# US 2015/0101710 A1 · Method for Low-Pressure Carbonitriding Using a Reduced Temperature Gradient in an Initial Nitridation Phase

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0101710 A1
- Document ID: US20150101710A1
- Status: Published application
- Kind: A1
- Application number: 14/354,358
- Filed: 2012-10-08
- Published: 2015-04-16
- Earliest claimed: 2011-10-31
- Assignees: EMC Technologies, Inc.
- Applicants: ECM Technologies
- Inventors: Philippe Lapierre; Jerome Lardinois; Yves Giraud; Alfred Rallo
- Web page: https://patentgrep.com/patent/US20150101710A1

## CPC

- C23C 8/32: of ferrous surfaces
- C21D 1/18: Hardening (C21D1/02 takes precedence); Quenching with or without subsequent tempering (quenching devices C21D1/62)
- C22C 38/00: Ferrous alloys, e.g. steel alloys (cast-iron alloys C22C37/00)
- C23C 8/02: Pretreatment of the material to be coated (C23C8/04 takes precedence)
- C23C 8/34: more than one element being applied in more than one step
- C23C 8/80: After-treatment
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)
- C22C: ALLOYS (treatment of alloys C21D, C22F)

## Abstract

A method for the low-pressure carbonitriding of steel parts, in particular parts used in the manufacture of automobiles, comprises a heating step that includes a simple heating phase (M) followed by an initial nitridation phase (Ni) from a temperature between 700° C. to 750° C. to a temperature between 860° and 1000° C. and carried out using a reduced temperature gradient relative to the simple heating phase. Additionally, alternate cementing (C1-Cn) and nitridation (N1-Nn) steps are performed at constant temperature, wherein the final nitridation step is accompanied with a decrease in temperature immediately before quenching (T).

## Claims

### Claim 1

A low-pressure carbonitriding method of steel parts, particularly parts used to manufacture automobile vehicles, comprising alternate cementation and nitriding steps at constant temperature, preceded by a heating step comprising a simple heating phase followed by an initial nitriding phase during which the heating is carried on, and followed by a quenching step, wherein during the initial nitriding phase, the heating is performed with a decreased temperature gradient as compared with the simple heating phase.

### Claim 2 (depends on 1)

The low-pressure carbonitriding method of claim 1, wherein the initial nitriding phase comprises a temperature stage.

### Claim 3 (depends on 1)

The low-pressure carbonitriding method of claim 1, wherein the initial nitriding phase is carried out with a temperature gradient in the range from 3.5° C./min to 16° C./min.

### Claim 4 (depends on 1)

The low-pressure carbonitriding method of claim 1, wherein the simple heating phase is carried out with a temperature gradient in the range from 8° C./min to 70° C./min.

### Claim 5 (depends on 1)

The low-pressure carbonitriding method of claim 1, wherein the initial nitriding phase is carried out from a temperature between 700° C. and 750° C., and up to a temperature between 860° C. and 1,000° C.

### Claim 6 (depends on 1)

The low-pressure carbonitriding method of claim 1, wherein the initial nitriding phase is immediately followed by a first cementation step.

### Claim 7 (depends on 1)

The low-pressure carbonitriding method of claim 1, wherein it comprises a final nitriding step accompanied by a cooling immediately before the quenching.

### Claim 8 (depends on 7)

The low-pressure carbonitriding method of claim 7, wherein the cooling is achieved down to a temperature between 900° C. and 800° C.

### Claim 9 (depends on 7)

The low-pressure carbonitriding method of claim 7, wherein the cooling is carried out with a temperature gradient between 10° C./min and 1° C./min.

### Claim 10 (depends on 7)

The low-pressure carbonitriding method of claim 7, wherein the final nitriding step comprises a temperature stage.