# US 2015/0082632 A1 · Method for producing an aluminum piston

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0082632 A1
- Document ID: US20150082632A1
- Status: Published application
- Kind: A1
- Application number: 14/388,682
- Filed: 2013-03-25
- Published: 2015-03-26
- Earliest claimed: 2012-03-28
- Assignees: Mahle International GmbH
- Applicants: Mahle International GmbH
- Inventors: Karlheinz Bing; Thomas Hackh; Frank Schnaiter
- Web page: https://patentgrep.com/patent/US20150082632A1

## CPC

- B23P 15/10: pistons
- B23K 9/048: {on cylindrical surfaces}
- B23K 9/23: taking account of the properties of the materials to be welded
- B23K 10/027: {Welding for purposes other than joining, e.g. build-up welding}
- B23K 26/32: taking account of the properties of the material involved
- B23K 26/342: Build-up welding
- B23K 35/286: {Al as the principal constituent}
- C23C 4/04: characterised by the coating material
- C23C 4/08: containing only metal elements (C23C4/073 takes precedence)
- C23C 4/18: After-treatment
- C23C 24/04: Impact or kinetic deposition of particles
- F02B 23/06: the combustion space being arranged in working piston (F02B23/04 takes precedence)
- F02B 23/0651: {the fuel spray impinging on reflecting surfaces or being specially guided throughout the combustion space}
- F02B 23/0696: {W-piston bowl, i.e. the combustion space having a central projection pointing towards the cylinder head and the surrounding wall being inclined towards the cylinder wall}
- B23K 2101/003: {Pistons}
- B23K 2101/006: {Vehicles}
- B23K 2101/35: {Surface treated articles}
- B23K 2103/10: Aluminium or alloys thereof
- F02F 3/14: within combustion chambers
- F05C 2201/903: Aluminium alloy, e.g. AlCuMgPb F34,37
- F05C 2253/12: Coating
- Y02T 10/12: Improving ICE efficiencies
- Y10T 29/49249: Piston making
- B23P: METAL-WORKING NOT OTHERWISE PROVIDED FOR; COMBINED OPERATIONS; UNIVERSAL MACHINE TOOLS (arrangements for copying or controlling B23Q)
- B23K: SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- F02B: INTERNAL-COMBUSTION PISTON ENGINES; COMBUSTION ENGINES IN GENERAL (gas-turbine plants F02C; hot-gas or combustion-product positive-displacement engine plants F02G)
- F02F: CYLINDERS, PISTONS OR CASINGS, FOR COMBUSTION ENGINES; ARRANGEMENTS OF SEALINGS IN COMBUSTION ENGINES
- F05C: INDEXING SCHEME RELATING TO MATERIALS, MATERIAL PROPERTIES OR MATERIAL CHARACTERISTICS FOR MACHINES, ENGINES OR PUMPS OTHER THAN NON-POSITIVE-DISPLACEMENT MACHINES OR ENGINES
- Y02T: CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO TRANSPORTATION
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

A method for producing an aluminum piston for an internal combustion engine may including providing a piston bowl having a bowl edge and a bowl base; subjecting an area of at least one of the bowl edge and the bowl base to a welding treatment to introduce at least one additional element into a base material of the piston bowl and to produce intermetallic phases in the base material; the welding treatment may introduce at least one of the following additional elements at the specified concentrations, 1-7 wt. percentage of Ni, 1-15 wt. percentage of Cu and 1-5 wt. percentage of Fe.

## Claims

### Claim 1

A method for producing an aluminium piston for an internal combustion engine, comprising: providing a piston bowl having a bowl edge and a bowl base, subjecting an area of at least one of the bowl edge and the bowl base to a welding treatment to introduce at least one additional element into a base material of the piston bowl and to produce intermetallic phases in the base material, wherein the welding treatment introduces at least one of the following additional elements at the specified concentration, 1-7 wt. percentage of Ni, 1-15 wt. percentage of Cu and 1-5 wt. percentage of Fe.

### Claim 2 (depends on 1)

The method according to claim 1, wherein subjecting the area of at least one of the bowl edge and the bowl base to the welding treatment introduces at least one of the following additional elements at the specified concentration, 1-7 wt. percentage of Ni, 1-15 wt. percentage of Cu and 0.5-5 wt. percentage of Fe.

### Claim 3 (depends on 1)

The method according to claim 1, wherein the welding treatment includes at least one of the following with the specified ratio of arc energy input per unit length/weld penetration area E/A (J/mm3): (i) arc welding, via tungsten inert gas welding with E/A=7-17 J/mm3, (ii) arc welding via plasma welding with E/A=6-16 J/mm3, (iii) laser beam welding with E/A=80-90 J/mm3, and (iv) electron beam welding with E/A=5-15 J/mm3.

### Claim 4 (depends on 2)

The method according to claim 2, wherein the welding process includes at least one of the following with the specified energy input per unit length E (J/mm): (i) arc welding, via tungsten inert-gas welding with E=150-450 J/mm, (ii) arc welding via plasma welding with E=250-700 J/mm, (iii) laser beam welding with E=100-400 J/mm, and (iv) electron-beam welding with E=500-900 J/mm, wherein the additional elements are pre-heated to a temperature above room temperature.

### Claim 5 (depends on 1)

The method according to claim 1, wherein the welding treatment introduces at least one of the following additional elements at the specified concentration, 2-7 wt. percentage of Ni, 3-15 wt. percentage of Cu and 1-5 wt. percentage of Fe.

### Claim 6 (depends on 2)

The method according to claim 2, wherein the welding treatment introduces at least one of the following additional elements at the specified concentration, 2-7 wt. percentage of Ni, 3-15 wt. percentage of Cu and 0.5-1 wt. percentage of Fe.

### Claim 7 (depends on 1)

The method according to claim 1, wherein the welding produces intermetallic phases with a maximum longitudinal extension of less than 50 microns.

### Claim 8 (depends on 1)

The method according to claim 1, wherein the base material includes, with the following composition, Al of 60-90 wt. percentage, Si of 8-20 wt. percentage, Cu of 2-6 wt. percentage, Ni of 1-4 wt. percentage and Mg of 0.2-2 wt. percentage.

### Claim 9 (depends on 1)

The method according of claim 1, wherein the base material includes, with the following composition, Al of 75-85 wt. percentage, Si of 10-13 wt. percentage, Cu 3.5-5 of wt. percentage, Ni of 1.5-2.5 wt. percentage and Mg of 0.5-1.5 wt. percentage.

### Claim 10 (depends on 1)

The method according to claim 1, further comprising supplementing the base material with at least one of the additional elements, each at a concentration of less than 1 wt. percentage, Fe, Mn, Ti, Zr, V, Ca, Sr, Na, and P.

### Claim 11 (depends on 1)

The method according to claim 1, wherein the welding treatment includes adding the at least one additional element directly to a molten pool formed during welding in the form of at least one of a powder and a wire.

### Claim 12 (depends on 1)

The method according to claim 1, further comprising applying the at least one additional element to the base material before the welding process via at least one of thermal spraying, cold gas spraying, foil, paste, galvanic deposition and chemical deposition.

### Claim 13 (depends on 1)

The method according to claim 1, wherein the welding treatment includes using at least one of metal-inert gas welding, laser plasma powder hybrid welding and laser-MIG hybrid welding.

### Claim 14

An aluminium piston for an internal combustion engine, comprising: a piston bowl composed of a base material, the bowl having a bowl edge and a bowl base, wherein at least one of the bowl edge and the bowl base includes an intermetallic phase having a longitudinal extension of less than 50 microns, the intermetallic phase including at least one of the following elements at the specified concentrations: 1-7 percentage by weight of Ni, 1-15 percentage by weight of Cu, and 1-5 percentage by weight of Fe.

### Claim 15 (depends on 14)

The piston according to claim 14, wherein the base material includes, with the following compositions: 75 to 85 percentage by weight of Al, 10 to 13 percentage by weight of Si, 3.5 to 5 percentage by weight of Cu, 1.5 to 2.5 percentage by weight of Ni, and 0.5 to 1.5 percentage by weight of Mg.

### Claim 16 (depends on 3)

The method according to claim 3, wherein the base material includes, with the following compositions: 75 to 85 percentage by weight of Al, 10 to 13 percentage by weight of Si, 3.5 to 5 percentage by weight of Cu, 1.5 to 2.5 percentage by weight of Ni, and 0.5 to 1.5 percentage by weight of Mg.

### Claim 17 (depends on 4)

The method according to claim 4, wherein the additional elements are pre-heated to a temperature ranging from 100 to 300° C.

### Claim 18 (depends on 9)

The method according to claim 9, further comprising supplementing the base material with at least one of the additional elements of Fe, Mn, Ti, Zr, V, Ca, Sr, Na and P, each at a concentration of less than 1 percentage by weight.

### Claim 19

A method for producing a piston for an internal combustion engine, comprising:
forming a piston bowl having a bowl edge and a bowl base from a base material, the base material including, with the following compositions: 75 to 85 percentage by weight of Al, 10 to 13 percentage by weight of Si, 3.5 to 5 percentage by weight of Cu, 1.5 to 2.5 percentage by weight of Ni, and 0.5 to 1.5 percentage by weight of Mg; and
introducing at least one additional element into the base material via welding to produce intermetallic phases having a longitudinal extension of less than 50 microns, the at least one additional element including at least one of the following: 2 to 7 percentage by weight of Ni, 3 to 15 percentage by weight of Cu and 1 to 5 percentage by weight of Fe;
wherein the welding includes at least one of the following with the specified ratio of arc energy/weld penetration area ratio (E/A): tungsten inert gas welding with an E/A of 7 to 17 J/mm3, plasma welding with an E/A of 6 to 16 J/mm3, laser beam welding with an E/A of 80 to 90 J/mm3, and electron beam welding with an E/A of 5 to 15 J/mm3.

### Claim 20 (depends on 18)

The method according to claim 18, further comprising supplementing the base material with at least one of the additional elements of Fe, Mn, Ti, Zr, V, Ca, Sr, Na and P, each at a concentration of less than 1 percentage by weight.