# US 2015/0031212 A1 · Method for obtaining extreme selectivity of metal nitrides and metal oxides

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0031212 A1
- Document ID: US20150031212A1
- Status: Published application
- Kind: A1
- Application number: 14/514,264
- Filed: 2014-10-14
- Published: 2015-01-29
- Earliest claimed: 2004-09-01
- Assignees: Micron Technology, Inc.
- Applicants: Micron Technology, Inc.
- Inventors: Kevin R. Shea
- Web page: https://patentgrep.com/patent/US20150031212A1

## CPC

- H10P 50/00: Etching of wafers, substrates or parts of devices
- H10D 1/042: {using deposition processes to form electrode extensions}
- H10D 1/692: {Electrodes}
- H10D 1/716: {having vertical extensions}
- H10P 50/283: {by chemical means}
- H10P 50/667: {by liquid etching only}
- H10W 20/054: {by selectively removing parts thereof (H10W20/034 takes precedence)}
- H10B 12/033: {the capacitor extending over the transistor}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10
- H10B: ELECTRONIC MEMORY DEVICES

## Abstract

Methods for etching metal nitrides and metal oxides include using ultradilute HF solutions and buffered, low-pH HF solutions containing a minimal amount of the hydrofluoric acid species H2F2. The etchant can be used to selectively remove metal nitride layers relative to doped or undoped oxides, tungsten, polysilicon, and titanium nitride. A method is provided for producing an isolated capacitor, which can be used in a dynamic random access memory cell array, on a substrate using sacrificial layers selectively removed to expose outer surfaces of the bottom electrode.

## Claims

### Claim 1

A method of selectively etching a layer of metal nitrides or metal oxide, the method comprising:
heating a substrate having formed thereon a structure comprising a layer of metal oxide or metal nitride;
exposing the structure to a buffered hydrofluoric acid etch solution having a pH between about 3.5 and about 5.5; and
selectively etching the layer of metal oxide or metal nitride with an etch rate selectivity relative to an exposed layer of silicon greater than or equal to about 2000:1.

### Claim 2 (depends on 1)

The method of claim 1, wherein heating the substrate comprises heating to a temperature between about 50° C. and about 90° C.

### Claim 3 (depends on 1)

The method of claim 1, wherein the etch solution has a pH of between about 4.0 and 5.0.

### Claim 4 (depends on 1)

The method of claim 1, wherein the etch solution has a buffer to hydrofluoric ratio that is greater than about 400:1.

### Claim 5 (depends on 1)

The method of claim 1, wherein the exposed layer of silicon is a layer of polysilicon and selectively etching comprises etching with an etch rate selectivity relative to the exposed layer of polysilicon that is greater than or equal to about 2000:1.

### Claim 6 (depends on 1)

The method of claim 1, wherein the layer of metal oxide or metal nitride comprises a material selected from the group consisting of hafnium oxide, hafnium nitride, aluminum oxide, aluminum nitride and a combination thereof.

### Claim 7

A method of selectively removing a sacrificial material, the method comprising:
providing a structure which includes a sacrificial material comprising a metal oxide or a metal nitride and further includes a nonsacrificial material;
exposing the structure to a buffered hydrofluoric acid solution having a pH between about 3.5 and 5.5 and heated to a temperature between about 50° C. and about 90° C.; and
selectively removing the sacrificial material from the structure with an etch rate selectivity relative to the nonsacrificial material greater than about 500:1.

### Claim 8 (depends on 7)

The method of claim 7, wherein the sacrificial material comprises a material selected from the group consisting of hafnium oxide, hafnium nitride, aluminum oxide, aluminum nitride and a combination thereof.

### Claim 9 (depends on 8)

The method of claim 8, wherein the nonsacrificial material is selected from the group consisting of an oxide, polysilicon, tungsten, titanium nitride and a combination thereof.

### Claim 10 (depends on 9)

The method of claim 9, wherein the nonsacrificial material is an oxide and selectively removing comprises etching with an etch rate selectivity relative to the nonsacrificial material that is greater than about 800:1.

### Claim 11 (depends on 9)

The method of claim 9, wherein the nonsacrificial material is polysilicon and selectively removing comprises etching with an etch rate selectivity relative to the nonsacrificial material that is greater than about 2000:1

### Claim 12 (depends on 7)

The method of claim 7, wherein the buffered hydrofluoric acid is heated to a temperature between about 60° C. and about 85° C.

### Claim 13 (depends on 7)

The method of claim 7, wherein the sacrificial material comprises the metal oxide and selectively removing comprises etching at an etch rate exceeding about 5000 Å/min.

### Claim 14 (depends on 7)

The method of claim 7, wherein the buffered hydrofluoric acid solution has a buffer to hydrofluoric acid ratio that is greater than about 400:1.

### Claim 15

A method of selectively removing a sacrificial material, the method comprising:
providing a structure comprising a sacrificial material and a nonsacrificial material, the sacrificial material comprising a metal oxide or a metal nitride;
exposing the structure to a buffered hydrofluoric acid solution having a buffer to hydrofluoric acid ratio exceeding about 400:1; and
selectively removing the sacrificial material from the structure with an etch rate selectivity relative to the nonsacrificial material exceeding about 500:1.

### Claim 16 (depends on 15)

The method of claim 15, wherein the buffered hydrofluoric acid solution has a pH between about 3.5 and 5.5.

### Claim 17 (depends on 15)

The method of claim 15, wherein the buffer comprises NH4F.

### Claim 18 (depends on 15)

The method of claim 15, wherein exposing comprises contacting the structure to the buffered hydrofluoric acid solution that is heated to a temperature between about 50° C. and about 90° C.

### Claim 19 (depends on 15)

The method of claim 15, wherein the buffered hydrofluoric acid solution has a buffer to hydrofluoric ratio that is greater than about 500:1.