# US 2015/0101526 A1 · Method for tailoring the dopant profile in a laser crystal using zone processing

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0101526 A1
- Document ID: US20150101526A1
- Status: Published application
- Kind: A1
- Application number: 14/487,295
- Filed: 2014-09-16
- Published: 2015-04-16
- Earliest claimed: 2011-08-16
- Assignees: Raytheon Company
- Applicants: Raytheòn Company
- Inventors: Robert W. Byren
- Web page: https://patentgrep.com/patent/US20150101526A1

## CPC

- C30B 13/20: by induction, e.g. hot wire technique (C30B13/18 takes precedence)
- C30B 13/10: with addition of doping materials
- C30B 13/24: using electromagnetic waves
- C30B 29/12: Halides
- C30B 29/28: with formula A3Me5O12 wherein A is a rare earth metal and Me is Fe, Ga, Sc, Cr, Co or Al, e.g. garnets
- H01S 3/0617: {having a varying composition or cross-section in a specific direction}
- H01S 3/1611: {neodymium}
- H01S 3/1643: {YAG}
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR
- H01S: DEVICES USING THE PROCESS OF LIGHT AMPLIFICATION BY STIMULATED EMISSION OF RADIATION [LASER] TO AMPLIFY OR GENERATE LIGHT; DEVICES USING STIMULATED EMISSION OF ELECTROMAGNETIC RADIATION IN WAVE RANGES OTHER THAN OPTICAL

## Abstract

A lasing medium having a tailored dopant concentration and a method of fabrication thereof is disclosed. The lasing medium has a single crystal having a continuous body having a selected length, wherein the crystal comprises dopant distributed along the length of the body to define a dopant concentration profile. In one embodiment, the dopant concentration profile results in a uniform heating profile. A method of fabricating a laser crystal having a tailored dopant concentration profile includes arranging a plurality of polycrystalline segments together to form an ingot, the polycrystalline segments each having dopant distributed, providing a crystal seed at a first end of the ingot, and moving a heating element along the ingot starting from the first end to a second end of the ingot, the moving heating element creating a moving molten region within the ingot while passing therealong.

## Claims

### Claim 1

A method comprising:
arranging multiple polycrystalline segments together to form an ingot, the polycrystalline segments each having dopant distributed therein;
providing a crystal seed at a first end of the ingot; and
moving a heating element along the ingot from the first end to a second end of the ingot so as to create a single crystal, the moving heating element creating a moving molten region within the ingot while passing therealong;
wherein the single crystal represents a continuous body with a selected length, the dopant distributed along the length of the continuous body to define a tailored non-uniform dopant concentration profile.

### Claim 2 (depends on 1)

The method of claim 1, wherein the dopant comprises neodymium, ytterbium, erbium, holmium, or a combination thereof.

### Claim 3 (depends on 1)

The method of claim 1, wherein the heating element uses radio frequency (RF) induction.

### Claim 4 (depends on 1)

The method of claim 1, wherein each of the segments has a different dopant concentration.

### Claim 5 (depends on 1)

The method of claim 1, wherein each of the segments has a different length.

### Claim 6 (depends on 1)

The method of claim 1, wherein the seed crystal comprises a dopant concentration equal to a target concentration at the first end of the ingot.

### Claim 7 (depends on 1)

The method of claim 1, wherein the segment at the first end of the ingot has a higher dopant concentration than the segment at the second end of the ingot.

### Claim 8 (depends on 1)

The method of claim 1, wherein moving the heating element along the ingot comprises surrounding a portion of the ingot with the heating element.

### Claim 9 (depends on 1)

The method of claim 1, wherein interfaces between the moving molten region and the segments of the ingot are substantially normal to an axis of the ingot.

### Claim 10 (depends on 1)

The method of claim 1, wherein the crystal comprises Y3AI5O12, YLiF4, or Gd3Ga5O12.

### Claim at position 11

-19. (canceled)

### Claim 20

A method comprising:
arranging one or more polycrystalline segments to form an ingot, the one or more polycrystalline segments comprising at least one dopant;
providing a crystal seed at a first end of the ingot; and
moving a heating element along the ingot from the first end to a second end of the ingot so as to create a single crystal, the moving heating element creating a moving molten region within the ingot while passing along the ingot;
wherein the single crystal represents a continuous body with a selected length, the continuous body having a common crystal structure and a common lattice orientation as the crystal seed, the at least one dopant distributed along the length of the continuous body to define a tailored non-uniform dopant concentration profile.

### Claim 21 (depends on 20)

The method of claim 20, wherein the dopant comprises neodymium, ytterbium, erbium, holmium, or a combination thereof.

### Claim 22 (depends on 20)

The method of claim 20, wherein the heating element uses radio frequency (RF) induction.

### Claim 23 (depends on 20)

The method of claim 20, wherein:
the one or more polycrystalline segments comprise multiple polycrystalline segments; and
at least one of:
each of the segments has a different dopant concentration; or
each of the segments has a different length.

### Claim 24 (depends on 20)

The method of claim 20, wherein the seed crystal comprises a dopant concentration equal to a target concentration at the first end of the ingot.

### Claim 25 (depends on 20)

The method of claim 20, wherein:
the one or more polycrystalline segments comprise multiple polycrystalline segments; and
the segment at the first end of the ingot has a higher dopant concentration than the segment at the second end of the ingot.

### Claim 26 (depends on 20)

The method of claim 20, wherein moving the heating element along the ingot comprises surrounding a portion of the ingot with the heating element.

### Claim 27 (depends on 20)

The method of claim 20, wherein:
the one or more polycrystalline segments comprise multiple polycrystalline segments; and
interfaces between the moving molten region and the segments are substantially normal to an axis of the ingot.

### Claim 28 (depends on 20)

The method of claim 20, wherein the crystal comprises Y3AI5O12, YLiF4, or Gd3Ga5O12.

### Claim 29

A method comprising:
obtaining an ingot comprising one or more polycrystalline segments, the one or more polycrystalline segments comprising at least one dopant;
providing a crystal seed at one end of the ingot; and
moving a heating element along the ingot so as to create a single crystal, the moving heating element creating a moving molten region within the ingot while passing along the ingot;
wherein the single crystal represents a continuous body with a selected length, the continuous body having a common crystal structure and a common lattice orientation as the crystal seed, the at least one dopant distributed along the length of the continuous body to define a tailored non-uniform dopant concentration profile.