# US 2015/0083958 A1 · Insulating mineral foam

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0083958 A1
- Document ID: US20150083958A1
- Status: Published application
- Kind: A1
- Application number: 14/390,713
- Filed: 2013-04-05
- Published: 2015-03-26
- Earliest claimed: 2012-04-06
- Assignees: Lafarge
- Applicants: Lafarge
- Inventors: Sébastien Bernardi; Isabelle Javierre; Sylvain Duchand; Serge Sabio; Cédric Roy
- Web page: https://patentgrep.com/patent/US20150083958A1

## CPC

- E04B 1/76: specifically with respect to heat only (heat insulation in general F16L59/00)
- C04B 11/005: {Preparing or treating the raw materials}
- C04B 28/02: containing hydraulic cements other than calcium sulfates
- C04B 28/04: Portland cements
- C04B 28/065: {Calcium aluminosulfate cements, e.g. cements hydrating into ettringite}
- C04B 28/14: containing calcium sulfate cements {(gypsum-paper plates E04C)}
- C04B 38/10: by using foaming agents (C04B38/02 takes precedence){or by using mechanical means, e.g. adding preformed foam}
- C04B 2111/40: Porous or lightweight materials
- Y02W 30/91: Use of waste materials as fillers for mortars or concrete
- E04B: GENERAL BUILDING CONSTRUCTIONS; WALLS, e.g. PARTITIONS; ROOFS; FLOORS; CEILINGS; INSULATION OR OTHER PROTECTION OF BUILDINGS (border constructions of opening in walls, floors or ceilings E06B1/00; {electromagnetic shielding H05K9/0001})
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- Y02W: CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO WASTEWATER TREATMENT OR WASTE MANAGEMENT

## Abstract

A process for producing a mineral foam includes (i) separately preparing one or more slurries of cement, and an aqueous foam for which a D50 of bubbles is less than or equal to 400 μm; (ii) homogenizing the one or more slurries of cement with the aqueous foam to obtain a slurry of foamed cement; (iii) casting the slurry of foamed cement and leaving the cast slurry of foamed cement to set.

## Claims

### Claim 1

A process for production of a mineral foam comprising:
(i) separately preparing one or more slurries of cement, and an aqueous foam for which a D50 of bubbles is less than or equal to 400 μm;
(ii) homogenizing the one or more slurries of cement with the aqueous foam to obtain a slurry of foamed cement;
(iii) casting the slurry of foamed cement and leaving the cast slurry of foamed cement to set.

### Claim 2 (depends on 1)

The process for production of a mineral foam according to claim 1, wherein step (i) comprises the preparation of two slurries of cement, one of which is a slurry of calcium aluminate cement.

### Claim 3 (depends on 1)

The process for production of a mineral foam according to claim 1, wherein step (ii) comprises the introduction of the slurry or slurries of cement and the aqueous foam into a static mixer to obtain a slurry of foamed cement.

### Claim 4 (depends on 1)

A mineral foam obtainable according to the process of claim 1.

### Claim 5 (depends on 4)

The mineral foam obtainable according to claim 4 having a density of 100 to 600 kg/m3.

### Claim 6 (depends on 4)

A mineral foam according to claim 4 produced from a slurry of foamed cement comprising at least, in % by mass relative to the mass of the slurry of foamed cement:
from 20 to 70% of cement;
from 1 to 5% of calcium sulphate;
from 0.5 to 10% of calcium aluminate cement;
from 0.05 to 3% of a water reducer, a plasticizer or a superplasticizer;
from 0.001 to 0.5% of a retarder;
from 0.1 to 5% of a foaming agent;
from 15 to 40% of water;
the calcium aluminate cement/calcium sulphate ratio, expressed in mass percentage being from 0.5 to 2.5;
the calcium sulphate/cement ratio, expressed in mass percentage being from 0.03 to 0.09.

### Claim 7 (depends on 6)

The mineral foam according to claim 6, wherein the slurry of foamed cement comprises 15 to 50% of mineral particles.

### Claim 8 (depends on 7)

The mineral foam according to claim 7, wherein the mineral particles are selected from the group consisting of calcium carbonate, silica, ground glass, solid or hollow glass beads, glass granules, expanded glass powders, silica aerogels, silica fume, slags, ground sedimentary siliceous sands, fly ash or pozzolanic materials and mixtures thereof.

### Claim 9 (depends on 6)

The mineral foam according to claim 6, wherein the calcium aluminate cement/calcium sulphate ratio is from 0.6 to 2.2.

### Claim 10 (depends on 6)

The mineral foam according to claim 6, wherein the calcium sulphate/cement ratio is from 0.04 to 0.08.

### Claim 11 (depends on 4)

The mineral foam according to claim 4 produced from a slurry of foamed cement comprising at least, in % by mass relative to the mass of the slurry of foamed cement
from 30 to 75% of cement;
from 10 to 70% of fine mineral particles with a D50 less than or equal to 5 μm;
from 0 to 15% of ultrafine mineral particles with a D50 less than or equal to 1 μm;
from 0.05 to 3% of a water reducer, a plasticizer or a superplasticizer;
from 0.0001 to 1% of a retarder;
from 0 to 0.1% of a thickening agent;
from 0.01 to 5% of a foaming agent;
from 0 to 0.5% of alkaline sulphates;
from 0 to 1% of an accelerator;
from 10 to 70% of water;
the fine mineral particles/cement ratio, expressed in mass percentage, being comprised from 0.27 to 0.6;
the ultrafine mineral particles/fine particles ratio, expressed in mass percentage, being comprised from 0 to 0.5.

### Claim 12 (depends on 4)

The mineral foam according to claim 4 produced from a slurry of foamed cement comprising at least, in % by mass relative to the mass of foamed cement slurry
from 30 to 75% of cement obtained from clinker comprising at least one mineralogical C4A3$ phase;
from 0.05 to 3% of a water reducer, a plasticizer or a superplasticizer;
from 0 to 0.1% of a thickening agent;
from 0.01 to 5% of a foaming agent;
from 0.00001 to 0.01% of lithium salt;
from 10 to 70% of water.

### Claim 13 (depends on 4)

A method comprising using the mineral foam according to claim 4 as construction material.

### Claim 14 (depends on 4)

A method comprising using the mineral foam according to claim 4 as insulating material.

### Claim 15 (depends on 4)

An element of construction comprising a mineral foam according to claim 4.