# US 2015/0090419 A1 · Method for Manufacturing a High-Strength Blade-Type Golf Iron Head with a Thin Blade

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0090419 A1
- Document ID: US20150090419A1
- Status: Published application
- Kind: A1
- Application number: 14/452,602
- Filed: 2014-08-06
- Published: 2015-04-02
- Earliest claimed: 2013-09-30
- Assignees: Fusheng Precision Co., Ltd.
- Applicants: Fusheng Precision Co., Ltd.
- Inventors: Chien-Liang Li
- Web page: https://patentgrep.com/patent/US20150090419A1

## CPC

- A63B 53/047: {iron-type}
- B22C 9/043: {Removing the consumable pattern}
- B22D 13/06: of solid or hollow bodies in moulds rotating around an axis arranged outside the mould
- B22D 13/101: {Moulds}
- B22D 13/108: {Removing of casting}
- A63B 53/0408: {characterised by specific dimensions, e.g. thickness}
- A63B: APPARATUS FOR PHYSICAL TRAINING, GYMNASTICS, SWIMMING, CLIMBING, OR FENCING; BALL GAMES; TRAINING EQUIPMENT (apparatus for passive exercising, massage A61H)
- B22C: FOUNDRY MOULDING (moulding refractory materials in general B28B)
- B22D: CASTING OF METALS; CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES (shaping of plastics or substances in a plastic state B29C; metallurgical processing, selection of substances to be added to metal C21, C22)

## Abstract

A method for manufacturing a high-strength blade-type golf iron head with a thin blade includes placing a shell mold onto a rotary table. At least one metal ingot is placed into a crucible portion of the shell mold and is heated to melt in a vacuum environment. The rotary table rotates to cause the molten metal to flow into a cavity portion of the shell mold. The rotating shaft is slowly stopped, and the shell mold is removed after pouring. The shell mold is destroyed after the molten metal cools and solidifies, obtaining a casting. A cast product portion is separated from the casting to obtain at least one blade-type golf iron head having the blade with a minimum thickness of 3.5-5.0 mm. The weight of the blade-type golf iron head is reduced by 0.9-2.5%, and the center of gravity of the blade-type golf iron head is lowered by 0.2-0.75 mm.

## Claims

### Claim 1

A method for manufacturing a high-strength blade-type golf iron head with a thin blade comprising:
placing a shell mold onto a rotary table, with the shell mold including a crucible portion and a cavity portion in communication with the crucible portion, with the rotary table coupled to a rotating shaft rotatable about a rotating axis;
placing at least one metal ingot into the crucible portion of the shell mold, and melting the at least one metal ingot into molten metal in a vacuum environment;
driving the rotating shaft to rotate the rotary table, causing the molten metal to flow into the cavity portion of the shell mold;
slowly stopping the rotating shaft and removing the shell mold after pouring;
destroying the shell mold after the molten metal cools and solidifies, obtaining a casting having a cast product portion; and
separating the cast product portion from the casting to obtain at least one blade-type golf iron head having the blade with a minimum thickness of 3.5-5.0 mm, with a weight of the blade-type golf iron head reduced by 0.9-2.5%, and with the center of gravity of the blade-type golf iron head lowered by 0.2-0.75 mm.

### Claim 2 (depends on 1)

The method for manufacturing a high-strength blade-type golf iron head with a thin blade as claimed in claim 1, with the at least one metal ingot including a metal ingot of a high-strength steel alloy, and with the metal ingot having a composition identical to a composition of a high-strength blade-type golf iron head to be produced.

### Claim 3 (depends on 1)

The method for manufacturing a high-strength blade-type golf iron head with a thin blade as claimed in claim 1, with the at least one metal ingot including a plurality of metal ingots, with a composition of the molten metal of the plurality of metal ingots being identical to a composition of a high-strength blade-type golf iron head to be produced.

### Claim 4 (depends on 1)

The method for manufacturing a high-strength blade-type golf iron head with a thin blade as claimed in claim 1, further comprising forming the shell mold, with forming the shell mold including:
preparing a wax blank including a crucible blank and a casting blank, with the crucible blank including a first connecting portion on an outer periphery of the crucible blank, with the casting blank including a second connecting portion, with the first connecting portion and the second connecting portion integrally connected to each other;
forming an enveloping layer on an outer surface of the wax blank;
heating the wax blank and the enveloping layer to melt the wax out; and
sintering the dewaxed enveloping layer at a high temperature to form the shell mold including the crucible portion and the cavity portion integral with the crucible portion.

### Claim 5 (depends on 1)

The method for manufacturing a high-strength blade-type golf iron head with a thin blade as claimed in claim 1, wherein the shell mold includes a surface layer of a fire-resistant material including zirconium silicate, yttrium oxide, stabilized zirconium oxide, or aluminum oxide.

### Claim 6 (depends on 1)

The method for manufacturing a high-strength blade-type golf iron head with a thin blade as claimed in claim 1, wherein the shell mold includes a back layer of a material including a mullite compound containing 45-60 wt % of aluminum oxide and 55-40 wt % of silicon oxide.

### Claim 7 (depends on 1)