# US 2015/0031840 A1 · Method for producing epoxidized natural rubber, rubber composition for tires, and pneumatic tire

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0031840 A1
- Document ID: US20150031840A1
- Status: Published application
- Kind: A1
- Application number: 14/379,148
- Filed: 2013-03-07
- Published: 2015-01-29
- Earliest claimed: 2012-03-08
- Assignees: Sumitomo Rubber Industries, Ltd.
- Applicants: Sumitomo Rubber Industries, Ltd.
- Inventors: Sumiko Miyazaki
- Web page: https://patentgrep.com/patent/US20150031840A1

## CPC

- C08C 19/06: Epoxidation
- B60C 1/00: Tyres characterised by the chemical composition or the physical arrangement or mixture of the composition
- B60C 1/0016: {Compositions of the tread}
- C08L 15/00: Compositions of rubber derivatives (C08L11/00, C08L13/00 take precedence)
- C08C: TREATMENT OR CHEMICAL MODIFICATION OF RUBBERS
- B60C: VEHICLE TYRES; TYRE INFLATION; TYRE CHANGING; CONNECTING VALVES TO INFLATABLE ELASTIC BODIES IN GENERAL; DEVICES OR ARRANGEMENTS RELATED TO TYRES
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)

## Abstract

The present invention provides a method for producing epoxidized natural rubber with high productivity and at low cost, a rubber composition for a tire containing the epoxidized natural rubber, and a pneumatic tire formed from the rubber composition for a tire. The present invention relates to a method for producing epoxidized natural rubber, the method including: step (1) of reacting an acid anhydride with hydrogen peroxide to prepare an organic peracid; and step (2) of epoxidizing natural rubber latex with the obtained organic peracid.

## Claims

### Claim at position 1

1-5. (canceled)

### Claim 6

A method for producing epoxidized natural rubber, the method comprising:
step (1) of reacting an acid anhydride with hydrogen peroxide at a temperature of 5° C. to 40° C. for 5 minutes to 5 hours to prepare an organic peracid; and
step (2) of epoxidizing natural rubber latex with the obtained organic peracid.

### Claim 7 (depends on 6)

The method according to claim 6,
wherein step (1) comprises mixing the acid anhydride and the hydrogen peroxide together to prepare the organic peracid.

### Claim 8 (depends on 6)

The method according to claim 6,
wherein step (1) comprises adding dropwise the acid anhydride to the hydrogen peroxide to prepare the organic peracid.

### Claim 9 (depends on 6)

The method according to claim 6,
wherein the acid anhydride is acetic anhydride, and the organic peracid is peracetic acid.

### Claim 10 (depends on 6)

The method according to claim 6,
wherein the epoxidized natural rubber has a degree of epoxidation of 0.5 to 12 mol %, and the hydrogen peroxide has a concentration of not more than 20% by mass.