# US 2014/0349184 A1 · Binder Composition For An Electrode And Methods For Producing The Same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2014/0349184 A1
- Document ID: US20140349184A1
- Status: Published application
- Kind: A1
- Application number: 14/283,889
- Filed: 2014-05-21
- Published: 2014-11-27
- Earliest claimed: 2013-05-23
- Assignees: Hercules Corporated
- Applicants: Hercules Corporated
- Inventors: Sung Gun Chu; Alan E Goliaszewski
- Web page: https://patentgrep.com/patent/US20140349184A1

## CPC

- H01M 4/622: {being polymers}
- C08L 1/286: {substituted with acid radicals, e.g. carboxymethyl cellulose [CMC] (C08L1/282 takes precedence)}
- C08L 9/10: Latex (C08L9/04, C08L9/08 take precedence)
- C08L 25/14: with unsaturated esters
- C08L 33/00: Compositions of homopolymers or copolymers of compounds having one or more unsaturated aliphatic radicals, each having only one carbon-to-carbon double bond, and only one being terminated by only one carboxyl radical, or of salts, anhydrides, esters, amides, imides or nitriles thereof; Compositions of derivatives of such polymers
- C09J 101/28: Alkyl ethers
- C09J 101/284: {with hydroxylated hydrocarbon radicals}
- C09J 101/286: {substituted with acid radicals (C09J101/282 takes precedence)}
- H01M 4/13: Electrodes for accumulators with non-aqueous electrolyte, e.g. for lithium-accumulators; Processes of manufacture thereof
- H01M 4/139: Processes of manufacture
- C08L 2201/52: Aqueous emulsion or latex, e.g. containing polymers of a glass transition temperature (Tg) below 20°C
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- C09J: ADHESIVES; NON-MECHANICAL ASPECTS OF ADHESIVE PROCESSES IN GENERAL; ADHESIVE PROCESSES NOT PROVIDED FOR ELSEWHERE; USE OF MATERIALS AS ADHESIVES (preparation of glue or gelatine C09H)
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

The presently disclosed and/or claimed inventive process(es), procedure(s), method(s), product(s), result(s), and/or concept(s) (collectively hereinafter referred to as the “presently disclosed and/or claimed inventive concept(s)”) relates generally to the composition of a binder for use in battery electrodes and methods of preparing such. More particularly, but not by way of limitation, the presently disclosed and/or claimed inventive concept(s) relates to a binder composition containing an ionizable water soluble polymer and a redispersible powder containing a latex, a protective colloid, and an anticaking agent for use in the production and manufacture of electrodes of a lithium ion battery. Additionally, the presently disclosed and/or claimed inventive concept(s) relates generally to the compositions and methods of making electrodes, both anodes and cathodes, with a binder composition containing an ionizable water soluble polymer and a redispersible powder.

## Claims

### Claim at position 1

1-61. (canceled)

### Claim 62

A binder precursor composition for use in preparation of a lithium ion battery comprising:
an ionizable water soluble polymer; and
a redispersible powder comprising a protective colloid, an anticaking agent, and a latex polymer.

### Claim 63 (depends on 62)

The binder precursor composition of claim 62, wherein the ionizable water soluble polymer is present in the binder precursor composition in a range of from about 2% to about 75% by weight and the redispersible powder is present in the binder precursor composition in a range of from about 25% to about 98% by weight.

### Claim 64 (depends on 62)

The binder precursor composition of claim 62, wherein the protective colloid is present in the redispersible powder in a range of about 0.1% to about 10% by weight.

### Claim 65 (depends on 62)

The binder precursor composition of claim 62, wherein the anticaking agent is present in the redispersible powder in a range of about 1% to about 35% by weight.

### Claim 66 (depends on 62)

The binder precursor composition of claim 62, wherein the latex polymer is present in the redispersible powder in a range of about 30% to about 98.9% by weight.

### Claim 67 (depends on 62)

The binder precursor composition of claim 62, wherein the ionizable water soluble polymer is selected from the group consisting of a hydrophilically modified cellulose material, a polyacrylic acid, a polyacrylic acid copolymer, and combinations thereof.

### Claim 68 (depends on 67)

The binder precursor composition of claim 67, wherein the hydrophilically modified cellulose material is selected from carboxyalkyl cellulose and hydroxyalkyl cellulose.

### Claim 69 (depends on 68)

The binder precursor composition of claim 68, wherein the carboxyalkyl cellulose comprises carboxymethyl cellulose.

### Claim 70 (depends on 62)

The binder precursor composition of claim 62, wherein the protective colloid is selected from the group consisting of polyvinyl alcohol, polyvinyl acetate, a hydroxyalkyl cellulose polymer, and combinations thereof.

### Claim 71 (depends on 62)

The binder precursor composition of claim 62, wherein the anticaking agent is selected from the group consisting of calcium carbonate, kaolin, silica, carbon, lithium carbonate, and combinations thereof.

### Claim 72 (depends on 62)

The binder precursor composition of claim 62, wherein the latex polymer is selected from the group consisting of styrene butadiene, vinyl acetate ethylene, styrene acrylic, vinyl acrylic, ethylene vinylversatate, and combinations thereof.

### Claim 73 (depends on 62)

The binder precursor composition of claim 62, wherein the redispersible powder is in the form of particles, and wherein the average diameter of the particles is less than about 500 μm.

### Claim 74 (depends on 62)

The binder precursor composition of claim 62 further comprising an electrode active material.

### Claim 75 (depends on 74)

The binder precursor composition of claim 74, wherein the ionizable water soluble polymer is present in the binder precursor composition in a range of from about 0.25% to about 2.25% by weight, the redispersible polymer is present in the binder precursor composition in a range of from about 0.25% to about 3.5% by weight, and the electrode active material is present in the binder precursor composition in a range of from about 94.25% to about 99.5% by weight.

### Claim 76 (depends on 74)

The binder precursor composition of claim 74, wherein the electrode active material is an anode active material selected from the group consisting of 1) a carbonaceous material, 2) a silicon-based alloy, 3) a complex compound comprising a carbonaceous material and a metal selected from the group consisting of Al, Ag, Bi, In, Ge, Mg, Pb, Si, Sn, Ti, and combinations thereof, 4) a lithium complex metal oxide, 5) a lithium-containing nitride, and (6) combinations thereof.

### Claim 77

The binder precursor composition of 74, wherein the electrode active material is a cathode active material selected from the group consisting of lithium-containing transition metal oxides.

### Claim 78 (depends on 62)

An aqueous slurry composition formed by adding the binder precursor composition of claim 62 to water.

### Claim 79 (depends on 78)

The aqueous slurry composition of claim 78, wherein the slurry has a Brookfield viscosity in a range of from about 1,000 cps to about 15,000 cps at a shear rate in a range of from about 10 s−1 to about 40 s−1 at 25° C.

### Claim 80

An electrode for a lithium ion battery comprising:
a film comprising: (1) an electrode active material, and (2) a binder comprising an ionizable water soluble polymer, a protective colloid, an anticaking agent, and a latex polymer; and
a current collector.

### Claim 81 (depends on 80)

The electrode of claim 80, wherein the ionizable water soluble polymer is present in the film in a range of from about 0.25% to about 2.25% by weight, the protective colloid is present in the film in a range of from about 0.05% to about 0.2% by weight, the anticaking agent is present in the film in a range of from about 0.1% to about 0.5% by weight, the latex polymer is present in the film in a range of from about 0.5% to about 4% by weight, and the electrode active material is present in the film in a range of from about 94.25% to about 99.5% by weight.

### Claim 82 (depends on 80)

The electrode of claim 80, wherein the current collector comprises a metal selected from the group consisting of aluminum, copper, and combinations thereof.

### Claim 83 (depends on 80)

The electrode of claim 80, wherein a surface of the film is bound to a surface of the current collector forming a bond, wherein the adhesive strength of the bond is at least about 0.3 gf/mm as determined by 90 Degree Peel Adhesion Test.

### Claim 84 (depends on 80)

The electrode of claim 80, wherein the capacity retention percentage of the electrode at a C-Rate of 0.5 C and at 25° C. for 50 cycles is greater than about 80, and wherein the film thickness is in a range of from about 30 to about 100 μm.

### Claim 85 (depends on 80)

The electrode of claim 80, wherein the impedance of the electrode is less than about 300, and wherein the thickness of the film is less than about 70 μm.