# US 2015/0031790 A1 · Microgel-containing tread mixture for winter tyres

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0031790 A1
- Document ID: US20150031790A1
- Status: Published application
- Kind: A1
- Application number: 14/376,703
- Filed: 2013-02-11
- Published: 2015-01-29
- Earliest claimed: 2012-02-10
- Assignees: LANXESS Deutschland GmbH
- Applicants: LANXESS Deutschland GmbH
- Inventors: Werner Obrecht; Lothar Steger
- Web page: https://patentgrep.com/patent/US20150031790A1

## CPC

- C08L 9/06: Copolymers with styrene
- B29B 7/002: {Methods (chemical aspects C08J3/00)}
- B29B 7/286: {measuring properties of the mixture, e.g. temperature, density (B29B7/283 takes precedence)}
- B29B 7/726: {Measuring properties of mixture, e.g. temperature or density (B29B7/724 takes precedence)}
- B29B 7/7495: {for mixing rubber}
- B29B 7/90: Fillers or reinforcements {, e.g. fibres}
- B60C 1/0016: {Compositions of the tread}
- C08K 5/0025: {Crosslinking or vulcanising agents; including accelerators}
- C08K 5/548: containing sulfur {(C08K5/5477 takes precedence)}
- C08L 7/00: Compositions of natural rubber
- C08L 9/00: Compositions of homopolymers or copolymers of conjugated diene hydrocarbons
- C08L 19/006: {Rubber characterised by functional groups, e.g. telechelic diene polymers}
- B29B 7/183: {having a casing closely surrounding the rotors, e.g. of Banbury type (with single shaft B29B7/125)}
- B29B 7/38: rotary (B29B7/52 takes precedence)
- B29B 7/52: with rollers or the like, e.g. calenders
- C08L 2205/02: containing two or more polymers of the same C08L -group
- C08L 2205/03: containing three or more polymers in a blend
- Y02T 10/86: Optimisation of rolling resistance, e.g. weight reduction
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- B29B: PREPARATION OR PRETREATMENT OF THE MATERIAL TO BE SHAPED; MAKING GRANULES OR PREFORMS; RECOVERY OF PLASTICS OR OTHER CONSTITUENTS OF WASTE MATERIAL CONTAINING PLASTICS
- B60C: VEHICLE TYRES; TYRE INFLATION; TYRE CHANGING; CONNECTING VALVES TO INFLATABLE ELASTIC BODIES IN GENERAL; DEVICES OR ARRANGEMENTS RELATED TO TYRES
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)
- Y02T: CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO TRANSPORTATION

## Abstract

The present invention relates to vulcanizable rubber mixtures comprising at least the following components: I.) 100 parts by weight of an oil-free rubber matrix consisting of a) 15 to 79 parts by weight, preferably 20 to 70 parts by weight, of at least one solution SBR (S-SBR) (oil-free) having a glass transition temperature (Tg(S-SBR)) between −70° C. and −10° C., b) 20 to 75 parts by weight, preferably 25 to 70 parts by weight, of at least one 1,4-cis-polybutadiene (BR) (oil-free) having a glass transition temperature (Tg(BR)) between −95° C. and −115° C., c) 1 to 37.5 parts by weight, preferably 5 to 35 parts by weight, of natural rubber (NR) (oil-free) and/or at least one synthetic polyisoprene (IR) having a glass transition temperature (Tg(NR)) between −50° C. and −75° C. based on the oil-free natural rubber (NR) or the oil-free, synthetic polyisoprene (IR), II.) at least one hydroxyl-containing microgel based on polybutadiene, III.) at least one hydroxyl-containing, oxidic filler, IV.) at least one polysulphide-containing alkoxysilane, V.) at least one vulcanizing agent, VI.) optionally at least one rubber additive.

## Claims

### Claim 1

Vulcanizable rubber mixtures comprising at least the following components:
I.) 100 parts by weight of an oil-free rubber matrix consisting of
a) 15 to 79 parts by weight, preferably 20 to 70 parts by weight, of at least one solution SBR (S-SBR) (oil-free) having a glass transition temperature (Tg(S-SBR)) between −70° C. and −10° C.,
b) 20 to 75 parts by weight, preferably 25 to 70 parts by weight, of at least one 1,4-cis-polybutadiene (BR) (oil-free) having a glass transition temperature (Tg(BR)) between −95° C. and −115° C.,
c) 1 to 37.5 parts by weight, preferably 5 to 35 parts by weight, of natural rubber (NR) (oil-free) and/or at least one synthetic polyisoprene (IR) (oil-free) having a glass transition temperature (Tg(NR)) between −50° C. and −75° C.,
II.) at least one hydroxyl-containing microgel based on polybutadiene,
III.) at least one hydroxyl-containing, oxidic filler,
IV.) at least one polysulphide-containing alkoxysilane,
V.) at least one vulcanizing agent,
VI.) optionally at least one rubber additive.

### Claim 2 (depends on 1)

Vulcanizable rubber mixtures according to claim 1, characterized in that the oil-free rubber matrix I.) has a glass transition temperature (Tg(matrix)) between −70° C. and −90° C., the Tg(Matrix) being calculated by the general equation
Tg(matrix)=X(BR)×Tg(BR)+X(S-SBR)×Tg(S-SBR)+X(NR)×Tg(NR)
where
glass transition temperature of the rubber matrix (oil-free)
Tg(matrix)
parts by weight of 1,4-cis-polybutadiene (oil-free)
X(BR)
parts by weight of S-SBR(oil-free)
X(S-SBR)
parts by weight of NR or IR (oil-free)
X(NR)
glass transition temperature of 1,4-cis-polybutadiene (oil-free)
Tg(BR)
glass ransition temperature of S-SBR (oil-free)
Tg(S-SBR)
glass transition temperature of NR or IR (oil-free)
Tg(NR).

### Claim 3 (depends on 2)

Vulcanizable rubber mixtures according to claim 2, characterized in that the solution SBR has a Mooney viscosity (ML 1+4 at 100° C.) of 20 to 150 Mooney units, preferably of 30 to 100 Mooney units.

### Claim 4 (depends on 2)

Vulcanizable rubber mixtures according to claim 2, characterized in that the 1,4-cis-polybutadiene has a 1,4-cis content of at least 90 mol %.

### Claim 5 (depends on 4)

Vulcanizable rubber mixtures according to claim 4, characterized in that the 1,4-cis-polybutadiene is Ti—BR, Co—BR, Ni—BR or Nd—BR.

### Claim 6 (depends on 2)

Vulcanizable rubber mixtures according to claim 2, characterized in that the polyisoprene has a 1,4-cis content of at least 70 mol %.

### Claim 7 (depends on 2)

Vulcanizable rubber mixtures according to claim 2, characterized in that the hydroxyl-containing microgel II.) has a glass transition temperature (Tg(MICROGEL)) between −82° C. and −60° C., preferably −65° C. and −82° C., especially preferably −70° C. and −80° C.

### Claim 8 (depends on 2)

Vulcanizable rubber mixtures according to claim 2, characterized in that 1 to 50 parts by weight, preferably 2.5 to 30 parts by weight, more preferably 5 to 20 parts by weight, based on 100 parts by weight of oil-free rubber matrix, of the hydroxyl-containing microgel II.) are used.

### Claim 9 (depends on 8)

Vulcanizable rubber mixtures according to claim 8, characterized in that the hydroxyl-containing microgel has a gel content of more than 70% by weight, preferably more than 75% by weight, especially preferably more than 80% by weight.

### Claim 10 (depends on 9)

Vulcanizable rubber mixtures according to claim 9, characterized in that the hydroxyl-containing microgel has a swelling index (Qi) in toluene of less than 30, preferably less than 25, especially preferably less than 20.

### Claim 11 (depends on 10)

Vulcanizable rubber mixtures according to claim 10, characterized in that the hydroxyl-containing microgel has a particle size of 10 to 100 nm.

### Claim 12 (depends on 2)

Vulcanizable rubber mixtures according to claim 2, characterized in that the hydroxyl-containing, oxidic filler III.) is silica, the content thereof being in the range of 10 up to 150 parts by weight, preferably in the range of 20 to 120 parts by weight, and more preferably 25 to 100 parts by weight, based on 100 parts by weight of oil-free rubber matrix.

### Claim 13 (depends on 2)

Vulcanizable rubber mixtures according to claim 2, characterized in that the polysulphide-containing alkoxysilane is of the general formula (1) or (2)
Z-A-Sx-A-Z (1)
Z-A-Sy—R3 (2)
in which
x is an integer of 2 to 8,
y is an integer of 1 to 8,
A are the same or different and are each a divalent hydrocarbon group (“spacer”)
Z are the same or different and have one of the following formulae:
in which
R1 are the same or different, may be substituted or unsubstituted and are each a C1-C18 alkyl group, a C5-C18 cycloalkyl group or C6-C18 aryl group and
R2 are the same or different, may be substituted or unsubstituted and are each a C1-C18 alkoxy group, a C5-C18 cycloalkoxy group or C6-C18 aryloxy group and
and
R3 is hydrogen, straight-chain or branched alkyl, where the alkyl chain may optionally be interrupted by one or more, preferably up to five heteroatoms, especially oxygen, sulphur or N(H), aryl, preferably C6-C20-Aryl and/or a radical having the following structures:
in which R4 is an aliphatic, heteroaliphatic, cycloaliphatic, aromatic or heteroaromatic radical having 1 to 20, preferably 1 to 10, carbon atoms and having optionally 1 to 3 heteroatoms, preferably oxygen, nitrogen or sulphur.

### Claim 14 (depends on 13)

Vulcanizable rubber mixtures according to claim 13, characterized in that 0.2 to 12 parts by weight, preferably 1 to 10 parts by weight, based on 100 parts by weight of oil-free rubber matrix, of polysulphide-containing alkoxysilane are used.

### Claim 15 (depends on 1)

Vulcanizable rubber mixtures according to claim 1, characterized in that they do not comprise any polythiophosphorus compounds.

### Claim 16 (depends on 1)

Process for producing vulcanizable rubber mixtures according to claim 1, characterized in that components I.) to VI.) are mixed with one another in one or more stages, preferably by a three-stage mixing operation with two mixing stages in an internal mixer and a final mixing stage on a miler, or by a two-stage mixing operation in which the 1st mixing stage is effected in an internal mixer and the 2nd mixing stage on a roller, or by a two-stage mixing operation in which both mixing stages are effected in an internal mixer, the mixture being cooled prior to addition of those components which are added on the roller in the three-stage mixing operation to temperatures of <120° C., preferably <110° C.

### Claim 17 (depends on 1)

Process for producing vulcanizates, characterized in that vulcanizable rubber mixtures according to claim 1 are subjected to a crosslinking reaction, preferably at a temperature in the range of 100 to 250° C., especially 130 to 180° C., under a pressure in the range of 1 to 200 bar.

### Claim 18 (depends on 17)

Process according to claim 17, characterized in that the crosslinking takes place in the course of a shaping operation.

### Claim 19 (depends on 17)

Vulcanizates obtainable by the process according to claim 17.

### Claim 20 (depends on 1)

Use of vulcanizable rubber mixtures according to any of claim 1 for production of pneumatic tyres, especially winter tyres, tyre components, especially tyre treads, especially treads of winter tyres, subtreads, carcasses, sidewalls, reinforced sidewalls for runflat tyres and apex mixtures, and for the production of industrial rubber articles, preferably damping elements, roll coverings, conveyor belt coverings, drive belts, spinning cops, seals, golfball cores and shoe soles.