# US 2015/0079382 A1 · Carbon-On-Carbon Manufacturing

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0079382 A1
- Document ID: US20150079382A1
- Status: Published application
- Kind: A1
- Application number: 14/325,213
- Filed: 2014-07-07
- Published: 2015-03-19
- Earliest claimed: 2012-01-30
- Assignees: Firestar Engineering, LLC
- Applicants: Firestar Engineering, LLC
- Inventors: Gregory S. Mungas; Larry Buchanan; Jose T. Banzon, JR.
- Web page: https://patentgrep.com/patent/US20150079382A1

## CPC

- C04B 35/83: Carbon fibres in a carbon matrix
- B29C 35/0222: {the curing continuing after removal from the mould (B29C35/0233 takes precedence)}
- B29C 70/021: {Combinations of fibrous reinforcement and non-fibrous material}
- C04B 35/64: Burning or sintering processes (C04B33/32 takes precedence {; powder metallurgy B22F})
- C04B 41/009: {characterised by the material treated}
- C04B 41/5057: {Carbides}
- C04B 41/5059: {Silicon carbide}
- C04B 41/515: {Other specific metals}
- C04B 41/87: Ceramics
- C04B 41/88: Metals
- B29K 2105/0809: {Fabrics}
- B29K 2307/04: Carbon
- C04B 2235/425: Graphite
- C04B 2235/48: Organic compounds becoming part of a ceramic after heat treatment, e.g. carbonising phenol resins
- C04B 2235/5248: Carbon, e.g. graphite
- C04B 2235/5256: Two-dimensional, e.g. woven structures
- C04B 2235/5264: characterised by the diameter of the fibers
- C04B 2235/608: Green bodies or pre-forms with well-defined density
- C04B 2235/614: Gas infiltration of green bodies or pre-forms
- C04B 2235/616: Liquid infiltration of green bodies or pre-forms
- C04B 2235/65: Aspects relating to heat treatments of ceramic bodies such as green ceramics or pre-sintered ceramics, e.g. burning, sintering or melting processes
- C04B 2235/6581: Total pressure below 1 atmosphere, e.g. vacuum
- C04B 2235/661: Multi-step sintering
- D10B 2101/12: Carbon; Pitch
- Y10T 428/249921: Web or sheet containing structurally defined element or component
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- B29K: INDEXING SCHEME ASSOCIATED WITH SUBCLASSES B29B, B29C OR B29D, RELATING TO MOULDING MATERIALS OR TO MATERIALS FOR {MOULDS, } REINFORCEMENTS, FILLERS OR PREFORMED PARTS, e.g. INSERTS
- D10B: INDEXING SCHEME ASSOCIATED WITH SUBLASSES OF SECTION D, RELATING TO TEXTILES
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

The presently disclosed technology relates to carbon-on-carbon (C/C) manufacturing techniques and the resulting C/C products. One aspect of the manufacturing techniques disclosed herein utilizes two distinct curing operations that occur at different times and/or using different temperatures. The resulting C/C products are substantially non-porous, even though the curing operation(s) substantially gasify a liquid carbon-entrained filler material that saturates a carbon fabric that makes up the C/C products.

## Claims

### Claim 1

A method of manufacturing a carbon-on-carbon (C/C) composite, the method comprising:
curing a C/C lay-up within a mold under vacuum at a first curing temperature;
releasing the C/C lay-up from the mold; and
curing the C/C lay-up at a second curing temperature responsive to the releasing operation, wherein the second curing temperature is higher than the first curing temperature.

### Claim 2 (depends on 1)

The method of claim 1, wherein the first curing temperature substantially gasifies a carbon-entrained filler within the C/C lay-up.

### Claim 3 (depends on 2)

The method of claim 2, wherein the second curing temperature substantially bonds carbon powder within the carbon-entrained filler to carbon-fabric within the C/C lay-up.

### Claim 4 (depends on 1)

The method of claim 1, wherein the releasing operation includes removing a releasing layer that provides a barrier between the C/C lay-up and the mold.

### Claim 5 (depends on 4)

The method of claim 4, wherein the releasing layer does not undergo substantial chemical changes at the first curing temperature.

### Claim 6 (depends on 1)

The method of claim 1, further comprising:
cooling the C/C lay-up prior to the releasing operation and responsive to curing the C/C lay-up at the first curing temperature.

### Claim 7 (depends on 1)

The method of claim 1, further comprising:
applying an oxidation-resistant high-temperature coating to the C/C lay-up responsive to curing the C/C lay-up at the second curing temperature.

### Claim 8 (depends on 1)

The method of claim 1, wherein the first curing temperature ranges from about 100° C. to about 160° C. and the second curing temperature ranges from about 200° C. to about 300° C.

### Claim 9 (depends on 1)

The method of claim 1, wherein a duration of curing the C/C lay-up at the first curing temperature ranges from about 2 hours to about 6 hours and a duration of curing the C/C lay-up at the second curing temperature ranges from about 1 hour to about 3 hours.

### Claim 10 (depends on 1)

The method of claim 1, further comprising:
curing the C/C lay-up at a third curing temperature using carbon vapor deposition responsive to curing the C/C lay-up at the second curing temperature, wherein the third curing temperature is higher than the second curing temperature.

### Claim 11 (depends on 1)

The method of claim 1, wherein the curing of the C/C lay-up at the first curing temperature gasifies greater than 99% of a liquid-component of the C/C lay-up and achieves closed-cell porosity within the C/C lay-up less than 5% of the total C/C lay-up volume.

### Claim 12

A carbon-on-carbon (C/C) lay-up comprising:
one or more layers of carbon fabric, each layer substantially saturated with a volatile carbon-entrained filler;
a releasing layer positioned between the saturated carbon fabric and a mold; and
a breather layer positioned over the saturated carbon fabric, wherein the breather layer receives a vaporized liquid component of the carbon-entrained filler from the C/C lay-up when the C/C lay-up is cured during a first curing operation at a first curing temperature and a second curing operation at a second curing temperature, wherein the second curing temperature is higher than the first curing temperature.

### Claim 13 (depends on 12)

The C/C lay-up of claim 12, wherein the first curing temperature substantially gasifies the carbon-entrained filler within the C/C lay-up.

### Claim 14 (depends on 12)

The C/C lay-up of claim 12, wherein the second curing temperature substantially bonds carbon powder within the carbon-entrained filler to carbon-fabric within the C/C lay-up.

### Claim 15 (depends on 12)

The C/C lay-up of claim 12, wherein the releasing layer does not undergo substantial chemical changes at the first curing temperature.

### Claim 16 (depends on 12)

The C/C lay-up of claim 12, further comprising:
a vacuum bag that maintains the C/C lay-up under vacuum during one or both of the first curing operation and the second curing operation.

### Claim 17 (depends on 12)

The C/C lay-up of claim 12, wherein the first curing temperature ranges from about 100° C. to about 160° C. and the second curing temperature ranges from about 200° C. to about 300° C.

### Claim 18 (depends on 12)

The C/C lay-up of claim 12, wherein a duration of curing the C/C lay-up at the first curing temperature ranges from about 2 hours to about 6 hours and a duration of curing the C/C lay-up at the second curing temperature ranges from about 1 hour to about 3 hours.

### Claim 19 (depends on 12)

The C/C lay-up of claim 12, wherein the C/C lay-up is cured at a third curing temperature using carbon vapor deposition responsive to curing the C/C lay-up at the second curing temperature, wherein the third curing temperature is higher than the second curing temperature.

### Claim 20 (depends on 12)

The C/C lay-up of claim 12, wherein the curing of the C/C lay-up at the first curing temperature gasifies greater than 99% of a liquid-component of the C/C lay-up and achieves closed-cell porosity within the C/C lay-up less than 5% of the total C/C lay-up volume.