# US 2015/0031175 A1 · Method for manufacturing semiconductor device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0031175 A1
- Document ID: US20150031175A1
- Status: Published application
- Kind: A1
- Application number: 14/511,862
- Filed: 2014-10-10
- Published: 2015-01-29
- Earliest claimed: 2012-05-31
- Assignees: Fuji Electric Co., Ltd.
- Applicants: Fuji Electric Co., Ltd.
- Inventors: Hideaki TERANISHI; Haruo NAKAZAWA; Masaaki OGINO
- Web page: https://patentgrep.com/patent/US20150031175A1

## CPC

- H10D 12/032: {of vertical IGBTs}
- H10D 12/01: Manufacture or treatment
- H10D 62/83: being Group IV materials, e.g. B-doped Si or undoped Ge
- H10P 32/1404: {using predeposition followed by drive-in of impurities into the semiconductor surface, e.g. predeposition from a gaseous phase}
- H10P 32/1406: {by ion implantation}
- H10P 32/171: {being group IV material}
- H10W 10/011: {of isolation regions comprising dielectric materials}
- H10W 10/031: {of isolation regions comprising PN junctions}
- H10W 10/10: Isolation regions comprising dielectric materials
- H10W 10/30: Isolation regions comprising PN junctions
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

A method for manufacturing a semiconductor device, includes providing a silicon semiconductor substrate which is manufactured by a floating zone method; and performing thermal diffusion at a heat treatment temperature that is equal to or higher than 1290° C. and that is lower than a melting temperature of a silicon crystal to form a diffusion layer with a depth of 50 μm or more in the silicon semiconductor substrate, the thermal diffusion including a first heat treatment performed in an oxygen atmosphere or a mixed gas atmosphere of oxygen and inert gas, and a second heat treatment performed in a nitrogen atmosphere or a mixed gas atmosphere of nitrogen and oxygen to form the diffusion layer. The method suppresses the occurrence of crystal defects, reduces the amount of inert gas used, and reduces manufacturing costs.

## Claims

### Claim 1

A method for manufacturing a semiconductor device, comprising:
providing a silicon semiconductor substrate which is manufactured by a floating zone method; and
performing thermal diffusion at a heat treatment temperature that is equal to or higher than 1290° C. and that is lower than a melting temperature of a silicon crystal to form a diffusion layer with a depth of 50 μm or more in the silicon semiconductor substrate, the thermal diffusion including a first heat treatment performed in an oxygen atmosphere or a mixed gas atmosphere of oxygen and inert gas, followed by a second heat treatment performed in a nitrogen atmosphere or a mixed gas atmosphere of nitrogen and oxygen to form the diffusion layer.

### Claim 2 (depends on 1)

The method for manufacturing a semiconductor device according to claim 1, wherein the silicon semiconductor substrate is a silicon semiconductor substrate that is cut from a silicon crystal, which is produced by the floating zone method using polysilicon as a raw material.

### Claim 3 (depends on 1)

The method for manufacturing a semiconductor device according to claim 1, wherein the silicon semiconductor substrate is a semiconductor substrate that is cut from a silicon crystal, which is produced by the floating zone method using crystal silicon produced by a Czochralski method as a raw material.

### Claim 4 (depends on 1)

The method for manufacturing a semiconductor device according to claim 1, wherein, when the silicon semiconductor substrate has a thickness L (μm), the first heat treatment has a processing time t (hours) that satisfies t>3.5×10−6×L2.

### Claim 5 (depends on 1)

The method for manufacturing a semiconductor device according to claim 1, wherein, when the silicon semiconductor substrate has a thickness L (μm) and an interstitial silicon atom thereof has a diffusion coefficient at a processing temperature T of the first heat treatment is DT (μm2/h), the first heat treatment has a processing time t (hours) that satisfies t>L2/(16×DT).

### Claim 6 (depends on 1)

The method for manufacturing a semiconductor device according to claim 1, wherein, when the silicon substrate has a thickness corresponding to a breakdown voltage M (μm), the first heat treatment has a processing time t (hours) that satisfies t>3.5×10−6×M2.

### Claim 7 (depends on 1)

The method for manufacturing a semiconductor device according to claim 1, wherein, when the silicon substrate has a thickness corresponding to a breakdown voltage M (μm) and an interstitial silicon atom thereof has a diffusion coefficient at a processing temperature T of the first heat treatment is DT (μm2/h), the first heat treatment has a processing time t (hours) that satisfies t>M2/(16×DT).

### Claim 8 (depends on 1)

The method for manufacturing a semiconductor device according to claim 1, wherein the diffusion layer formed during performing thermal diffusion provides an isolation layer forming a reverse blocking insulated gate bipolar transistor.

### Claim 9 (depends on 2)

The method for manufacturing a semiconductor device according to claim 2, wherein the diffusion layer formed during performing thermal diffusion provides an isolation layer forming a reverse blocking insulated gate bipolar transistor.

### Claim 10 (depends on 3)

The method for manufacturing a semiconductor device according to claim 3, wherein the diffusion layer formed during performing thermal diffusion provides an isolation layer forming a reverse blocking insulated gate bipolar transistor.

### Claim 11 (depends on 4)

The method for manufacturing a semiconductor device according to claim 4, wherein the diffusion layer formed during performing thermal diffusion provides an isolation layer forming a reverse blocking insulated gate bipolar transistor.

### Claim 12 (depends on 5)

The method for manufacturing a semiconductor device according to claim 5, wherein the diffusion layer formed during performing thermal diffusion provides an isolation layer forming a reverse blocking insulated gate bipolar transistor.

### Claim 13 (depends on 6)

The method for manufacturing a semiconductor device according to claim 6, wherein the diffusion layer formed during performing thermal diffusion provides an isolation layer forming a reverse blocking insulated gate bipolar transistor.

### Claim 14 (depends on 7)

The method for manufacturing a semiconductor device according to claim 7, wherein the diffusion layer formed during performing thermal diffusion provides an isolation layer forming a reverse blocking insulated gate bipolar transistor.