# US 2015/0031178 A1 · Method of cmos manufacturing utilizing multi-layer epitaxial hardmask films for improved gate spacer control

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0031178 A1
- Document ID: US20150031178A1
- Status: Published application
- Kind: A1
- Application number: 13/950,909
- Filed: 2013-07-25
- Published: 2015-01-29
- Earliest claimed: 2013-07-25
- Assignees: Texas Instruments Incorporated
- Applicants: Texas Instruments Incorporated
- Inventors: Deborah Jean RILEY; Seung-Chul SONG
- Web page: https://patentgrep.com/patent/US20150031178A1

## CPC

- H10D 84/038: {using silicon technology, e.g. SiGe}
- H10D 84/0167: {Manufacturing their channels}
- H10D 84/017: {Manufacturing their source or drain regions, e.g. silicided source or drain regions}
- H10D 84/0179: {the gate conductors having different shapes or dimensions}
- H10D 84/0184: {Manufacturing their gate sidewall spacers}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

An integrated circuit containing PMOS transistors may be formed by forming a dual layer hard mask. A first layer of the hard mask is carbon-containing silicon nitride formed using a hydrocarbon reagent. A second layer of the hard mask is chlorine-containing silicon nitride formed on the first layer using a chlorinated silane reagent. After SiGe epitaxial source/drain regions are formed, the hard mask is removed using a wet etch which removes the second layer at a rate at least three times faster than the first layer.

## Claims

### Claim 1

A method of forming an integrated circuit, comprising the steps of:
forming a first layer of a dual layer hard mask over a gate of a p-channel metal oxide semiconductor (PMOS) transistor, said first layer being silicon nitride formed by a plasma enhanced chemical vapor deposition (PECVD) process with a first chlorinated silane reagent, a hydrocarbon, and ammonia;
forming a second layer of said dual layer hard mask on said first layer, said second layer being chlorine-containing silicon nitride formed by a PECVD process with a second chlorinated silane reagent and ammonia and free of a hydrocarbon reagent;
removing said second layer and said first layer from horizontal surfaces of said integrated circuit by an anisotropic etch, leaving said second layer and said first layer on lateral surfaces of gate offset spacers disposed on lateral surfaces of said gate of said PMOS transistor;
subsequently removing material from a substrate of said integrated circuit to form source/drain cavities adjacent to said gate of said PMOS transistor;
subsequently forming silicon-germanium (SiGe) source/drain regions in said source/drain cavities by an epitaxial process;
subsequently removing said second layer by a first phase of a wet etch process in which an etch rate of said second layer is at least three times faster than an etch rate of said first layer; and
subsequently removing said first layer by a second phase of said wet etch process, so that at least a portion of said gate offset spacers remains after said second phase of said wet etch process is completed.

### Claim 2 (depends on 1)

The method of claim 1, in which said first chlorinated silane reagent is hexachlorodisilane.

### Claim 3 (depends on 1)

The method of claim 1, in which said hydrocarbon is ethylene.

### Claim 4 (depends on 1)

The method of claim 1, in which said first layer is formed at 550° C. to 650° C.

### Claim 5 (depends on 1)

The method of claim 1, in which said first layer is 4 nanometers to 10 nanometers thick.

### Claim 6 (depends on 1)

The method of claim 1, in which said second chlorinated silane reagent is hexachlorodisilane.

### Claim 7 (depends on 1)

The method of claim 1, in which said second layer is formed at 550° C. to 600° C.

### Claim 8 (depends on 1)

The method of claim 1, in which said second layer is 10 nanometers to 30 nanometers thick.

### Claim 9 (depends on 1)

The method of claim 1, in which a thickness of said second layer on vertical surfaces of said integrated circuit is at least 80 percent of a thickness of said second layer on horizontal surfaces of said integrated circuit.

### Claim 10 (depends on 1)

The method of claim 1, in which a thickness of said second layer on vertical surfaces in a static random access memory (SRAM) of said integrated circuit and a thickness of said second layer on vertical surfaces in a logic circuit of said integrated circuit are within 5 percent of each other.

### Claim 11 (depends on 1)

The method of claim 1, in which said first phase of said wet etch process includes a phosphoric acid containing etch step.

### Claim 12 (depends on 11)

The method of claim 11, in which said phosphoric acid containing etch step is performed at 150° C. to 160° C.

### Claim 13 (depends on 11)

The method of claim 11, in which said phosphoric acid containing etch step is performed for 30 seconds to 75 seconds.

### Claim 14 (depends on 1)

The method of claim 1, in which said second phase of said wet etch process is a continuation of said first phase of said wet etch process.

### Claim 15 (depends on 1)

The method of claim 1, in which an etch rate of said first layer in said second phase of said wet etch process is 0.4 nanometers per minute to 0.8 nanometers per minute.

### Claim 16 (depends on 1)

The method of claim 1, further comprising the step of forming an etch mask over said integrated circuit so as to expose said PMOS transistor and cover an n-channel metal oxide semiconductor (NMOS) transistor, performed after said step of forming said second layer and prior to said step of removing said second layer and said first layer from horizontal surfaces of said integrated circuit.

### Claim 17 (depends on 1)

The method of claim 1, in which:
said PMOS transistor is a low-voltage PMOS transistor;
said integrated circuit includes a high-voltage PMOS transistor, in which a gate dielectric layer of said high-voltage PMOS transistor is at least 30 percent thicker than a gate dielectric layer of said low-voltage PMOS transistor;
said first layer is formed over a gate of said high-voltage PMOS transistor;
said step of removing said second layer and said first layer from horizontal surfaces of said integrated circuit leaves said second layer and said first layer on lateral surfaces of gate offset spacers disposed on lateral surfaces of said gate of said high-voltage PMOS transistor; and
said step of removing material from said substrate of said integrated circuit also forms source/drain cavities adjacent to said gate of said high-voltage PMOS transistor.

### Claim 18

A method of forming an integrated circuit, comprising the steps of:
forming a first layer of a dual layer hard mask over a gate of a PMOS transistor and a gate of an NMOS transistor, said first layer being silicon nitride formed by a PECVD process with a first chlorinated silane reagent, a hydrocarbon, and ammonia;
forming a second layer of said dual layer hard mask on said first layer, said second layer being chlorine-containing silicon nitride formed by a PECVD process with a second chlorinated silane reagent and ammonia and free of a hydrocarbon reagent;
forming an etch mask over said second layer of said dual layer hard mask so as to cover said NMOS transistor and expose said PMOS transistor;
removing said second layer and said first layer from horizontal surfaces of said integrated circuit by an anisotropic etch, leaving said second layer and said first layer on lateral surfaces of gate offset spacers disposed on lateral surfaces of said gate of said PMOS transistor, and leaving said second layer and said first layer over said NMOS transistor;
subsequently removing said etch mask;
subsequently removing material from a substrate of said integrated circuit to form source/drain cavities adjacent to said gate of said PMOS transistor;
subsequently forming SiGe source/drain regions in said source/drain cavities by an epitaxial process;
subsequently removing said second layer by a first phase of a wet etch process in which an etch rate of said second layer is at least three times faster than an etch rate of said first layer; and
subsequently removing said first layer by a second phase of said wet etch process, so that at least a portion of said gate offset spacers remains after said second phase of said wet etch process is completed.

### Claim 19

A method of forming an integrated circuit, comprising the steps of:
forming a first layer of a dual layer hard mask over a gate of a low-voltage PMOS transistor, a gate of a high-voltage PMOS transistor in which a gate dielectric layer of said high-voltage PMOS transistor is at least 30 percent thicker than a gate dielectric layer of said low-voltage PMOS transistor, and a gate of an NMOS transistor, said first layer being silicon nitride formed by a PECVD process with a first chlorinated silane reagent, a hydrocarbon, and ammonia;
forming a second layer of said dual layer hard mask on said first layer, said second layer being chlorine-containing silicon nitride formed by a PECVD process with a second chlorinated silane reagent and ammonia and free of a hydrocarbon reagent;
forming an etch mask over said second layer of said dual layer hard mask so as to cover said NMOS transistor and expose said high-voltage PMOS transistor and said low-voltage PMOS transistor;
removing said second layer and said first layer from horizontal surfaces of said integrated circuit by an anisotropic etch, leaving said second layer and said first layer on lateral surfaces of gate offset spacers disposed on lateral surfaces of said gate of said low-voltage PMOS transistor and said high-voltage PMOS transistor, and leaving said second layer and said first layer over said NMOS transistor;
subsequently removing said etch mask;
subsequently removing material from a substrate of said integrated circuit to form source/drain cavities adjacent to said gate of said low-voltage PMOS transistor and adjacent to said gate of said high-voltage PMOS transistor;
subsequently forming SiGe source/drain regions in said source/drain cavities by an epitaxial process;
subsequently removing said second layer by a first phase of a wet etch process in which an etch rate of said second layer is at least three times faster than an etch rate of said first layer; and
subsequently removing said first layer by a second phase of said wet etch process, so that at least a portion of said gate offset spacers remains after said second phase of said wet etch process is completed.