# US 2015/0084061 A1 · Semiconductor photo-detecting device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0084061 A1
- Document ID: US20150084061A1
- Status: Published application
- Kind: A1
- Application number: 14/496,998
- Filed: 2014-09-25
- Published: 2015-03-26
- Earliest claimed: 2013-09-25
- Assignees: Seoul Viosys Co., Ltd.
- Applicants: Seoul Viosys Co., Ltd.
- Inventors: Ki Yon PARK; Hwa Mok KIM; Kyu-Ho LEE; Sung Hyun LEE; Hyung Kyu KIM
- Web page: https://patentgrep.com/patent/US20150084061A1

## CPC

- H10F 30/227: the potential barrier being a Schottky barrier
- H10F 71/1274: {comprising nitrides, e.g. InGaN or InGaAlN}
- H10F 71/1278: {comprising nitrides, e.g. GaN}
- H10F 77/1246: {III-V nitrides, e.g. GaN}
- H10F 77/12485: {comprising nitride compounds, e.g. InGaN}
- Y02E 10/544: Solar cells from Group III-V materials
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- H10F: INORGANIC SEMICONDUCTOR DEVICES SENSITIVE TO INFRARED RADIATION, LIGHT, ELECTROMAGNETIC RADIATION OF SHORTER WAVELENGTH OR CORPUSCULAR RADIATION
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

A photo-detecting device includes a first nitride layer, a low-current blocking layer disposed on the first nitride layer, a light absorption layer disposed on the low-current blocking layer, and a Schottky junction layer disposed on the light-absorption layer. The low-current blocking layer includes a multilayer structure.

## Claims

### Claim 1

A photo-detecting device, comprising:
a first nitride layer;
a low-current blocking layer disposed on the first nitride layer, the low-current blocking layer comprising a multilayer structure;
a light absorption layer disposed on the low-current blocking layer; and
a Schottky junction layer disposed on the light-absorption layer.

### Claim 2 (depends on 1)

The photo-detecting device of claim 1, wherein a defect concentration of the low-current blocking layer is greater than a defect concentration of the light-absorption layer.

### Claim 3 (depends on 1)

The photo-detecting device of claim 1, wherein the light absorption layer comprises at least one of AlGaN, InGaN, AlInGaN, and GaN.

### Claim 4 (depends on 3)

The photo-detecting device of claim 3, wherein the multilayer structure comprises:
at least one of a binary, ternary, and quaternary nitride layer comprising (Al, In, Ga)N; and
at least two nitride layers of different composition ratios.

### Claim 5 (depends on 1)

The photo-detecting device of claim 1, wherein a thickness of the light absorption layer is in a range of 0.1 μm to 0.5 μm.

### Claim 6 (depends on 1)

The photo-detecting device of claim 1, wherein a thickness of the low-current blocking layer is in a range of 10 nm to 100 nm.

### Claim 7 (depends on 1)

The photo-detecting device of claim 1, further comprising:
a substrate, the first nitride layer being disposed on the substrate; and
a second nitride layer disposed between the substrate and the first nitride layer,
wherein the second nitride layer increases crystallinity of the first nitride layer.

### Claim 8 (depends on 1)

The photo-detecting device of claim 1, wherein the first nitride layer comprises an undoped GaN layer or an n-type-doped GaN layer.

### Claim 9 (depends on 1)

The photo-detecting device of claim 1, further comprising:
a cap layer disposed between the light absorption layer and the Schottky junction layer,
wherein the cap layer comprises an Mg-doped nitride layer.

### Claim 10 (depends on 1)

The photo-detecting device of claim 1, further comprising:
a first electrode disposed on the Schottky junction layer; and
a second electrode disposed on an exposed region of the first nitride layer,
wherein the light absorption layer and the low-current blocking layer are removed in the exposed region.

### Claim 11 (depends on 1)

The photo-detecting device of claim 1, wherein a UV-to-visible light rejection ratio of the photo-detecting device is greater than or equal to 104 at a peak wavelength of visible light of 600 nm.

### Claim 12

A method of manufacturing a photo-detecting device, the method comprising:
forming a first nitride layer;
forming a low-current blocking layer comprising a multilayer structure on the first nitride layer;
forming a light absorption layer on the low-current blocking layer; and
forming a Schottky junction layer on the light absorption layer,
wherein the low-current blocking layer is formed at a lower temperature than the light absorption layer.

### Claim 13 (depends on 12)

The method of claim 12, wherein the low-current blocking layer is formed at a temperature 30° C. to 200° C. lower than a formation temperature of the light absorption layer.

### Claim 14 (depends on 12)

The method of claim 12, wherein:
the multilayer structure comprises at least one of a binary, ternary, and quaternary nitride layer comprising (Al, In, Ga)N; and
the multilayer structure is formed by repetitively stacking at least two nitride layers of s different composition ratios.

### Claim 15 (depends on 14)

The method of claim 14, wherein the at least two nitride layers are formed at different ambient pressures.

### Claim 16 (depends on 15)

The method of claim 15, wherein a temperature and an inflow rate of a source gas used to form the at least two nitride layers are held substantially constant while the at least two nitride layers are being formed.

### Claim 17 (depends on 12)

The method of claim 12, further comprising:
forming a second nitride layer on a substrate,
wherein the first nitride layer is formed on the second nitride layer, the second nitride layer being disposed between the first nitride layer and the substrate,
wherein the second nitride layer is formed at a lower temperature than the first nitride layer.

### Claim 18 (depends on 12)

The method of claim 12, further comprising:
forming, before forming the Schottky junction layer, a cap layer comprising an Mg-doped nitride layer on the light absorption layer.

### Claim 19 (depends on 12)

The method of claim 12, further comprising:
exposing, before forming the Schottky junction layer, a portion of the first nitride layer by removing corresponding portions of the light absorption layer and the low-current blocking layer.

### Claim 20 (depends on 19)

The method of claim 19, further comprising:
forming a first electrode on the Schottky junction layer; and
forming a second electrode on the portion of the first nitride layer.