# US 2015/0090928 A1 · Cathode materials for lithium battery having higher performance

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0090928 A1
- Document ID: US20150090928A1
- Status: Published application
- Kind: A1
- Application number: 14/565,558
- Filed: 2014-12-10
- Published: 2015-04-02
- Earliest claimed: 2006-03-20
- Assignees: LG Chem, Ltd.
- Applicants: LG Chem, Ltd.
- Inventors: Jens M. Paulsen; Hong-Kyu Park; Sun Sik Shin; Sinyoung Park; Hyeyun Cha
- Web page: https://patentgrep.com/patent/US20150090928A1

## CPC

- H01M 4/525: of mixed oxides or hydroxides containing iron, cobalt or nickel for inserting or intercalating light metals, e.g. LiNiO2, LiCoO2 or LiCoOxFy
- C01G 53/502: containing lithium and cobalt
- C01G 53/504: with the molar ratio of nickel with respect to all the metals other than alkali metals higher than or equal to 0.5, e.g. Li(MzNixCoyMn1-x-y-z)O2 with x ≥ 0.5
- H01M 4/505: of mixed oxides or hydroxides containing manganese for inserting or intercalating light metals, e.g. LiMn2O4 or LiMn2OxFy
- C01P 2006/40: Electric properties
- Y02E 60/10: Energy storage using batteries
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C01G: COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSES C01D OR C01F (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts or peroxyacids C01B15/00; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium, or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds containing nitrogen, other non-metals and metal C01B21/082}; metal amides C01B21/092; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanamide C01C3/16; thiocyanates C01C3/20)
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

Provided is a method for preparing the heat-treated mixture of an oxide powder (a) represented by Formula I and an oxide powder (b) represented by Formula II, LiCoO2 (I) LizMO2 (II) wherein 0.95<z<1.1; M=Ni1-x-yMnxCoy, 0<y<0.5, and a ratio of Mn to Ni (x/(1-x-y)) is in the range of 0.4 to 1.1, comprising mixing (i) a Co-containing precursor, (ii) an Mn—Ni-containing precursor, and (iii) optionally, an Li-containing precursor, and heat-treating the mixture at a temperature of more than 400° C. under an oxygen-containing atmosphere.

## Claims

### Claim 1

A method for preparing the heat-treated mixture of an oxide powder (a) represented by Formula I and an oxide powder (b) represented by Formula II, wherein a mixing ratio of the oxide powder (a):oxide powder (b) is in the range of 30:70 to 90:10, the oxide powder (a) is monolithic particles having a D50 of more than 10 μm, and the oxide powder (b) is agglomerated particles having a D50 of less than 10 μm, and heat treatment is carried out at a temperature of 400° C. or higher:
LiCoO2 (I)
LizMO2 (II)
wherein 0.95<z<1.1; M=Ni1-x-yMnxCoy, 0<y<0.5, and a ratio of Mn to Ni (x/(1-x-y)) is in the range of 0.4 to 1.1, comprising mixing (i) a Co-containing precursor, (ii) an Mn—Ni-containing precursor, and (iii) optionally, an Li-containing precursor, and heat-treating the mixture at a temperature of more than 400° C. under an oxygen-containing atmosphere.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the heat treatment is carried out at a temperature of 700 to 1050° C. in air.

### Claim 3 (depends on 2)

The method according to claim 2, wherein the heat treatment is carried out at a temperature of 900 to 1000° C. in air.

### Claim 4 (depends on 1)

The method according to claim 1, wherein the Co-containing precursor is selected from the group consisting of a cobalt oxide, a cobalt hydroxide, a cobalt oxohydroxide, a cobalt carbonate, a cobalt carbonate-hydroxide, a lithium cobalt oxide and any combination thereof;
the Mn—Ni-containing precursor is selected from the group consisting of a mixed oxide, a mixed hydroxide, a mixed oxohydroxide, a mixed carbonate, a mixed carbonate-hydroxide, a lithium-mixed transition metal oxide and any combination thereof; and
the Li-containing precursor is LiCO3.

### Claim 5 (depends on 1)

The method according to claim 1, wherein the Co-containing precursor is Co3O4 or LiCoO2.

### Claim 6 (depends on 1)

The method according to claim 1, wherein the Mn—Ni-containing precursor is a compound of Formula MOOH (M=Ni1-x-yMnxCoy: and x, y and z are as defined above) or a lithium-mixed transition metal oxide of Formula LizNi1-x-yMnxCoyO2 (x, y and z are as defined above).

### Claim 7 (depends on 1)

The method according to claim 1, wherein the Co-containing precursor has a D50 of more than 10 μm, and the Mn—Ni containing precursor has a D50 of less than 10 μm.