# US 2015/0101658 A1 · Photovoltaic device and method for manufacturing same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0101658 A1
- Document ID: US20150101658A1
- Status: Published application
- Kind: A1
- Application number: 14/399,376
- Filed: 2013-04-15
- Published: 2015-04-16
- Earliest claimed: 2012-05-10
- Assignees: Sharp Kabushiki Kaisha
- Applicants: Sharp Kabushiki Kaisha
- Inventors: Kazuhito Nishimura; Yoshiyuki Nasuno; Shinya Honda; Takashi Yamada
- Web page: https://patentgrep.com/patent/US20150101658A1

## CPC

- H10F 71/1224: {comprising microcrystalline silicon}
- C23C 16/24: Deposition of silicon only
- C23C 16/509: using internal electrodes
- C23C 16/5096: {Flat-bed apparatus}
- H10F 10/166: the Group IV-IV heterojunctions being heterojunctions of crystalline and amorphous materials, e.g. silicon heterojunction [SHJ] photovoltaic cells
- H10F 10/17: Photovoltaic cells having only PIN junction potential barriers
- H10F 10/172: comprising multiple PIN junctions, e.g. tandem cells
- H10F 71/00: Manufacture or treatment of devices covered by this subclass (patterning processes to connect thin photovoltaic cells in integrated devices, or assemblies of multiple devices, having photovoltaic cells H10F19/33; manufacture or treatment of encapsulations or containers for integrated devices, or assemblies of multiple devices, having photovoltaic cells H10F19/80; manufacture or treatment of integrated devices, or assemblies of multiple devices, comprising at least one element in which radiation controls the flow of current H10F39/00)
- H10F 71/103: {including only Group IV materials}
- H10F 71/121: {The active layers comprising only Group IV materials}
- H10F 77/939: {Output lead wires or elements}
- H10P 14/24: using chemical vapour deposition [CVD]
- H10P 14/3208: {Silicon carbide}
- H10P 14/3211: {Silicon, silicon germanium or germanium}
- H10P 14/3408: {Silicon carbide}
- H10P 14/3411: {Silicon, silicon germanium or germanium}
- H10P 14/3442: {N-type}
- H10P 14/3444: {P-type}
- Y02E 10/545: Microcrystalline silicon PV cells
- Y02E 10/547: Monocrystalline silicon PV cells
- Y02E 10/548: Amorphous silicon PV cells
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- H10F: INORGANIC SEMICONDUCTOR DEVICES SENSITIVE TO INFRARED RADIATION, LIGHT, ELECTROMAGNETIC RADIATION OF SHORTER WAVELENGTH OR CORPUSCULAR RADIATION
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

A photovoltaic device (10) includes a photovoltaic layer (3) in which a p-type semiconductor layer (31), an i-type semiconductor layer (32), and an n-type semiconductor layer (33) are successively stacked. The p-type semiconductor layer (31) is formed from a p-type thin silicon films (311 to 313). The p-type thin silicon films (311 and 312) are formed by depositing silicon thin films having a p-type conductivity type and then by nitriding the silicon thin films using pulse power in which a 100 Hz to 1 kHz low-frequency pulse power is superimposed on a 1 MHz and 50 MHz high-frequency power as plasma excitation power, and using conditions in which the density of the high-frequency power is 100 to 300 mW/cm2, the pressure during plasma processing is 300 to 600 Pa, and the substrate temperature during plasma processing is 140° C. to 190° C. The p-type thin silicon film (313) is deposited under the above conditions.

## Claims

### Claim 1

A photovoltaic device that includes a photovoltaic portion that converts light to electricity, the photovoltaic device comprising:
a substrate; and
a silicon-based semiconductor layer formed with the substrate as a support base body and configuring the photovoltaic portion,
wherein the silicon-based semiconductor layer includes
a first silicon-based semiconductor layer that has a p-type conductivity type,
a second silicon-based semiconductor layer that has an n-type conductivity type, and
a third silicon-based semiconductor layer that has an i-type conductivity type, and
wherein at least one of the first and second silicon-based semiconductor layers has a structure in which a layer including nitrogen atoms is interposed in a thickness direction between layers not including nitrogen atoms or a structure in which a layer having a first nitrogen atom concentration is interposed in the thickness direction between layers having a second nitrogen atom concentration lower than the first nitrogen atom concentration.

### Claim 2 (depends on 1)

The photovoltaic device according to claim 1,
wherein the substrate includes
an insulating support body as a support body of the photovoltaic portion, and
a transparent conductive film arranged on the insulating support body in contact with the insulating support body.

### Claim 3 (depends on 2)

The photovoltaic device according to claim 2,
wherein the insulating support body is formed from a light-transmitting substrate, and
wherein the transparent conductive film is arranged between the light-transmitting substrate and the first silicon-based semiconductor layer.

### Claim 4 (depends on 2)

The photovoltaic device according to claim 2,
wherein the insulating support body is formed from a non-light-transmitting substrate, and
wherein the transparent conductive film is arranged between the non-light-transmitting substrate and the second silicon-based semiconductor layer.

### Claim 5 (depends on 1)

The photovoltaic device according to claim 1,
wherein the substrate is formed from a silicon substrate, and
wherein the first silicon-based semiconductor layer is arranged on the opposite side to the second silicon-based semiconductor layer with respect to the silicon substrate.

### Claim 6 (depends on 1)

The photovoltaic device according to claim 1,
wherein the substrate is formed from a silicon substrate,
wherein the first silicon-based semiconductor layer is arranged on one side of the silicon substrate, and
wherein the second silicon-based semiconductor layer is arranged neighboring the first silicon-based semiconductor layer in the in-plane direction of the silicon substrate.

### Claim 7

A method for manufacturing a photovoltaic device by a plasma CVD method, the method comprising:
a first plasma processing step of depositing the first silicon-based semiconductor layer that has a p-type conductivity type or an n-type conductivity type above the substrate;
a second plasma processing step of irradiating the first silicon-based semiconductor layer with plasma in which a raw material gas including nitrogen atoms is excited; and
a third plasma processing step of depositing a second silicon-based semiconductor layer that has the same conductivity type as the first silicon-based semiconductor layer on the first silicon-based semiconductor layer,
wherein the second plasma processing step uses pulsed power in which a low frequency pulse power of 100 Hz to 1 kHz is superimposed on a high frequency power of 1 MHz to 50 MHz as a plasma excitation power,
wherein the density of the high frequency power is 100 mW/cm2 to 300 mW/cm2,
wherein the pressure during the plasma processing is 300 Pa to 600 Pa, and
wherein the substrate temperature during plasma processing is 140° C. to 190° C.

### Claim 8 (depends on 7)

The method for manufacturing a photovoltaic device according to claim 7,
wherein the duty ratio of the low frequency pulse is 0.1 to 0.5.

### Claim 9 (depends on 7)

The method for manufacturing a photovoltaic device according to claim 7,
wherein the plasma irradiation time in the second plasma processing step is 5 to 60 seconds.

### Claim 10 (depends on 7)

The method for manufacturing a photovoltaic device according to claim 7,
wherein the first to third plasma processing steps are executed in the same processing chamber.

### Claim 11 (depends on 7)

The method for manufacturing a photovoltaic device according to claim 7,
wherein the first to third plasma processing steps are executed at the same processing pressure.

### Claim 12 (depends on 7)

The method for manufacturing a photovoltaic device according to claim 7,
wherein the first and second silicon-based semiconductor layers are microcrystalline silicon semiconductor layers.

### Claim 13 (depends on 7)

The method for manufacturing a photovoltaic device according to claim 7,
wherein a silicon-based semiconductor layer having a p-type conductivity type is deposited in the first and third plasma processing steps.

### Claim 14 (depends on 7)

The method for manufacturing a photovoltaic device according to claim 7, further comprising:
a fourth plasma processing step, in which a microcrystalline silicon having an intrinsic conductivity type is deposited, after the silicon-based semiconductor layer having a p-type conductivity type is deposited by the first to third plasma processing steps.

### Claim 15 (depends on 7)

The method for manufacturing a photovoltaic device according to claim 7,
wherein the pin-type photovoltaic portion that has a p-type conductivity type layer manufactured using the first to third plasma processing steps is manufactured in the same processing chamber.

### Claim 16 (depends on 7)

The method for manufacturing a photovoltaic device according to claim 7,
wherein the processing chamber in which the plasma processing step is executed has a pair of a cathode electrode and an anode electrode that are supplied with the plasma excitation power, and
wherein the size of the cathode electrode and the anode electrode is 1 m2 to 3 m2 with respect to one photovoltaic portion.

### Claim 17 (depends on 7)

The method for manufacturing a photovoltaic device according to claim 7,
wherein the processing chamber in which the plasma processing step is executed has a plurality of pairs of cathode electrodes and anode electrodes, and
wherein one power source supplies plasma excitation power to the plurality of pairs of cathode electrodes and the anode electrodes.
