# US 2015/0084062 A1 · Monolithically integrated vertical power transistor and bypass diode

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0084062 A1
- Document ID: US20150084062A1
- Status: Published application
- Kind: A1
- Application number: 14/255,405
- Filed: 2014-04-17
- Published: 2015-03-26
- Earliest claimed: 2013-09-20
- Assignees: Cree, Inc.
- Applicants: Cree, Inc.
- Inventors: Vipindas Pala; Lin Cheng; Anant Kumar Agarwal; John Williams Palmour; Edward Robert Van Brunt
- Web page: https://patentgrep.com/patent/US20150084062A1

## CPC

- H10D 84/146: {the built-in components being Schottky barrier diodes}
- H10D 12/031: {of IGBTs}
- H10D 30/0291: {of vertical DMOS [VDMOS] FETs}
- H10D 30/0297: {using recessing of the gate electrodes, e.g. to form trench gate electrodes}
- H10D 30/635: {having no inversion channels, e.g. vertical accumulation channel FETs [ACCUFET] or normally-on vertical IGFETs}
- H10D 30/668: {having trench gate electrodes, e.g. UMOS transistors}
- H10D 62/157: {Impurity concentrations or distributions}
- H10D 62/393: {Body regions of DMOS transistors or IGBTs (cell layout of DMOS H10D62/127)}
- H10D 62/8325: {Silicon carbide}
- H10D 84/156: {the built-in components being Schottky barrier diodes}
- H10P 30/204: {into Group IV semiconductors}
- H10P 30/2042: {into crystalline silicon carbide}
- H10P 30/208: {of electrically inactive species}
- H10P 30/21: {of electrically active species}
- H10D 8/411: {PN diodes having planar bodies}
- H10D 8/60: Schottky-barrier diodes
- H10D 62/106: {having supplementary regions doped oppositely to or in rectifying contact with regions of the semiconductor bodies, e.g. guard rings with PN or Schottky junctions}
- H10D 62/60: Impurity distributions or concentrations
- H10D 64/64: Electrodes comprising a Schottky barrier to a semiconductor
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A vertical field-effect transistor (FET) device includes a monolithically integrated bypass diode connected between a source contact and a drain contact of the vertical FET device. According to one embodiment, the vertical FET device includes a pair of junction implants separated by a junction field-effect transistor (JFET) region. At least one of the junction implants of the vertical FET device includes a deep well region that is shared with the integrated bypass diode, such that the shared deep well region functions as both a source junction in the vertical FET device and a junction barrier region in the integrated bypass diode. The vertical FET device and the integrated bypass diode may include a substrate, a drift layer over the substrate, and a spreading layer over the drift layer, such that the junction implants of the vertical FET device are formed in the spreading layer.

## Claims

### Claim 1

A semiconductor device comprising:
a substrate;
a drift layer over the substrate;
a spreading layer over the drift layer;
a pair of junction barrier regions in the spreading layer and opposite the drift layer;
an anode contact over the surface of the spreading layer opposite the drift layer; and
a cathode contact over the surface of the substrate opposite the drift layer.

### Claim 2 (depends on 1)

The semiconductor device of claim 1 wherein each one of the pair of junction barrier regions is laterally separated from the other.

### Claim 3 (depends on 1)

The semiconductor device of claim 1 wherein:
the substrate is a heavily doped N layer;
the drift layer is a lightly doped N layer; and
the spreading layer is a heavily doped N layer, such that the respective doping concentrations of each one of the substrate, the drift layer, and the spreading layer are different from one another.

### Claim 4 (depends on 3)

The semiconductor device of claim 3 wherein:
the doping concentration of the drift layer is between about 6E15 cm−3 and 1.5E16 cm−3; and
the doping concentration of the spreading layer is between about 5E16 cm−3 and 2E17 cm−3.

### Claim 5 (depends on 4)

The semiconductor device of claim 4 wherein each one of the pair of junction barrier regions is a heavily doped P region.

### Claim 6 (depends on 5)

The semiconductor device of claim 5 wherein each one of the pair of junction barrier regions has a doping concentration between about 5E17 cm−3 and 1E20 cm−3.

### Claim 7 (depends on 3)

The semiconductor device of claim 3 wherein the spreading layer comprises multiple layers.

### Claim 8 (depends on 7)

The semiconductor device of claim 7 wherein each layer of the spreading layer has a different doping concentration.

### Claim 9 (depends on 8)

The semiconductor device of claim 8 wherein:
a first layer of the spreading layer opposite the drift layer has a doping concentration of about 2E17 cm−3;
a second layer of the spreading layer adjacent to the drift layer has a doping concentration of about 5E16 cm−3; and
the doping concentration of each additional layer of the spreading layer between the first layer and the second layer decreases in proportion to the distance of the layer from the first layer, starting at the doping concentration of the first layer, and ending at the doping concentration of the second layer.

### Claim 10 (depends on 3)

The semiconductor device of claim 3 wherein the doping concentration of the spreading layer is graded.

### Claim 11 (depends on 10)

The semiconductor device of claim 10 wherein a portion of the spreading layer closest to the drift layer has a doping concentration of about 5E16 cm−3 that is gradated as the spreading layer extends away from the drift layer to a doping concentration of about 2E17 cm−3.

### Claim 12 (depends on 1)

The semiconductor device of claim 1 wherein the semiconductor device is a silicon carbide (SiC) device.

### Claim 13 (depends on 1)

The semiconductor device of claim 1 wherein the anode contact comprises a low barrier height Schottky metal.

### Claim 14 (depends on 13)

The semiconductor device of claim 13 wherein the anode contact comprises Tantalum.

### Claim 15

A method of manufacturing a semiconductor device comprising:
growing a drift layer on a substrate;
growing a spreading layer over the drift layer;
implanting a pair of junction barrier regions in the spreading layer and opposite the drift layer;
providing an anode contact over the surface of the spreading layer opposite the substrate; and
providing a cathode contact over a surface of the substrate opposite the drift layer.

### Claim 16 (depends on 15)

The method of claim 15 wherein each one of the pair of junction barrier regions is laterally separated from the other.

### Claim 17 (depends on 15)

The method of claim 15 wherein:
the substrate is a heavily doped N layer;
the drift layer is a lightly doped N layer; and
the spreading layer is a heavily doped N layer, such that the respective doping concentrations of each one of the substrate, the drift layer, and the spreading layer are different from one another.

### Claim 18 (depends on 15)

The method of claim 15 wherein:
the doping concentration of the drift layer is between about 6E15 cm−3 and 1.5E16 cm−3; and
the doping concentration of the spreading layer is between about 5E16 cm−3 and 2E17 cm−3.

### Claim 19 (depends on 17)

The method of claim 17 wherein each one of the pair of junction barrier regions is a heavily doped P region.

### Claim 20 (depends on 19)

The method of claim 19 wherein each one of the pair of junction barrier regions has a doping concentration between about 5E17 cm−3 and 1E20 cm−3.

### Claim 21 (depends on 17)

The method of claim 17 wherein the spreading layer comprises multiple layers.

### Claim 22 (depends on 21)

The method of claim 21 wherein each layer of the spreading layer has a different doping concentration.

### Claim 23 (depends on 22)

The method of claim 22 wherein:
a first layer of the spreading layer opposite the drift layer has a doping concentration of about 2E17 cm−3;
a second layer of the spreading layer adjacent to the drift layer has a doping concentration of about 5E16 cm−3; and
the doping concentration of each additional layer of the spreading layer between the first layer and the second layer decreases in proportion to the distance of the layer from the first layer, starting at the doping concentration of the first layer, and ending at the doping concentration of the second layer.

### Claim 24 (depends on 17)

The method of claim 17 wherein the doping concentration of the spreading layer is graded.

### Claim 25 (depends on 24)

The method of claim 24 wherein the portion of a spreading layer closest to the drift layer has a doping concentration of about 5E16 cm−3 that is graduated as the spreading layer extends away from the drift layer to a doping concentration of about 2E17 cm−3.

### Claim 26 (depends on 15)

The method of claim 15 wherein the semiconductor device is a silicon carbide (SiC) device.

### Claim 27 (depends on 15)

The method of claim 15 wherein the anode contact comprises a low barrier height Schottky metal.

### Claim 28 (depends on 27)

The method of claim 27 wherein the anode contact comprises Tantalum.