# US 2015/0030926 A1 · Electrolytic manganese dioxide, method for producing same, and use of same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0030926 A1
- Document ID: US20150030926A1
- Status: Published application
- Kind: A1
- Application number: 14/380,022
- Filed: 2013-02-20
- Published: 2015-01-29
- Earliest claimed: 2012-02-21
- Assignees: Tosoh Corporation
- Applicants: Tosoh Corporation
- Inventors: Kazumasa Suetsugu; Kazuo Sekitani
- Web page: https://patentgrep.com/patent/US20150030926A1

## CPC

- H01M 4/50: of manganese
- C25B 1/21: Manganese oxides
- H01M 6/06: Dry cells, i.e. cells wherein the electrolyte is rendered non-fluid
- H01M 2220/30: Batteries in portable systems, e.g. mobile phone, laptop
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C25B: ELECTROLYTIC OR ELECTROPHORETIC PROCESSES FOR THE PRODUCTION OF COMPOUNDS OR NON-METALS; APPARATUS THEREFOR (anodic or cathodic protection C23F13/00; single-crystal growth C30B)
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

The object of the present invention is to provide electrolytic manganese dioxide excellent in the middle rate discharge characteristic as compared with conventional electrolytic manganese dioxide, and a method for its production and its application. Electrolytic manganese dioxide characterized in that the potential as measured in a 40 wt % KOH aqueous solution by using a mercury/mercury oxide reference electrode as a standard is higher than 250 mV and less than 310 mV, and the volume of pores having a pore diameter of at least 2 nm and at most 50 nm is at most 0.0055 cm3/g. Of such electrolytic manganese dioxide, the volume of pores having a pore diameter of at least 2 nm and at most 200 nm is preferably at most 0.0555 cm3/g.

## Claims

### Claim 1

Electrolytic manganese dioxide characterized in that the potential as measured in a 40 wt % KOH aqueous solution by using a mercury/mercury oxide reference electrode as a standard is higher than 250 mV and less than 310 mV, and the volume of pores having a pore diameter of at least 2 nm and at most 50 nm is at most 0.0055 cm3/g.

### Claim 2 (depends on 1)

The electrolytic manganese dioxide according to claim 1, wherein the volume of pores having a pore diameter of at least 2 nm and at most 200 nm is at most 0.0555 cm3/g.

### Claim 3 (depends on 1)

The electrolytic manganese dioxide according to claim 1, wherein the BET specific surface area is at least 12 m2/g and less than 36 m2/g.

### Claim 4 (depends on 1)

The electrolytic manganese dioxide according to claim 1, wherein the bulk density is at least 1.5 g/cm3.

### Claim 5 (depends on 1)

The electrolytic manganese dioxide according to claim 1, wherein the apparent particle density is at least 3.4 g/cm3.

### Claim 6 (depends on 1)

The electrolytic manganese dioxide according to claim 1, wherein the full width at half maximum of the diffraction line of the (110) plane in the vicinity of 2θ=22±1° in a XRD measurement pattern using CuKα radiation as the light source is at least 1.6° and at most 2.6°.

### Claim 7 (depends on 1)

A method for producing the electrolytic manganese dioxide as defined in claim 1, by suspending manganese oxide in a solution of sulfuric acid/manganese sulfate mixture, characterized in that manganese oxide particles are continuously mixed with the solution of sulfuric acid/manganese sulfate mixture, and electrolysis is carried out at a concentration of the manganese oxide particles in the solution of sulfuric acid/manganese sulfate mixture of at least 2.5 mg/L and at most 50 mg/L, at a sulfuric acid concentration in the solution of sulfuric acid/manganese sulfate mixture of at least 25 g/L and at most 55 g/L, at an electrolysis current density of at least 0.5 A/dm2 and at most 1.0 A/dm2.

### Claim 8 (depends on 7)

The method for producing the electrolytic manganese dioxide according to claim 7, wherein the electrolysis current density is at least 0.55 A/dm2 and at most 0.88 A/dm2.

### Claim 9 (depends on 7)

The method for producing the electrolytic manganese dioxide according to claim 7, wherein the concentration of the manganese oxide particles is higher than 3 mg/L and at most 30 mg/L.

### Claim 10 (depends on 7)

The method for producing the electrolytic manganese dioxide according to claim 7, wherein the sulfuric acid concentration at the termination of the electrolysis is higher than the sulfuric acid concentration at the initiation of the electrolysis.

### Claim 11 (depends on 1)

A cathode active material containing the electrolytic manganese dioxide as defined in claim 1.