# US 2015/0083965 A1 · Core-shell structured silicate luminescent material and preparation method therefor

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0083965 A1
- Document ID: US20150083965A1
- Status: Published application
- Kind: A1
- Application number: 14/397,942
- Filed: 2012-05-08
- Published: 2015-03-26
- Earliest claimed: 2012-05-08
- Assignees: Ocean's King Lighting Science & Technology Co., Ltd.; Shenzhen Ocean's King Lighting Engineering Co., Ltd.
- Inventors: Mingjie Zhou; Rong Wang; Guitang Chen
- Web page: https://patentgrep.com/patent/US20150083965A1

## CPC

- C09K 11/025: {non-luminescent particle coatings or suspension media}
- B05D 3/0413: {Heating with air}
- B05D 3/0453: {After-treatment}
- C09K 11/02: Use of particular materials as binders, particle coatings or suspension media therefor
- C09K 11/77742: {Silicates}
- C09K 11/77922: {Silicates}
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE
- B05D: PROCESSES FOR APPLYING FLUENT MATERIALS TO SURFACES, IN GENERAL (conveying articles or workpieces through baths of liquid B65G, e.g. B65G49/02)

## Abstract

A core-shell structured silicate luminescent material and a preparation method thereof. The molecular formula of the luminescent material is: MLn1-xSiO4:xRE@SiO2; where @ represents a coating, where M is one or two elements among Li, Na, and K, where Ln is one or two elements among Y, Sc, Lu and La, where the value of x is 0<x≦0.6; and where RE is one, two, or three elements among Tb, Gd, Sm, Eu, Dy, Ce and Tm. The compositions of the luminescent material are all chemicals of increased chemical stability, and, when subjected to electron beam bombardment for an extended period, provide a stable matrix and do not decompose easily.

## Claims

### Claim 1

A core-shell structured silicate luminescent material, wherein having the molecular formula of: MLn1-xSiO4:xRE@SiO2;
where, @ represents a coating;
M is one or two elements selected from Li, Na, and K;
Ln is one or two elements among Y, Sc, Lu and La, x is 0<x≦0.6; and;
RE is one, two or three elements selected from Tb, Gd, Sm, Eu, Dy, Ce and Tm.

### Claim 2 (depends on 1)

A core-shell structured silicate luminescent material according to claim 1, wherein x is 0.01≦x≦0.3.

### Claim 3

A method of preparing a core-shell structured silicate luminescent material comprising the step of:
mixing 10 to 20 parts by volume of water, 15 to 50 parts by volume of anhydrous ethanol and 1 to 7 parts by volume of ammonia water, followed by dropwisely adding 0.5 to 3 parts by volume of tetraethylorthosilicate under stirring, stirring to react for 2 h to 6 h further, removing impurities after being separated by centrifugation, taking the precipitate and redispersing the same to 10 to 20 parts by volume of anhydrous ethanol to give a suspension of SiO2 microsphere;
according to the stoichiometric ratio of the formula of MLn1-xSiO4:xRE, taking by measurement the corresponding nitrate solution of RE and nitrate solution of M, mixing the same homogenously, and subjecting the same to a water bath at 50° C. to 90° C., which the pH of the resulting mixture was adjusted to 1 to 6, followed by dropwisely adding tetraethylorthosilicate to give the resulting mixture, where M is one or two elements selected from Li, Na and K, Ln is one or more elements selected from Y, Sc, Lu and La, x ranges from 0<x≦0.6, RE is one, two or three elements selected from Tb, Gd, Sm, Eu, Dy, Ce and Tm;
according to the stoichiometric ratio of the formula of MLn1-xSiO4:xRE@SiO2, adding said suspension of SiO2 microsphere into said resulting mixture in a water bath at 50° C. to 90° C., stirring sufficiently to give a gel, drying the gel to give a precursor;
pre-baking said precursor, and subjecting the same to grinding, repeating the operation of grinding after pre-baking 1 to 4 times, followed by calcined in air or under a reducing atmosphere, to give the core-shell structured silicate luminescent material after cooling, having the molecular formula of: MLn1-xSiO4:xRE@SiO2, where @ represents a coating.

### Claim 4 (depends on 3)

A method of preparing the core-shell structured silicate luminescent material according to claim 3, wherein the step of removing impurities after separation by centrifugation comprises subjecting said suspension of SiO2 microsphere containing impurities to centrifugal separation spinning at 12000 rpm, taking the precipitate, followed by washing the precipitate with deionized water three times.

### Claim 5 (depends on 3)

A method of preparing the core-shell structured silicate luminescent material according to claim 3, wherein the concentration of said corresponding nitrate solution of RE and nitrate solution of M ranges from 0.1M to 5M.

### Claim 6 (depends on 3)

A method of preparing the core-shell structured silicate luminescent material according to claim 3, wherein x ranges from 0.01≦x≦0.3.

### Claim 7 (depends on 3)

A method of preparing the core-shell structured silicate luminescent material according to claim 3, wherein the step of drying the gel to give the precursor comprises completely drying the gel at 80° C. to 150° C. to give the precursor.

### Claim 8 (depends on 3)

A method of preparing the core-shell structured silicate luminescent material according to claim 3, wherein the step of pre-baking said precursor and subjecting the same to grinding comprises pre-baking the precursor at 500° C. to 800° C. for 2 h to 7 h, followed by subjecting the same to grinding after cooling.

### Claim 9 (depends on 3)

A method of preparing the core-shell structured silicate luminescent material according to claim 3, wherein the temperature of calcined in air or under a reducing atmosphere is 900° C. to 1600° C., and the time of calcined is 2 h to 10 h.

### Claim 10 (depends on 3)

A method of preparing the core-shell structured silicate luminescent material according to claim 3, wherein said reducing atmosphere is a mixed atmosphere comprised of 95 vol % of N2 and 5 vol % of H2.