

### Claim 5 (depends on 4)

The molded, low moisture vapor transmission plastic container of claim 4, wherein the second layer of the sidewall is an EVOH layer.

### Claim 6 (depends on 4)

The molded, low moisture vapor transmission plastic container of claim 4, wherein the second layer of the sidewall is formed from a high density polyethylene layer having a resin density of between 0.953 and 0.965 grams/cc.

### Claim 7 (depends on 1)

The molded, low moisture vapor transmission plastic container of claim 1, further comprising a closure, wherein the neck includes an engagement structure, wherein the closure is coupled to the neck by the engagement structure.

### Claim 8 (depends on 7)

The molded, low moisture vapor transmission plastic container of claim 7, wherein the engagement structure is threading.

### Claim 9 (depends on 7)

The molded, low moisture vapor transmission plastic container of claim 7, further comprising a pharmaceutical product located within the interior contents cavity of the container.

### Claim 10

A low moisture vapor transmission plastic container comprising:
a sidewall including an inner surface, an outer surface and a thickness;
a bottom wall located at a lower end of the sidewall, the bottom wall including an inner surface and an outer surface, wherein the inner surfaces of the sidewall and the bottom wall define an interior contents cavity; and
a neck located at an upper end of the sidewall and including an engagement structure configured to engage a closure to seal the container;
wherein at least a portion of the sidewall is formed from a moisture barrier, high density polyethylene resin having a resin density greater than 0.960 and less than 0.970 grams/cc and a polydispersity index between 8 and 10, wherein the sidewall has a thickness between 10 mil and 50 mils, wherein the moisture barrier, high density polyethylene resin has a water vapor transmission rate such that less than 0.050 grams of water per day traverse a layer of the moisture barrier, high density polyethylene resin having thickness of 1 mil and a surface area of 100 in2.

### Claim 11 (depends on 10)

The low moisture vapor transmission plastic container of claim 10, wherein the moisture barrier, high density polyethylene resin is an octene homopolymer.

### Claim 12 (depends on 11)

The low moisture vapor transmission plastic container of claim 11, wherein the container is blow-molded, and the density of moisture barrier, high density polyethylene resin of the sidewall following blow-molding is between 0.945 and 0.95 grams/cc.

### Claim 13 (depends on 10)

The low moisture vapor transmission plastic container of claim 10, wherein the sidewall includes at least two layers of polymer material.

### Claim 14 (depends on 13)

The low moisture vapor transmission plastic container of claim 13, wherein at least one layer of the sidewall is an EVOH layer.

### Claim 15 (depends on 13)

The low moisture vapor transmission plastic container of claim 13, the sidewall has a thickness of about 40 mils.

### Claim 16 (depends on 13)

The low moisture vapor transmission plastic container of claim 13, wherein the moisture barrier, high density polyethylene resin has a water vapor transmission rate such that less than 0.040 grams of water per day traverse a layer of the moisture barrier, high density polyethylene resin having thickness of 1 mil and a surface area of 100 in2.

### Claim 17

A method of forming low moisture vapor transmission plastic containers comprising:
molding a first group of a plurality of container from a polyethylene resin having a resin density greater than 0.960 and less than 0.970 grams/cc and a polydispersity index between 8.5 and 9.0;
testing the moisture vapor transmission rate of a wall of each container of the first group, wherein the container formed from the polyethylene resin has a water vapor transmission rate such that less than 0.050 grams of water per day traverse a layer of the polyethylene resin having thickness of 1 mil and a surface area of 100 in2; and
molding a second group of a plurality of containers, each container of the second group having a layer formed from the polyethylene resin and having a sidewall defining an interior cavity and a neck defining an opening into the interior cavity.

### Claim 18 (depends on 17)

The method of claim 17, wherein the first group of containers and the second group of containers are formed by blow-molding, and the density the polyethylene resin following blow-molding is between 0.945 and 0.95 grams/cc.

### Claim 19 (depends on 18)

The method of claim 18, wherein the polyethylene resin is an octene homopolymer.

### Claim 20 (depends on 18)

The method of claim 18, wherein a sidewall of the containers of the second group of containers has a thickness between 10 mil and 50 mil.