# US 2015/0101381 A1 · Method of cold rolling a seamless pipe

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0101381 A1
- Document ID: US20150101381A1
- Status: Published application
- Kind: A1
- Application number: 14/391,808
- Filed: 2013-04-05
- Published: 2015-04-16
- Earliest claimed: 2012-04-12
- Assignees: Nippon Steel & Sumitomo Metal Corporation
- Applicants: Nippon Steel & Sumitomo Metal Corporation
- Inventors: Osamu Miyahara
- Web page: https://patentgrep.com/patent/US20150101381A1

## CPC

- B21B 21/00: Pilgrim-step tube-rolling {, i.e. pilger mills}
- B21B 23/00: Tube-rolling not restricted to methods provided for in only one of groups B21B17/00, B21B19/00, B21B21/00, e.g. combined processes {planetary tube rolling, auxiliary arrangements, e.g. lubricating, special tube blanks, continuous casting combined with tube rolling}(B21B25/00 takes precedence)
- B21B 2261/04: Thickness, gauge
- B21B 2263/20: End shape; fish tail; tongue
- B21B: ROLLING OF METAL (auxiliary operations used in connection with metal-working operations covered in B21, see B21C; bending by rolling B21D; manufacture of particular objects, e.g. screws, wheels, rings, barrels, balls, by rolling B21H; pressure welding by means of a rolling mill B23K20/04)

## Abstract

In performing cold rolling on a seamless pipe as a mother pipe, it is possible to inhibit the generation of metal chips from the end portions of the mother pipe, and to prevent the formation of indentations therein that may be caused by the metal chips to thereby provide good surface appearance. This is made possible by using a mother pipe (1) having end portions at the cold rolling starting side and finishing side that have been R-chamfered, at each outer edge and at each inner edge, such that (T0−T1)/2≦R≦T0/2 is satisfied, where R is a radius (mm) of the R-chamfer on the outer edges and the inner edges of the end portions, T0 is a wall thickness of the mother pipe, and T1 is a wall thickness of the pipe after cold rolling.

## Claims

### Claim 1

A method of cold rolling a seamless pipe, including cold rolling a seamless pipe as a mother pipe using a Pilger mill, the method comprising:
using a mother pipe having end portions at a cold rolling starting side and at a cold rolling finishing side, the end portions being R-chamfered at outer edges thereof and inner edges thereof such that the following formula (1) is satisfied:
(T0−T1)/2≦R≦T0/2 . . . (1)
where R is a radius (mm) of the R-chamfer on the outer edges and the inner edges of the end portions, T0 is a wall thickness (mm) of the mother pipe, and T1 is a wall thickness (mm) of the pipe after cold rolling.