# US 2015/0054134 A1 · Silicon wafer and manufacturing method thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0054134 A1
- Document ID: US20150054134A1
- Status: Published application
- Kind: A1
- Application number: 14/518,594
- Filed: 2014-10-20
- Published: 2015-02-26
- Earliest claimed: 2009-03-25
- Assignees: Sumco Corporation
- Applicants: Sumco Corporation
- Inventors: Toshiaki ONO; Wataru ITO; Jun FUJISE
- Web page: https://patentgrep.com/patent/US20150054134A1

## CPC

- C30B 33/02: Heat treatment (C30B33/04, C30B33/06 take precedence)
- C30B 23/025: {characterised by the substrate}
- C30B 25/186: {being specially pre-treated by, e.g. chemical or physical means}
- C30B 29/06: Silicon
- H10D 62/60: Impurity distributions or concentrations
- H10D 62/83: being Group IV materials, e.g. B-doped Si or undoped Ge
- H10D 62/834: further characterised by the dopants
- H10P 36/20: Intrinsic gettering, i.e. thermally inducing defects by using oxygen present in the silicon body
- H10P 72/0436: {mainly by radiation}
- H10P 72/7611: {characterised by edge profile or support profile}
- Y10S 438/918: Special or nonstandard dopant
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- Y10S: TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS

## Abstract

A method of manufacturing a silicon wafer provides a silicon wafer which can reduce the precipitation of oxygen to prevent a wafer deformation from being generated and can prevent a slip extension due to boat scratches and transfer scratches serving as a reason for a decrease in wafer strength, even when the wafer is provided to a rapid temperature-rising-and-falling thermal treatment process.

## Claims

### Claim 1

A method of manufacturing a silicon epitaxial wafer which is provided to a semiconductor device manufacturing process having a thermal treatment process of which the highest temperature ranges from 1050° C. to the melting point of silicon and of which the temperature rising and falling rate ranges from 150° C./sec to 10000° C./sec, the method comprising:
an epitaxial process of causing an epitaxial layer to grow on the surface of a substrate, which is doped with boron so as to have resistivity of 0.02 Ωcm to 1 kΩcm and of which the initial oxygen concentration Oi is in the range of 14.0×1017 to 22×1017 atoms/cm3 (Old-ASTM; ASTM F 121, 1970-1979 published by American Society for Testing and Materials International); and
an oxygen precipitation nuclei dissolution process of treating a wafer in the treatment temperature range of 1150° C. to 1300° C., the retention time range of 5 sec to 1 min, and the temperature-falling rate range of 10° C./sec to 0.1° C./sec,
wherein the oxygen precipitation nuclei dissolution process is performed before or after the epitaxial process,
the thermal treatment process is applied to only an outermost surface layer of the silicon epitaxial wafer, and
the oxygen precipitates density is equal to or less than 5×104 pcs/cm2 in the silicon epitaxial wafer.

### Claim 2

A method of manufacturing a silicon epitaxial wafer which is provided to a semiconductor device manufacturing process having a thermal treatment process of which the highest temperature ranges from 1050° C. to the melting point of silicon and of which the temperature rising and falling rate ranges from 150° C./sec to 10000° C./sec, the method comprising:
an epitaxial process of causing an epitaxial layer to grow on the surface of a substrate, which is doped with nitrogen of 1×1013 to 5×1014 atoms/cm3; and
an oxygen precipitation nuclei dissolution process of treating a wafer in the treatment temperature range of 1200° C. to 1300° C., the retention time range of 5 sec to 1 min, and the temperature-falling rate range of 10° C./sec to 0.1° C./sec after the epitaxial process,
wherein the thermal treatment process is applied to only an outermost surface layer of the silicon epitaxial wafer, and
the oxygen precipitates density is equal to or less than 5×104 pcs/cm2 in the silicon epitaxial wafer.

### Claim 3 (depends on 1)

The method of manufacturing a silicon epitaxial wafer according to claim 1, wherein the treatment atmosphere in the oxygen precipitation nuclei dissolution process is set to an atmosphere of non-oxidizing gas not containing nitrogen.

### Claim 4 (depends on 1)

The method of manufacturing a silicon epitaxial wafer according to claim 1, wherein the treatment atmosphere in the oxygen precipitation nuclei dissolution process is set to a mixed atmosphere of non-oxidizing gas not containing 1% or more of nitrogen and oxygen gas.

### Claim 5 (depends on 1)

A silicon epitaxial wafer manufactured by the method of manufacturing a silicon epitaxial wafer according to claim 1.

### Claim 6 (depends on 2)

The method of manufacturing a silicon epitaxial wafer according to claim 2, wherein the treatment atmosphere in the oxygen precipitation nuclei dissolution process is an atmosphere of a non-oxidizing gas not containing nitrogen.

### Claim 7 (depends on 2)

The method of manufacturing a silicon epitaxial wafer according to claim 2, wherein the treatment atmosphere in the oxygen precipitation nuclei dissolution process is a mixed atmosphere of a non-oxidizing gas not containing 1% or more of nitrogen and oxygen gas.

### Claim 8 (depends on 2)

A silicon epitaxial wafer manufactured by the method of manufacturing the silicon epitaxial wafer according to claim 2.

### Claim 9 (depends on 1)

The method of manufacturing a silicon epitaxial wafer according to claim 1, wherein the wafer includes a front surface and back surface, both having a flat main surface, a front sloped chamfered portion having an angle θ1, which is in a range of from 10° to 50°, a back sloped chamfered portion having an angle θ2, which is in a range of from 10° to 30°, and front and back curved portions, which connect the front and back chamfered portions to a peripheral edge of the wafer.

### Claim 10 (depends on 2)

The method of manufacturing a silicon epitaxial wafer according to claim 2, wherein the wafer includes a front surface and back surface, both having a flat main surface, a front sloped chamfered portion having an angle θ1, which is in a range of from 10° to 50°, a back sloped chamfered portion having an angle θ2, which is in a range of from 10° to 30°, and front and back curved portions, which connect the front and back chamfered portions to a peripheral edge of the wafer.