# US 2015/0101934 A1 · Controlled trivalent chromium pretreatment

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0101934 A1
- Document ID: US20150101934A1
- Status: Published application
- Kind: A1
- Application number: 14/052,719
- Filed: 2013-10-12
- Published: 2015-04-16
- Earliest claimed: 2013-10-12
- Assignees: Hamilton Sundstrand Corporation
- Applicants: Hamilton Sundstrand Corporation
- Inventors: Sameh Dardona; Mark R. Jaworowski; Sergei F. Burlatsky; Dmitri Novikov; Lei Chen
- Web page: https://patentgrep.com/patent/US20150101934A1

## CPC

- C25D 3/06: from solutions of trivalent chromium
- C25D 5/18: Electroplating using modulated, pulsed or reversing current
- C25D 9/04: with inorganic materials
- C25D 9/06: by anodic processes
- C25D 21/12: Process control or regulation (controlling or regulating in general G05)
- C25D: PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTION OF COATINGS; ELECTROFORMING; APPARATUS THEREFOR

## Abstract

A method for forming a trivalent chromium coating on an aluminum alloy substrate includes adding a chromium-containing solution to a vessel, immersing the aluminum alloy substrate in the chromium-containing solution, immersing a counter electrode in the chromium-containing solution, and applying an electrical potential bias to the aluminum alloy substrate with respect to its equilibrium potential to form a trivalent chromium coating on an outer surface of the aluminum alloy substrate. A method for forming a trivalent chromium coating on a metal substrate includes adding a chromium-containing solution to a vessel, immersing the metal substrate in the chromium-containing solution, immersing a counter electrode in the chromium-containing solution, and modulating an electrical potential difference between the metal substrate and the counter electrode to form a trivalent chromium coating on an outer surface of the metal substrate.

## Claims

### Claim 1

A method for forming a trivalent chromium coating on an aluminum alloy substrate, the method comprising:
adding a chromium-containing solution to a vessel;
immersing the aluminum alloy substrate in the chromium-containing solution;
immersing a counter electrode in the chromium-containing solution; and
applying an electrical potential bias to the aluminum alloy substrate with respect to its equilibrium potential to form a trivalent chromium coating on an outer surface of the aluminum alloy substrate.

### Claim 2 (depends on 1)

The method of claim 1, wherein the electrical potential bias is between about −0.1 V and about −1.3 V with respect to a standard hydrogen electrode (SHE) to promote dissolution of Al3+ ions from the outer surface of the aluminum alloy substrate and promote deposition of ZrO2 or TiO2 on the outer surface of the aluminum alloy substrate.

### Claim 3 (depends on 1)

The method of claim 1, wherein the electrical potential bias is between about −1.3 V and about −1.6 V with respect to a SHE to promote deposition of Cr(OH)3 on the outer surface of the aluminum alloy substrate.

### Claim 4 (depends on 1)

The method of claim 1, wherein the electrical potential bias is modulated between a positive value and a negative value relative to the equilibrium potential of the aluminum alloy substrate.

### Claim 5 (depends on 4)

The method of claim 4, wherein the electrical potential bias is at the positive value for a period of time longer than the negative value to promote dissolution of Al3+ ions from the outer surface of the aluminum alloy substrate and promote deposition of ZrO2 or TiO2 on the outer surface of the aluminum alloy substrate.

### Claim 6 (depends on 5)

The method of claim 5, wherein the electrical potential bias is between about 0 V and about 0.6 V with respect to a SHE at the positive value.

### Claim 7 (depends on 4)

The method of claim 4, wherein the electrical potential bias is at the negative value for a period of time longer than the positive value to promote deposition of Cr(OH)3 on the outer surface of the aluminum alloy substrate.

### Claim 8 (depends on 7)

The method of claim 7, wherein the electrical potential bias is between about −0.8 V and about −1.8 V with respect to a SHE at the negative value.

### Claim 9 (depends on 4)

The method of claim 4, wherein a difference between the positive value and the negative value is less than about 1.5 V with respect to a SHE.

### Claim 10 (depends on 1)

The method of claim 1, wherein the chromium-containing solution is maintained at a pH between about 3.6 and about 3.9 while the electrical potential bias is maintained.

### Claim 11 (depends on 4)

The method of claim 4, further comprising:
monitoring formation of the trivalent chromium coating using in situ spectroscopic ellipsometry; and
modulating the electrical potential bias between the positive value and the negative value depending on results obtained from the spectroscopic ellipsometry.

### Claim 12

A method for forming a trivalent chromium coating on a metal substrate, the method comprising:
adding a chromium-containing solution to a vessel;
immersing the metal substrate in the chromium-containing solution;
immersing a counter electrode in the chromium-containing solution; and
modulating an electrical potential difference between the metal substrate and the counter electrode to form a trivalent chromium coating on an outer surface of the metal substrate.

### Claim 13 (depends on 12)

The method of claim 12, wherein the electrical potential difference varies between a positive value and a negative value.

### Claim 14 (depends on 12)

The method of claim 12, wherein the electrical potential difference with respect to the metal substrate is at the positive value for a period of time longer than the negative value to promote dissolution of Al3+ ions from the outer surface of the aluminum alloy substrate and promote deposition of ZrO2 or TiO2 on the outer surface of the aluminum alloy substrate.

### Claim 15 (depends on 12)

The method of claim 12, wherein the electrical potential difference with respect to the metal substrate is at the negative value for a period of time longer than the positive value to promote deposition of Cr(OH)3 on the outer surface of the aluminum alloy substrate.