# US 2014/0349478 A1 · Method including an etching of a portion of an interlayer dielectric in a semiconductor structure, a degas process and a preclean process

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2014/0349478 A1
- Document ID: US20140349478A1
- Status: Published application
- Kind: A1
- Application number: 13/901,739
- Filed: 2013-05-24
- Published: 2014-11-27
- Earliest claimed: 2013-05-24
- Assignees: Globalfoundries Inc.
- Applicants: GLOBALFOUNDRIES Inc.
- Inventors: Frank Koschinsky; Bernd Hintze; Oliver Witnik
- Web page: https://patentgrep.com/patent/US20140349478A1

## CPC

- H10W 20/081: {by forming openings in the dielectric parts}
- H10P 70/234: {the processing being the formation of vias or contact holes}
- H10W 20/096: {by contacting with gases, liquids or plasmas}
- H10W 20/097: {by thermally treating}
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A method includes providing a semiconductor structure. The semiconductor structure includes a substrate having a frontside and a backside, an electrically conductive feature including copper provided at the frontside of the substrate and a low-k interlayer dielectric provided over the electrically conductive feature. A portion of the interlayer dielectric is etched. In the etch process, a surface of the electrically conductive feature is exposed. A degas process is performed, wherein the semiconductor structure is exposed to a first gas, and wherein the semiconductor structure is heated from the backside and from the frontside. A preclean process may be performed. The preclean process may include a first phase wherein the semiconductor structure is exposed to a substantially non-ionized second gas and a second phase wherein the semiconductor structure is exposed to a plasma created from the second gas.

## Claims

### Claim 1

A method, comprising:
providing a semiconductor structure, the semiconductor structure comprising a substrate having a frontside and a backside, an electrically conductive feature comprising copper provided at said frontside of said substrate and a low-k interlayer dielectric provided over said electrically conductive feature;
etching a portion of said interlayer dielectric, a surface of said electrically conductive feature being exposed in the etch process;
performing a degas process, wherein said semiconductor structure is exposed to a first gas, and wherein said semiconductor structure is heated from said backside and from said frontside; and
performing a preclean process, said preclean process comprising at least one of exposing said semiconductor structure to a substantially non-ionized second gas and using a plasma created from said second gas.

### Claim 2 (depends on 1)

The method of claim 1, wherein said preclean process comprises a first phase wherein said semiconductor structure is exposed to said substantially non-ionized second gas and a second phase wherein said plasma created from said second gas is used.

### Claim 3 (depends on 1)

The method of claim 1, wherein said first gas comprises at least one of argon, hydrogen, nitrogen, a hydrocarbon and ammonia.

### Claim 4 (depends on 3)

The method of claim 3, wherein said semiconductor structure is heated from an initial temperature to approximately a first process temperature during a first phase of said degas process, and wherein said semiconductor structure is maintained at approximately said first process temperature during a second phase of said degas process, a duration of said first phase of said degas process being shorter than about one half of a total duration of said degas process.

### Claim 5 (depends on 4)

The method of claim 4, wherein said first process temperature is at least one of within a range from about 250-350° C., within a range from about 275-325° C., within a range from about 290-310° C., and approximately equal to 300° C.

### Claim 6 (depends on 5)

The method of claim 5, wherein said initial temperature is at least one of within a range from about 100-200° C., within a range from about 125-175° C., within a range from about 140-160° C., and approximately equal to 150° C.

### Claim 7 (depends on 6)

The method of claim 6, further comprising a preheating process wherein said semiconductor structure is heated from about room temperature to said initial temperature before said degas process.

### Claim 8 (depends on 4)

The method of claim 4, wherein said total duration of said degas process is less than about 120 seconds.

### Claim 9 (depends on 8)

The method of claim 8, wherein said total duration of said degas process is at least one of within a range from about 30-90 seconds, within a range from about 40-80 seconds, within a range from about 50-70 seconds, approximately equal to 45 seconds and approximately equal to 60 seconds.

### Claim 10 (depends on 2)

The method of claim 2, wherein said second gas comprises hydrogen.

### Claim 11 (depends on 10)

The method of claim 10, wherein said plasma created from said second gas is a remote plasma.

### Claim 12 (depends on 11)

The method of claim 11, wherein a duration of said second phase of said preclean process is at least one of within a range from about one-fourth of a total duration of said preclean process to about three-fourths of said total duration of said preclean process, within a range from about one-third of said total duration of said preclean process to about two-thirds of said total duration of said preclean process, approximately equal to one-third of said total duration of said preclean process and approximately equal to one-half of said total duration of said preclean process.

### Claim 13 (depends on 12)

The method of claim 12, wherein said semiconductor structure is heated from said backside during said preclean process.

### Claim 14 (depends on 13)

The method of claim 13, wherein said semiconductor structure is heated to a second process temperature during said preclean process, wherein said second process temperature is at least one of within a range from about 260-360° C., within a range from about 285-335° C., within a range from about 300-320° C., and approximately equal to 310° C.

### Claim 15 (depends on 4)

The method of claim 4, wherein said first gas comprises at least one of hydrogen, nitrogen, a hydrocarbon and ammonia.

### Claim 16 (depends on 3)

The method claim 3, wherein said first gas is preheated to approximately said first process temperature.

### Claim 17 (depends on 1)

The method of claim 1, wherein said low-k interlayer dielectric comprises at least one of a porous silicon dioxide, a carbon-doped silicon dioxide, a porous carbon-doped silicon dioxide, a polyimide, a polynorbornene, a benzozyclobutene, a polytetraflouroethylene, a carbon-doped silicon nitride, a porous carbon-doped silicon nitride, a fluorine-doped silicon dioxide, a porous fluorine-doped silicon dioxide, silsesquioxane and methylsilsesquioxane.

### Claim 18 (depends on 1)

The method of claim 1, wherein said degas process is performed in a first chamber of a semiconductor processing tool and said preclean process is performed in a second chamber of said semiconductor processing tool.

### Claim 19

A method, comprising:
providing a semiconductor structure, said semiconductor structure comprising a substrate having a frontside and a backside, an electrically conductive feature comprising copper provided at said frontside of said substrate and a low-k interlayer dielectric provided over said electrically conductive feature;
etching a portion of said interlayer dielectric, a surface of said electrically conductive feature being exposed in the etch process; and
performing a degas process, wherein said semiconductor structure is exposed to a substantially non-ionized gas comprising at least one of hydrogen, nitrogen, a hydrocarbon and ammonia.

### Claim 20 (depends on 19)

The method of claim 19, wherein said gas is preheated to approximately a process temperature of said degas process.

### Claim 21 (depends on 20)

The method of claim 20, wherein said semiconductor structure is heated from an initial temperature to approximately said process temperature of said degas process during a first phase of said degas process, and wherein said semiconductor structure is maintained at approximately said process temperature of said degas process during a second phase of said degas process, a duration of said first phase of said degas process being shorter than about one-half of a total duration of said degas process.

### Claim 22

A method, comprising:
providing a semiconductor structure, said semiconductor structure comprising a substrate having a frontside and a backside, an electrically conductive feature comprising copper provided at said frontside of said substrate and an ultra-low-k interlayer dielectric having a dielectric constant of 3 or less provided over said electrically conductive feature;
etching a portion of said interlayer dielectric, a surface of said electrically conductive feature being exposed in the etch process;
performing a degas process, wherein said semiconductor structure is exposed to argon, and wherein said semiconductor structure is heated from said backside and from said frontside, wherein said semiconductor structure is heated from an initial temperature to approximately a first process temperature during a first phase of said degas process, and wherein said semiconductor structure is maintained at approximately said first process temperature during a second phase of said degas process, a duration of said first phase of said degas process being shorter than about one-half of a total duration of said degas process, said first process temperature being in a range from about 290-310° C., said total duration of said degas process being in a range from about 50-70 seconds; and
performing a preclean process, said preclean process comprising a first phase wherein said semiconductor structure is exposed to substantially non-ionized hydrogen and a second phase wherein a remote hydrogen plasma is used, a duration of said second phase of said preclean process being in a range from about one-quarter of a total duration of said preclean process to about one-half of said total duration of said preclean process, said total duration of said preclean process being in a range from about 30-50 seconds, wherein said semiconductor structure is heated to a second process temperature in a range from about 300-320° C. during said preclean process.