# US 2015/0083960 A1 · Magnetic body and electronic component using the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0083960 A1
- Document ID: US20150083960A1
- Status: Published application
- Kind: A1
- Application number: 14/491,726
- Filed: 2014-09-19
- Published: 2015-03-26
- Earliest claimed: 2013-09-20
- Assignees: Taiyo Yuden Co., Ltd.
- Applicants: Taiyo Yuden Co., Ltd.
- Inventors: Atsushi TANADA; Kiyoshi TANAKA
- Web page: https://patentgrep.com/patent/US20150083960A1

## CPC

- H01F 1/14766: {Fe-Si based alloys}
- C22C 33/0257: {characterised by the range of the alloying elements}
- C22C 38/06: containing aluminium
- C22C 38/34: with more than 1.5% by weight of silicon
- H01F 1/24: the particles being insulated
- H01F 1/33: mixtures of metallic and non-metallic particles; metallic particles having oxide skin
- B22F 2998/10: Processes characterised by the sequence of their steps
- C22C 33/0285: {with Cr, Co, or Ni having a minimum content higher than 5%}
- C22C 2202/02: Magnetic
- H01F: MAGNETS; INDUCTANCES; TRANSFORMERS; SELECTION OF MATERIALS FOR THEIR MAGNETIC PROPERTIES
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- B22F: WORKING METALLIC POWDER; MANUFACTURE OF ARTICLES FROM METALLIC POWDER; MAKING METALLIC POWDER (making alloys by powder metallurgy C22C); APPARATUS OR DEVICES SPECIALLY ADAPTED FOR METALLIC POWDER

## Abstract

A magnetic body constituted by magnetic grains bonded together via oxide film, which magnetic grains contain a Fe—Si-M soft magnetic alloy (where M is a metal element more easily oxidized than Fe) that contains sulfur atoms (S). The magnetic body preferably contains 0.004 to 0.012 percent by weight of S, 1.5 to 7.5 percent by weight of Si, and 2 to 8 percent by weight of metal M.

## Claims

### Claim 1

A magnetic body constituted by magnetic grains bonded together via oxide film, wherein the magnetic grains contain a Fe—Si-M soft magnetic alloy (where M is a metal element more easily oxidized than Fe), which alloy contains sulfur atoms (S).

### Claim 2 (depends on 1)

A magnetic body according to claim 1, which contains 0.004 to 0.012 percent by weight of S.

### Claim 3 (depends on 1)

A magnetic body according to claim 1, which consists of 1.5 to 7.5 percent by weight of Si, 2 to 8 percent by weight of metal M, as well as S, Fe, oxygen atoms, and unavoidable impurities.

### Claim 4 (depends on 2)

A magnetic body according to claim 2, which consists of 1.5 to 7.5 percent by weight of Si, 2 to 8 percent by weight of metal M, as well as S, Fe, oxygen atoms, and unavoidable impurities.

### Claim 5 (depends on 1)

A magnetic body according to claim 1, whose apparent density is between 5.7 and 7.2 g/cm3.

### Claim 6 (depends on 1)

A magnetic body according to claim 1, wherein the metal M is Cr or Al.

### Claim 7 (depends on 1)

A magnetic body according to claim 1, wherein S is dispersed in the Fe—Si-M soft magnetic alloy.

### Claim 8 (depends on 1)

A magnetic body according to claim 1, wherein the magnetic grains are bonded fixedly together primarily via the oxide film without any other intervening layer and partially by direct bonding without any intervening layer.

### Claim 9 (depends on 1)

A magnetic body according to claim 1, wherein the magnetic grains are manufactured according to an atomization method.

### Claim 10 (depends on 1)

A magnetic body according to claim 1, wherein the magnetic grains are manufactured according to an atomization method and S is added in a manufacturing process according to the atomization method.

### Claim 11 (depends on 1)

A magnetic body according to claim 1, wherein the oxide film contains an oxide of magnetic grains themselves and bonding via oxide film is achieved by heat treatment.

### Claim 12 (depends on 1)

An electronic component equipped with a magnetic core that contains a magnetic body according to claim 1.