# US 2015/0028354 A1 · Silicon Carbide Devices Having Smooth Channels

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0028354 A1
- Document ID: US20150028354A1
- Status: Published application
- Kind: A1
- Application number: 14/482,137
- Filed: 2014-09-10
- Published: 2015-01-29
- Earliest claimed: 2005-05-24
- Assignees: Cree, Inc.
- Applicants: Cree, Inc.
- Inventors: Mrinal K. Das; Michael Laughner
- Web page: https://patentgrep.com/patent/US20150028354A1

## CPC

- H10D 30/66: Vertical DMOS [VDMOS] FETs
- H10D 12/031: {of IGBTs}
- H10D 30/0291: {of vertical DMOS [VDMOS] FETs}
- H10D 62/156: {Drain regions of DMOS transistors}
- H10D 62/157: {Impurity concentrations or distributions}
- H10D 62/159: {Shapes}
- H10D 62/8325: {Silicon carbide}
- H10D 12/032: {of vertical IGBTs}
- Y10S 438/931: Silicon carbide semiconductor
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- Y10S: TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS

## Abstract

Methods of forming silicon carbide power devices are provided. An n− silicon carbide layer is provided on a silicon carbide substrate. A p-type silicon carbide well region is provided on the n− silicon carbide layer. A buried region of p+ silicon carbide is provided on the p-type silicon carbide well region. An n+ region of silicon carbide is provided on the buried region of p+ silicon carbide. A channel region of the power device is adjacent the buried region of p+ silicon carbide and the n+ region of silicon carbide. An n− region is provided on the channel region and a portion of the n− region is removed from the channel region so that a portion of the n− region remains on the channel region to provide a reduction in a surface roughness of the channel region.

## Claims

### Claim 1

A silicon carbide power device, comprising:
an n-type silicon carbide region;
a p-type silicon carbide region adjacent the n-type silicon carbide region; and
an n− silicon carbide region that provides a reduction in surface roughness of a channel region of the silicon carbide power device.

### Claim 2 (depends on 1)

The device of claim 1:
wherein the n-type silicon carbide region and p-type silicon carbide region include steps of up to several hundred angstroms in height on surfaces thereof; and
wherein the n− silicon carbide region is provided on the steps on the surfaces of the n-type silicon carbide region and p-type silicon carbide region, the presence of the n− silicon carbide region on the steps providing the reduction in surface roughness of the channel region of the silicon carbide power device.

### Claim 3 (depends on 2)

The device of claim 2, wherein the reduction in the surface roughness is a reduction in a root mean square (RMS) surface roughness of from at least about 28 Å to less than about 1.0 Å.

### Claim 4 (depends on 2)

The device of claim 2, wherein the channel region of the silicon carbide power device has a root mean square (RMS) surface roughness of less than about 1.0 Å.

### Claim 5 (depends on 2)

The device of claim 2, further comprising a gate insulating layer on the n-type silicon carbide layer and the p-type silicon carbide region, wherein the n− silicon carbide region fills in peaks and valleys on the surfaces of the n-type silicon carbide layer and the p-type silicon carbide region to provide a smoother interface between the channel region and a gate insulating layer.

### Claim 6 (depends on 2)

The device of claim 2, wherein the n− silicon carbide region has a thickness of from about 1000 to about 5000 Å.

### Claim 7 (depends on 2)

The device of claim 2, wherein the channel region of the silicon carbide includes the n-type silicon carbide region, the p-type silicon carbide region and the n− silicon carbide region.

### Claim 8 (depends on 2)

The device of claim 2, further comprising a sacrificial oxide layer on the channel region, wherein the presence and removal of the sacrificial oxide layer further reduces the RMS surface roughness of the channel region.

### Claim 9 (depends on 8)

The device of claim 8, wherein the RMS surface roughness of the surface of the channel region is no greater than about 0.7 Å.