# US 2015/0031208 A1 · Method of manufacturing semiconductor device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0031208 A1
- Document ID: US20150031208A1
- Status: Published application
- Kind: A1
- Application number: 14/245,304
- Filed: 2014-04-04
- Published: 2015-01-29
- Earliest claimed: 2013-07-25
- Assignees: Mitsubishi Electric Corporation
- Applicants: Mitsubishi Electric Corporation
- Inventors: Takuichiro SHITOMI; Yusuke KAWASE; Junichi YAMASHITA; Manabu YOSHINO
- Web page: https://patentgrep.com/patent/US20150031208A1

## CPC

- H10P 50/691: {for Group IV materials or Group III-V materials}
- H10P 14/61: using masks
- H10P 50/642: {Chemical etching}
- H10P 50/73: {using masks for insulating materials}
- H10P 90/1906: {Preparing SOI wafers}
- H10P 90/1914: {using bonding}
- H10W 10/181: {Semiconductor-on-insulator [SOI] isolation regions, e.g. buried oxide regions of SOI wafers}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

A method of manufacturing a semiconductor device, includes the steps of forming a top surface nitride film on a top surface of a substrate and a bottom surface nitride film on a bottom surface of the substrate, forming a protective film on the top surface nitride film, removing the bottom surface nitride film by wet etching while the top surface nitride film is being protected by the protective film, removing the protective film after the removing of the bottom surface nitride film, patterning the top surface nitride film so as to form an opening in the top surface nitride film, and forming a second oxide film on the bottom surface of the substrate while forming a first oxide film on a surface portion of the substrate which is exposed by the opening.

## Claims

### Claim 1

A method of manufacturing a semiconductor device, comprising the steps of:
forming a top surface nitride film on a top surface of a substrate and a bottom surface nitride film on a bottom surface of said substrate;
forming a protective film on said top surface nitride film;
removing said bottom surface nitride film by wet etching while said top surface nitride film is being protected by said protective film;
removing said protective film after said removing of said bottom surface nitride film;
patterning said top surface nitride film so as to form an opening in said top surface nitride film; and
forming a second oxide film on said bottom surface of said substrate while forming a first oxide film on a surface portion of said substrate which is exposed by said opening.

### Claim 2

A method of manufacturing a semiconductor device, comprising the steps of:
forming a top surface nitride film on a top surface of a substrate;
patterning said top surface nitride film so as to form an opening in said top surface nitride film; and
forming a second oxide film on a bottom surface of said substrate while forming a first oxide film on a surface portion of said substrate which is exposed by said opening.

### Claim 3 (depends on 1)

The method according to claim 1, wherein said first oxide film is a LOCOS oxide film having a thickness of 1000 nm or more.

### Claim 4 (depends on 1)

The method according to claim 1, wherein:
said substrate includes a support substrate, a buried oxide film formed on a top surface of said support substrate, a bottom surface oxide film formed on a bottom surface of said support substrate, and an SOI layer formed on a surface of said buried oxide film; and
said buried oxide film and said bottom surface oxide film have a thickness of 2 μm or more.

### Claim 5 (depends on 1)

The method according to claim 1, wherein said substrate is a Si substrate.

### Claim 6

A method of manufacturing a semiconductor device, comprising the steps of:
forming a bottom surface polysilicon on a bottom surface of a substrate having a top surface oxide film formed on a top surface thereof, said top surface oxide film being exposed on a top surface side of said substrate, said bottom surface polysilicon being exposed on a bottom surface side of said substrate; and
removing said exposed top surface oxide film by wet etching while leaving said exposed bottom surface polysilicon intact;
wherein said substrate has a buried oxide film on said top surface side thereof and a bottom surface oxide film on said bottom surface side thereof.

### Claim 7 (depends on 6)

The method according to claim 6, wherein said top surface oxide film is an oxide film which has a thickness of 200 nm or more and which is used as a mask in a well formation process.

### Claim 8 (depends on 1)

The method according to claim 1, wherein said substrate is a wafer having a diameter of 8 inches or more.