# US 2015/0027522 A1 · All-black-contact solar cell and fabrication method

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0027522 A1
- Document ID: US20150027522A1
- Status: Published application
- Kind: A1
- Application number: 14/241,762
- Filed: 2011-11-16
- Published: 2015-01-29
- Earliest claimed: 2011-11-16
- Assignees: Trina Solar Energy Development Pte Ltd
- Inventors: Thomas Mueller; Armin Gerhard Aberle
- Web page: https://patentgrep.com/patent/US20150027522A1

## CPC

- H10F 77/935: {for photovoltaic devices or modules}
- H10F 10/146: {Back-junction photovoltaic cells, e.g. having interdigitated base-emitter regions on the back side}
- H10F 71/129: {Passivating}
- H10F 77/219: {Arrangements for electrodes of back-contact photovoltaic cells}
- H10F 77/315: {the coatings being antireflective or having enhancing optical properties}
- H10F 77/703: {of the semiconductor bodies, e.g. textured active layers}
- Y02E 10/547: Monocrystalline silicon PV cells
- H10F: INORGANIC SEMICONDUCTOR DEVICES SENSITIVE TO INFRARED RADIATION, LIGHT, ELECTROMAGNETIC RADIATION OF SHORTER WAVELENGTH OR CORPUSCULAR RADIATION
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A method of fabricating an all-back-contact (ABC) solar cell is disclosed. A doped layer of a first polarity (102) is formed on a rear side of a wafer (100). A first masking structure (106, 110) is formed on the doped layer of the first polarity. Portions of the first masking structure (106, 110) are removed using a first laser ablation process. Doped regions of a second polarity (118, 135, 137) are formed in areas where the first masking structure has been removed. Contact bars (134, 136) are formed by screen printing and firing such that each contact bar is in contact with one of the doped regions (135, 137).

## Claims

### Claim 1

A method of fabricating an all-back-contact (ABC) solar cell comprising:
forming a doped layer of a first polarity on a rear side of a wafer;
forming a first masking structure on the doped layer of the first polarity;
removing portions of the first masking structure using a first laser ablation process;
forming doped regions of a second polarity in areas where the first masking structure has been removed; and
forming contact bars by screen printing and firing such that each contact bar is in contact with one of the doped regions.

### Claim 2 (depends on 1)

The method as claimed in claim 1, further comprising applying a first alignment process for the first laser ablation process; and applying a second corresponding alignment process for the screen printing of the contact bars.

### Claim 3 (depends on 1)

The method as claimed in claim 1, wherein forming the doped region of the second polarity comprises:
applying a caustic etch to expose deeper lying regions of the wafer in the openings formed in the first masking structure by the first laser ablation process, and
doping the exposed portions of the wafer.

### Claim 4 (depends on 1)

The method as claimed in claim 1, further comprising forming a dielectric passivation structure over the entire rear surface of the wafer.

### Claim 5 (depends on 4)

The method as claimed in claim 4, wherein forming the contact bars by screen printing comprises screen printing a fritted metal paste on the dielectric passivation structure and firing the fritted paste to form at least respective seed layers of the contact bars.

### Claim 6 (depends on 5)

The method as claimed in claim 5, wherein the fritted metal paste is screen printed such that the contact bars are in contact with the silicon wafer after the firing process.

### Claim 7 (depends on 5)

The method as claimed in claim 5, further comprising built-up of the contact bars from the seed layers using screen printing or ink-jet printing.

### Claim 8 (depends on 4)

The method as claimed in claim 4, wherein forming the contact bars by screen printing comprises forming openings in the dielectric passivation structure and screen printing a non-fritted metal paste to form the contact bars.

### Claim 9 (depends on 8)

The method as claimed in claim 8, wherein the openings in the dielectric passivation layer are formed by a second laser ablation process.

### Claim 10 (depends on 1)

The method as claimed in claim 1, wherein forming the doped layer of the first polarity comprises using diffusion doping from a solid or gaseous source, or ion implantation.

### Claim 11 (depends on 1)

The method as claimed in claim 1, wherein forming the doped regions of the second polarity comprises using diffusion doping from a solid or gaseous source, or ion implantation.

### Claim 12 (depends on 1)

The method as claimed in claim 1, further comprising texturing a front surface of the wafer.

### Claim 13 (depends on 1)

The method as claimed in claim 1, further comprising forming a dielectric structure on a front surface of the wafer.

### Claim 14 (depends on 13)

The method as claimed in claim 13, wherein the dielectric structure has passivation and anti-reflective properties.

### Claim 15 (depends on 1)

An all-back-contact (ABC) solar cell formed using the method as claimed in claim 1.

### Claim 16 (depends on 15)

The solar cell as claimed in claim 15, further comprising a dielectric passivation structure over the entire rear surface of the wafer.

### Claim 17 (depends on 15)

The solar cell as claimed in claim 15, further comprising a textured front surface of the wafer.

### Claim 18 (depends on 15)

The solar cell as claimed in claim 15, further comprising a dielectric stack on a front surface of the wafer.

### Claim 19 (depends on 18)

The solar cell as claimed in claim 18, wherein the dielectric stack has passivation and anti-reflective properties.