# US 2015/0101453 A1 · Fluoride-free Continuous Casting Mold Flux For Low-carbon Steel

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0101453 A1
- Document ID: US20150101453A1
- Status: Published application
- Kind: A1
- Application number: 14/386,763
- Filed: 2013-03-20
- Published: 2015-04-16
- Earliest claimed: 2012-03-22
- Assignees: Baoshan Iron & Steel Co., Ltd.
- Applicants: Baoshan Iron & Steel Co., Ltd.
- Inventors: Chen Zhang; Dexiang Cai; Jianguo Shen; Feng Mei
- Web page: https://patentgrep.com/patent/US20150101453A1

## CPC

- B22D 11/11: Treating the molten metal
- B22D 11/103: Distributing the molten metal, e.g. using runners, floats, distributors
- B22D: CASTING OF METALS; CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES (shaping of plastics or substances in a plastic state B29C; metallurgical processing, selection of substances to be added to metal C21, C22)

## Abstract

The invention provides a fluoride-free continuous casting mold flux for low-carbon steel, comprising, based on weight, Na2O 5-10%, MgO 3-10%, MnO 3-10%, B2O3 3-10%, Al2O3≦6%, Li2O<3%, C 1-3%, and the balance of CaO and SiO2 as well as inevitable impurities, wherein the ratio of CaO/SiO2 is 0.8˜1.3. The mold flux has a melting point of 95˜1150° C., a viscosity at 1300° C. of 0.1-0.3 Pa·s, and a crystallization rate of 10-50% as determined according to the method described in the specification for examining crystallization property. The boron-containing, fluoride-free flux developed according to the invention has a moderate crystallization rate, can be used in a crystallizer to control transfer of heat from molten steel effectively, and has been applied successfully in a low-carbon steel slab conticaster with a metallurgical effect that arrives at the level of a traditional fluoride-containing flux to full extent.

## Claims

### Claim 1

A fluoride-free continuous casting mold flux for low-carbon steel, comprising, based on weight, Na2O 5-10%, MgO 3-10%, MnO 3-10%, B2O3 3-10%, Al2O3≦6%, Li2O<3%, C 1-3%, and the balance of CaO and SiO2 as well as inevitable impurities, wherein the ratio of CaO/SiO2 is 0.8˜1.3.

### Claim 2 (depends on 1)

The fluoride-free continuous casting mold flux for low-carbon steel according to claim 1, wherein 50 g of the mold flux is melted at 1350° C. and then poured into a steel crucible to be cooled naturally, followed by characterization of the crystallization rate of the mold flux by the proportion of crystals at a section, wherein the crystallization rate of the mold flux ranges between 10 and 50%.

### Claim 3 (depends on 1)

The fluoride-free continuous casting mold flux for low-carbon steel according to claim 1, wherein the content of Na2O is 6-9.5%.

### Claim 4 (depends on 1)

The fluoride-free continuous casting mold flux for low-carbon steel according to claim 1, wherein the content of MgO is 5-9%.

### Claim 5 (depends on 1)

The fluoride-free continuous casting mold flux for low-carbon steel according to claim 1, wherein the content of MnO is 5-10%.

### Claim 6 (depends on 1)

The fluoride-free continuous casting mold flux for low-carbon steel according to claim 1, wherein the content of B2O3 is 4-10%.

### Claim 7 (depends on 1)

The fluoride-free continuous casting mold flux for low-carbon steel according to claim 1, wherein the content of Al2O3 is 0.5-6%.

### Claim 8 (depends on 1)

The fluoride-free continuous casting mold flux for low-carbon steel according to claim 1, wherein the content of Li2O is ≦2.5%.

### Claim 9 (depends on 1)

The fluoride-free continuous casting mold flux for low-carbon steel according to claim 1, wherein the content of C is 1.3-2.8%.

### Claim 10 (depends on 1)

The fluoride-free continuous casting mold flux for low-carbon steel according to claim 1, wherein the mold flux has a melting point of 950-150° C. and a viscosity at 1300° C. of 0.1-0.3 Pa·s.