# US 2015/0028011 A1 · System and method of controlling heat input in tandem hot-wire applications

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0028011 A1
- Document ID: US20150028011A1
- Status: Published application
- Kind: A1
- Application number: 13/949,828
- Filed: 2013-07-24
- Published: 2015-01-29
- Earliest claimed: 2013-07-24
- Assignees: Lincoln Global, Inc.
- Applicants: Lincoln Global, Inc.
- Inventors: Steven R. PETERS
- Web page: https://patentgrep.com/patent/US20150028011A1

## CPC

- B23K 9/09: Arrangements or circuits for arc welding with pulsed current or voltage
- B23K 9/02: Seam welding; Backing means; Inserts
- B23K 9/093: {the frequency of the pulses produced being modulable}
- B23K 9/1093: {Consumable electrode or filler wire preheat circuits}
- B23K 9/1735: {making use of several electrodes}
- B23K 26/348: in combination with arc heating, e.g. tungsten inert gas [TIG], metal inert gas [MIG] or plasma welding
- B23K: SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM

## Abstract

A system and method is provided. The system includes a high intensity energy source to create a molten puddle on a surface of a workpiece and a wire feeder that feeds a wire to the molten puddle via a contact tube. The system also includes a power supply that outputs a first heating current during a first mode of operation and a second heating current during a second mode of operation. The system further includes a controller that initiates the first mode of operation in the power supply to heat the wire to a desired temperature and switches the power supply from the first mode of operation to the second mode of operation to create a micro-arc. The second mode of operation provides at least one of an increased heat input to the molten puddle and an increased agitation of the molten puddle relative to the first mode of operation.

## Claims

### Claim 1

A welding system, said system comprising:
a high intensity energy source to create a molten puddle on a surface of a workpiece;
a wire feeder that feeds a wire to said molten puddle via a contact tube;
a power supply that outputs a first heating current during a first mode of operation and a second heating current during a second mode of operation, said power supply providing said first heating current or said second heating current to said wire via said contact tube; and
a controller that initiates said first mode of operation in said power supply to heat said wire to a desired temperature and switches said power supply from said first mode of operation to said second mode of operation to create micro-arcs, said micro-arcs created between said wire and said workpiece,
wherein said second mode of operation provides at least one of an increased heat input to said molten puddle and an increased agitation of said molten puddle relative to said first mode of operation, and
wherein said controller controls a frequency of micro-arcs during said second mode of operation by changing at least one of a current setpoint corresponding to a heating current segment of said second heating current and a ramp rate from a first current value of said second heating current to a second current value, said second current value corresponding to a current value needed to form a micro-arc.

### Claim 2 (depends on 1)

The welding system of claim 1, wherein said second current value is 1% to 10% above said current value needed to form said micro-arc.

### Claim 3 (depends on 1)

The welding system of claim 1, wherein said second heating current is one of a steady-state current, a pulsed DC current, and variable polarity current.

### Claim 4 (depends on 3)

The welding system of claim 3, wherein said second heating current is said pulsed DC current,
wherein said pulsed DC current comprises a series of pulses with each pulse of said series of pulses having a pulse current value, and
wherein said pulses of said series of pulses are separated by background current segments with each background current segment having a background current value that is lower than said pulse current values of adjacent pulses of said series of pulses.

### Claim 5 (depends on 4)

The welding system of claim 4, wherein said heating current segment is said pulse and said current setpoint is changed to control said frequency.

### Claim 6 (depends on 4)

The welding system of claim 4, wherein said heating current segment is said background current segment and said current setpoint is changed to control said frequency.

### Claim 7 (depends on 4)

The welding system of claim 4, wherein said first current value and said second current value correspond to average current values of said second heating current and said ramp rate between said first current value and said second current value is changed to control said frequency.

### Claim 8 (depends on 4)

The welding system of claim 4, wherein said creation of said micro-arc occurs for every nth pulse in said series of pulses.

### Claim 9 (depends on 5)

The welding system of claim 5, wherein said current setpoint is changed over said series of pulses.

### Claim 10 (depends on 6)

The welding system of claim 6, wherein said current setpoint is changed over said series of pulses.

### Claim 11

A method of welding, said method comprising:
creating a molten puddle on a surface of a workpiece;
feeding a wire to said molten puddle via a contact tube;
outputting a first heating current during a first mode of operation and a second heating current during a second mode of operation to said contact tube;
initiating said first mode of operation to heat said wire to a desired temperature;
switching from said first mode of operation to said second mode of operation to create micro-arcs, said micro-arcs created between said wire and said workpiece; and
controlling a frequency of micro-arcs during said second mode of operation by changing at least one of a current setpoint corresponding to a heating current segment of said second heating current and a ramp rate from a first current value of said second heating current to a second current value, said second current value corresponding to a current value needed to form a micro-arc,
wherein said second mode of operation provides at least one of an increased heat input to said molten puddle and an increased agitation of said molten puddle relative to said first mode of operation.

### Claim 12 (depends on 11)

The method of claim 11, wherein said second current value is 1% to 10% above said current value needed to form said micro-arc.

### Claim 13 (depends on 11)

The method of claim 11, wherein said second heating current is one of a steady-state current, a pulsed DC current, and variable polarity current.

### Claim 14 (depends on 13)

The method of claim 13, wherein said second heating current is said pulsed DC current,
wherein said pulsed DC current comprises a series of pulses with each pulse of said series of pulses having a pulse current value, and
wherein said pulses of said series of pulses are separated by background current segments with each background current segment having a background current value that is lower than said pulse current values of adjacent pulses of said series of pulses.

### Claim 15 (depends on 14)

The method of claim 14, wherein said heating current segment is said pulse and said current setpoint is changed to control said frequency.

### Claim 16 (depends on 14)

The method of claim 14, wherein said heating current segment is said background current segment and said current setpoint is changed to control said frequency.

### Claim 17 (depends on 14)

The method of claim 14, wherein said first current value and said second current value correspond to average current values of said second heating current and said ramp rate between said first current value and said second current value is changed to control said frequency.

### Claim 18 (depends on 14)

The method of claim 14, wherein said creation of said micro-arc occurs for every nth pulse in said series of pulses.

### Claim 19 (depends on 15)

The method of claim 15, wherein said current setpoint is changed over said series of pulses.

### Claim 20 (depends on 16)

The method of claim 16, wherein said current setpoint is changed over said series of pulses.