# US 2015/0020466 A1 · Method for manufacturing insulating glazing

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2015/0020466 A1
- Document ID: US20150020466A1
- Status: Published application
- Kind: A1
- Application number: 14/294,377
- Filed: 2014-06-03
- Published: 2015-01-22
- Earliest claimed: 2009-11-18
- Assignees: Agc Glass Europe
- Applicants: AGC Glass Europe
- Inventors: Olivier Bouesnard; Francois Closset
- Web page: https://patentgrep.com/patent/US20150020466A1

## CPC

- C03C 27/10: with the aid of adhesive specially adapted for that purpose
- B23K 31/02: relating to soldering or welding
- C03C 27/046: {of metals, metal oxides or metal salts only}
- C03C 27/08: with the aid of intervening metal
- C23C 4/01: Selective coating, e.g. pattern coating, without pre-treatment of the material to be coated
- E06B 3/673: Assembling the units (E06B3/677 takes precedence {; making hollow glass sheets or bricks C03B23/24})
- E06B 3/67334: {by soldering; Preparing the panes therefor}
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- B23K: SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- E06B: FIXED OR MOVABLE CLOSURES FOR OPENINGS IN BUILDINGS, VEHICLES, FENCES OR LIKE ENCLOSURES IN GENERAL, e.g. DOORS, WINDOWS, BLINDS, GATES (shades or blinds for greenhouses A01G9/22; curtains A47H; lids for car boots or bonnets B62D25/10; skylights E04B7/18; sunshades, awnings E04F10/00)

## Abstract

The Present invention relates to a method for manufacturing at least one portion of a seal ensuring gas-tightness between at least one first and one second glass panel in a glazing system, the method including the following steps: depositing a first adhesive layer on a first peripheral area of the first panel and a second adhesive layer on a second peripheral area of the second panel; welding a first metal seal element to the first adhesive layer; welding a second metal seal element or said first metal seal element to the second adhesive layer. According to the invention, the first and second adhesive layers are deposited using a high speed oxy-fuel flame-spraying method.

## Claims

### Claim 1

A process for manufacturing at least one portion of a seal ensuring gas-tightness between at least one first and one second glass panel in a glazing, the process comprises comprising:
preheating a first peripheral zone of the first panel and a second peripheral zone of the second panel to a temperature higher than 150° C.;
depositing, after said preheating, a first adhesion layer onto the first peripheral zone of the first panel and a second adhesion layer onto the second peripheral zone of the second panel;
welding a first metal seal element to the first adhesion layer; and
welding a second metal seal element or said first metal seal element to the second adhesion layer;
wherein depositing the first and second adhesion layers comprises a high-velocity oxy-fuel flame-spraying process.

### Claim 2 (depends on 1)

The process of claim 1, further comprising:
depositing a metal solder layer onto at least a portion of the first adhesion layer, the second adhesion layer, or both,
wherein a weld of the first metal seal element, the second metal seal element, or both is a fusion weld of the metal solder layer.

### Claim 3 (depends on 1)

The process of claim 1, wherein at least a portion of the welding is ultrasonic or induction welding.

### Claim 4 (depends on 1)

The process of claim 1, wherein the glazing is a vacuum glazing.

### Claim 5 (depends on 1)

The process of claim 1, comprising welding a second metal seal element to the second adhesion layer,
wherein the process further comprises welding the first metal seal element to the second metal seal element.

### Claim 6 (depends on 1)

The process of claim 1, further comprising:
exposing the first adhesion layer, the second adhesion layer, or both to a carburising flame before welding to that adhesion layer.

### Claim 7 (depends on 1)

The process of claim 1, wherein the first and second adhesion layers each comprise at least one adhesive material selected from the group consisting of copper, copper alloy, aluminum, aluminum alloy, iron, iron alloy, platinum, platinum alloy, titanium, titanium alloy, tin, and tin alloy.

### Claim 8 (depends on 1)

The process of claim 1, wherein the first and second adhesion layers each comprise an adhesive material that has a coefficient of thermal expansion of 3 to 23×10−6 K−1.

### Claim 9 (depends on 1)

The process of claim 1, further comprising:
exposing the first adhesion layer, the second adhesion layer, or both to a soldering flux before welding, before depositing a metal solder layer, or before both.

### Claim 10 (depends on 1)

The process of claim 1, wherein the first metal seal element, the second metal seal element, or both, comprises a metal weld layer prior to welding to the first or second adhesion layer.

### Claim 11 (depends on 1)

The process of claim 1,
wherein the depositing the first and second adhesion layers is in an atmosphere at atmospheric pressure;
welding the first metal seal element to the first adhesion layer is in an atmosphere at atmospheric pressure;
the process comprises welding a second metal seal element distinct from the first metal seal element to the second adhesion layer in an atmosphere at atmospheric pressure; and
the process further comprises welding the first metal seal element to the second metal seal element in an atmosphere at reduced pressure or under vacuum.

### Claim 12 (depends on 1)

The process of claim 1, wherein the first and second metal seal elements each comprise at least one material selected from the group consisting of copper, copper alloy, aluminum, aluminum alloy, iron, and iron alloy.

### Claim 13 (depends on 1)

The process of claim 1, wherein the first and second metal seal elements, an adhesive material of the first and second adhesion layers, or both comprise an iron alloy comprising iron in a content of 53-55% wt., nickel in a content of 28-30% wt., and cobalt in a content of 16-18% wt.

### Claim 14 (depends on 1)

The process of claim 1,
wherein the high-velocity oxy-fuel flame-spraying process employs a spraying assembly comprising a first inlet, a second inlet, a third inlet, and an outlet,
wherein the first, second, and third inlets lead to a combustion chamber,
and wherein the high-velocity oxy-fuel flame-spraying process comprises:
injecting, under pressure, a fuel and oxygen through the first inlet;
injecting an adhesive material into the second inlet;
combusting the fuel and the oxygen, thereby melting the adhesive material in the combustion chamber;
injecting a gas under pressure through the third inlet of the spraying assembly, thereby enabling spraying of the molten adhesive material from the assembly via the outlet at a supersonic speed; and
orienting the outlet of the assembly towards a peripheral zone, thereby enabling formation of an adhesion layer.

### Claim 15 (depends on 14)

The process of claim 14, wherein an angle between an axis of the outlet and the glass panel is from 45° to 90°.

### Claim 16 (depends on 14)

The process of claim 14,
wherein the high-velocity oxy-fuel flame-spraying process comprises moving the spraying assembly and the glass panel relative to one another at a speed of from 5 to 30 m/min.

### Claim 17 (depends on 1)

The process of claim 1, wherein the first and second peripheral zones of the first and second panels are on a respective edge of the first and second panels.

### Claim 18 (depends on 1)

A glazing, obtained by a process comprising the process of claim 1.

### Claim 19 (depends on 15)

The process of claim 15, wherein the angle between the axis of the outlet and the glass panel is from 70° to 90°.

### Claim 20 (depends on 16)

The process of claim 16, wherein the high-velocity oxy-fuel flame-spraying process comprises moving the spraying assembly and the glass panel relative to one another at a speed of from 5 to 20 m/min.