# US 2015/0101664 A1 · Protecting the surface of a light absorber in a photoanode

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0101664 A1
- Document ID: US20150101664A1
- Status: Published application
- Kind: A1
- Application number: 14/512,248
- Filed: 2014-10-10
- Published: 2015-04-16
- Earliest claimed: 2013-10-10
- Assignees: California Institute of Technology
- Applicants: The California Institute of Technology
- Inventors: Shu Hu; Nathan S. Lewis
- Web page: https://patentgrep.com/patent/US20150101664A1

## CPC

- C25B 1/55: Photoelectrolysis
- C25B 11/04: characterised by the material
- C25B 11/051: Electrodes formed of electrocatalysts on a substrate or carrier
- C25B: ELECTROLYTIC OR ELECTROPHORETIC PROCESSES FOR THE PRODUCTION OF COMPOUNDS OR NON-METALS; APPARATUS THEREFOR (anodic or cathodic protection C23F13/00; single-crystal growth C30B)

## Abstract

A photoanode includes a passivation layer on a light absorber. The passivation layer is more resistant to corrosion than the light absorber. The photoanode includes a surface modifying layer that is location on the passivation layer such that the passivation layer is between the light absorber and the surface modifying layer. The surface modifying layer reduces a resistance of the passivation layer to conduction of holes out of the passivation layer.

## Claims

### Claim 1

A device, comprising:
a photoanode that includes a passivation layer on a light absorber,
the passivation layer being more resistant to corrosion than the light absorber; and
the photoanode including a surface modifying layer on the passivation layer such that the passivation layer is between the light absorber and the surface modifying layer,
the surface modifying layer reducing a resistance of the passivation layer to conduction of holes out of the passivation layer.

### Claim 2 (depends on 1)

The device of claim 1, wherein the modifying layer and surface modifying layer are selected such that application of a voltage across the surface modifying and passivation layer so as to generate an anodic current through both the surface modifying layer and the passivation layer results in anodic current density that is higher for the modifying layer and the passivation layer than would result for application of the same voltage across the passivation layer without the surface modifying layer being on the passivation layer.

### Claim 3 (depends on 3)

The device of claim 3, wherein when the applied voltage is 0.3 vs. SCE, the anodic current density for the combination of the surface modifying layer and the passivation layer is at least 10 mA/cm2 higher than the current density for the passivation layer alone.

### Claim 4 (depends on 3)

The device of claim 3, wherein when the applied voltage is 0.3 V vs. SCE, the anodic current density for the combination of the surface modifying layer and the passivation layer is at least 30 mA/cm2 higher than the current density for the passivation layer alone.

### Claim 5 (depends on 3)

The device of claim 3, wherein the application of the 0.3 V across the passivation layer without the surface modifying layer being on the passivation layer results in an anodic current density of 0 mA/cm2.

### Claim 6 (depends on 1)

The device of claim 1, wherein the surface modifying layer is in ohmic contact with the passivation layer.

### Claim 7 (depends on 1)

The device of claim 1, wherein a material for the surface modifying layer mixes with the material of the passivation layer at an interface of the surface modifying layer and the passivation layer, the intermixing being such that at a distance of 3 nm into the passivation layer the molar % of the passivation layer that is the material for the surface modifying layer is at least 20%.

### Claim 8 (depends on 1)

The device of claim 1, wherein the passivation layer includes a metal oxide.

### Claim 9 (depends on 1)

The device of claim 1, wherein the passivation layer includes one or more components selected from a group consisting of TiO2, SrTiO3, SnO2, K2Ti2O5, K2Ti4O9, BaTiO3, PbTiO3, ZrO2, HfO2, SnO2, In2O3, FeOx, MnOx, NiOx, CoOx, WO3, ZnO, Ta2O5, NbOx, Al2O3, MgO, SiO2, and BiOx where x is greater than or equal to 1 and/or less than or equal to 2.

### Claim 10 (depends on 1)

The device of claim 1, wherein the surface modifying layer includes one or more components selected from the group consisting of elemental Ni, Co, Fe, Mn, Au, Ag, Ir, Ru, Rh, W, and Ti; oxides that include one or more items selected from the group consisting of Ni, Co, Fe, Mn, Au, Ag, Ir, Ru, Rh, W, and Ti; nitrides that include one or more items selected from the group consisting of Ni, Co, Fe, Mn, Au, Ag, Ir, Ru, Rh, W, and Ti; and oxynitrides that include one or more items selected from the group consisting of Ni, Co, Fe, Mn, Au, Ag, Ir, Ru, Rh, W, and Ti.

### Claim 11 (depends on 1)

The device of claim 1, wherein an oxidation catalyst is on the surface modification layer such that the surface modification layer is between the oxidation catalyst and the passivation layer.

### Claim 12 (depends on 11)

The device of claim 11, wherein the oxidation catalyst includes one or more components selected from the group consisting of elemental Ni, Co, Fe, Mn, Ir, Ru, Rh, Ta, W, and Ti; oxides that include one or more items selected from the group consisting of Ni, Co, Fe, Mn, Ir, Ru, Rh, Ta, W, and Ti.

### Claim 13 (depends on 1)

The device of claim 1, wherein the surface modification layer is positioned on a surface of the passivation layer such that the surface modification layer is not positioned on portions of the surface.

### Claim 14 (depends on 13)

The device of claim 13, wherein the surface modification layer is arranged in discrete islands on the passivation layer.

### Claim 15 (depends on 14)

The device of claim 14, wherein the islands have a diameter dimension that is in a range of 11 nm to 100 μm, an average separation between the islands is in a range of 10 nm to 500 m, and a thickness of each island of 1 nm-2 μm, the dimension being selected from the group consisting of the width, length, and diameter.

### Claim 16 (depends on 1)

The device of claim 1, wherein an aspect-ratio for the light-absorber is in a range of 5:1 to 200:1.

### Claim 17 (depends on 1)

The device of claim 1, wherein the photoanode is included in a solar fuels generator.

### Claim 18 (depends on 1)

The device of claim 1, wherein the photoanode is immersed a liquid with a basic pH.

### Claim 19 (depends on 1)

The device of claim 1, wherein passivation layer is arranged on the light absorber such that an environment in which the photoanode is located does not directly contact the light absorber.

### Claim 20 (depends on 1)

The device of claim 1, wherein the passivation layer conducts holes through defect mediated conduction.