# US 2014/0275357 A1 · Asphalt including modified toner based additive

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2014/0275357 A1
- Document ID: US20140275357A1
- Status: Published application
- Kind: A1
- Application number: 14/205,697
- Filed: 2014-03-12
- Published: 2014-09-18
- Earliest claimed: 2013-03-15
- Assignees: Close the Loop Technologies Pty Ltd.
- Applicants: Close the Loop Technologies Pty Ltd.
- Inventors: Steve Morriss
- Web page: https://patentgrep.com/patent/US20140275357A1

## CPC

- C08K 11/00: Use of ingredients of unknown constitution, e.g. undefined reaction products
- C04B 26/26: Bituminous materials, e.g. tar, pitch {(C08L95/00 takes precedence)}
- C04B 40/0039: {Premixtures of ingredients}
- C08K 3/34: Silicon-containing compounds
- C08K 3/346: {Clay}
- C09D 195/00: Coating compositions based on bituminous materials, e.g. asphalt, tar, pitch
- C09J 195/00: Adhesives based on bituminous materials, e.g. asphalt, tar, pitch
- E04D 7/00: Roof covering {exclusively consisting of} sealing masses applied in situ; Gravelling of flat roofs
- C04B 2111/00586: {Roofing materials}
- E04D 1/20: of plastics; {of asphalt;} of fibrous materials
- Y02W 30/91: Use of waste materials as fillers for mortars or concrete
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- C09D: COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR (cosmetics A61K; processes for applying liquids or other fluent materials to surfaces, in general, B05D; staining wood B27K5/02; glazes or vitreous enamels C03C; natural resins, French polish, drying-oils, driers, turpentine, per se, C09F; polishing compositions other than French polish, ski waxes C09G; adhesives or use of materials as adhesives C09J; materials for sealing or packing joints or covers C09K3/10; materials for stopping leaks C09K3/12; processes for the electrolytic or electrophoretic production of coatings C25D)
- C09J: ADHESIVES; NON-MECHANICAL ASPECTS OF ADHESIVE PROCESSES IN GENERAL; ADHESIVE PROCESSES NOT PROVIDED FOR ELSEWHERE; USE OF MATERIALS AS ADHESIVES (preparation of glue or gelatine C09H)
- E04D: ROOF COVERINGS; SKY-LIGHTS; GUTTERS; ROOF-WORKING TOOLS (coverings of outer walls by plaster or other porous material E04F13/00)
- Y02W: CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO WASTEWATER TREATMENT OR WASTE MANAGEMENT

## Abstract

An asphalt and asphalt concrete incorporating a modified toner based additive are provided.

## Claims

### Claim 1

An asphalt incorporating a modified toner based additive.

### Claim 2 (depends on 1)

The asphalt of claim 1, including between 40 and 99.8 weight percent bitumen and between 0.2 and 60 weight percent modified toner based additive.

### Claim 3 (depends on 2)

The asphalt of claim 2, wherein said modified toner based additive includes a mixture of:
between 18 and 98 weight percent toner; and
between 2 and 82 weight percent of a material selected from a group consisting of a gelling clay, a reactive agent, an elastomer, a functional filler, a handling and agglomerating agent and mixtures thereof.

### Claim 4 (depends on 3)

The asphalt of claim 3, wherein said gelling clay is selected from a group consisting of montmorillonite clay, kaolin clay, calcined kaolin clay, gilsonite clay, bentonite clay, attapulgite clay and mixtures thereof.

### Claim 5 (depends on 4)

The asphalt of claim 4, wherein said reactive agent is selected from a group consisting of a peroxide, hydrogen peroxide, benzoyl peroxide, a sulfur containing compound, sulfuric acid, sulfur and mixtures thereof.

### Claim 6 (depends on 5)

The asphalt of claim 5, wherein said elastomer is selected from a group consisting of latex rubber, crumb rubber, ground tire rubber, waste water-based paint and mixtures thereof.

### Claim 7 (depends on 6)

The asphalt of claim 6, wherein said functional filler is selected from a group consisting of fly ash, bag house fines, ash, carbon black and mixtures thereof.

### Claim 8 (depends on 7)

The asphalt of claim 7, wherein said handling and agglomerating agent is selected from a group consisting of an oil a wax, soybean oil, linseed oil, engine oil, recycled engine oil, vegetable oil, engineering oil, recycled engineering oil, ship oil, recycled ship oil, olive oil, hydraulic oil, hydrogenated castor oil (HCO), hydrogenated palm oil, stearic acid, sasol C80, montan E, paraffin, carnauba wax, slack wax, sasol H1, recycled PE wax, sasobit, microcrystalline wax and mixtures thereof.

### Claim 9 (depends on 3)

The asphalt of claim 3, wherein said modified toner based additive includes a first component selected from a first group consisting of an oil, a wax, soybean oil, linseed oil, engine oil, recycled engine oil, vegetable oil, engineering oil, recycled engineering oil, ship oil, recycled ship oil, olive oil, hydraulic oil, hydrogenated castor oil (HCO), hydrogenated palm oil, stearic acid, sasol C80, montan E, paraffin, carnauba wax, slack wax, sasol H1, recycled PE wax, sasobit, microcrystalline wax, ash, fly ash, bag house fines, carbon black, kaolin clay, calcined kaolin clay, clay, gilsonite, montmorillonite clay, bentonite clay, attapulgite clay and mixtures thereof and a second elastomeric component selected from a second group consisting of an elastomer, crumb rubber, latex rubber, waste water-based paint, ground tire rubber and mixtures thereof.

### Claim 10 (depends on 9)

The asphalt of claim 9, wherein a weight percent ratio of said first component to said second elastomeric component in said modified toner based additive is between 1 to 1 and 1 to 10.

### Claim 11 (depends on 9)

The asphalt of claim 9 wherein a weight percent ratio of toner to second elastomeric component in said additive is between 1 to 1 and 1 to 6.

### Claim 12 (depends on 1)

The asphalt of claim 1 wherein said modified toner based additive includes a weight percent ratio of toner to elastomer of between 1 to 1 and 1 to 6 so as to provide a single asphalt additive with a proper balance between plastomeric properties of said toner and elastomeric properties of said elastomer to improve both high temperature and low temperature performance of said asphalt.

### Claim 13 (depends on 3)

The asphalt of claim 3, wherein said modified toner based additive mixture includes between 0.1 and 7.0 weight percent compatibilizer.

### Claim 14 (depends on 13)

The asphalt of claim 13, wherein said compatibilizer is selected from a group of materials consisting of maleic anhydride (MAH) grafted polymer, benzoyl peroxide (BPO), polyphosphoric acid (PPA), trans polyoctenamer rubber (TOR) and mixtures thereof.

### Claim 15

An asphalt concrete incorporating a modified toner based additive comprising a toner/elastomer composite.

### Claim 16 (depends on 15)

The asphalt concrete of claim 15, including between 70-94.8 weight percent aggregate, between 5 and 15 weight percent bitumen and between 0.2 and 10 weight percent modified toner based additive.

### Claim 17 (depends on 16)

The asphalt concrete of claim 16, wherein said modified toner based additive includes a mixture of:
between 98 and 18 weight percent toner; and
between 2 and 82 weight percent of a material selected from a group consisting of a gelling clay, a reactive agent, an elastomer, a functional filler, a handling and agglomerating agent and mixtures thereof.

### Claim 18 (depends on 17)

The asphalt concrete of claim 17, wherein:
said gelling clay is selected from a group consisting of montmorillonite clay, kaolin clay, calcined kaolin clay, gilsonite clay, bentonite clay, attapulgite clay and mixtures thereof;
said reactive agent is selected from a group consisting of a peroxide, hydrogen peroxide, benzoyl peroxide, a sulfur containing compound, sulfuric acid, sulfur and mixtures thereof;
said elastomer is selected from a group consisting of latex rubber, crumb rubber, ground tire rubber, waste water-based paint and mixtures thereof;
said functional filler is selected from a group consisting of fly ash, bag house fines, ash, carbon black and mixtures thereof; and
said handling and agglomerating agent is selected from a group consisting of an oil a wax, soybean oil, linseed oil, engine oil, recycled engine oil, vegetable oil, engineering oil, recycled engineering oil, ship oil, recycled ship oil, olive oil, hydraulic oil, hydrogenated castor oil (HCO), hydrogenated palm oil, stearic acid, sasol C80, montan E, paraffin, carnauba wax, slack wax, sasol H1, recycled PE wax, sasobit, microcrystalline wax and mixtures thereof.

### Claim 19 (depends on 15)

The asphalt concrete of claim 15, wherein said modified toner based additive includes a first component selected from a group consisting of an oil, a wax, soybean oil, linseed oil, engine oil, recycled engine oil, vegetable oil, engineering oil, recycled engineering oil, ship oil, recycled ship oil, olive oil, hydraulic oil, hydrogenated castor oil (HCO), hydrogenated palm oil, stearic acid, sasol C80, montan E, paraffin, carnauba wax, slack wax, sasol H1, recycled PE wax, sasobit, microcrystalline wax, ash, fly ash, bag house fines, carbon black, kaolin clay, calcined kaolin clay, clay, montmorillonite clay, gilsonite clay, bentonite clay, attapulgite clay and mixtures thereof and a second elastomeric component selected from a group consisting of an elastomer, crumb rubber, latex rubber, waste water-based paint, ground tire rubber and mixtures thereof.

### Claim 20 (depends on 19)

The asphalt concrete of claim 19, wherein a weight percent ratio of said first component to said second component in said additive is between 1 to 1 and 1 to 10.

### Claim 21 (depends on 19)

The asphalt concrete of claim 19, wherein a weight percent ratio of toner to second component in said additive is between 1 to 1 and 1 to 6.

### Claim 22 (depends on 15)

The asphalt concrete of claim 15, wherein said modified toner based additive includes a weight percent ratio of toner to elastomer of between 1 to 1 and 1 to 6 so as to provide a single asphalt additive with a proper balance between plastomeric properties of said toner and elastomeric properties of said elastomer to improve both high temperature and low temperature performance of said asphalt.

### Claim 23 (depends on 17)

The asphalt concrete of claim 17, wherein said modified toner based additive mixture includes between 0.1 and 7.0 weight percent compatibilizer.

### Claim 24 (depends on 23)

The asphalt concrete of claim 23, wherein said compatibilizer is selected from a group of materials consisting of a maleic anhydride (MAH) grafted polymer, benzoyl peroxide (BPO), polyphosphoric acid (PPA), transpolyoctenamer rubber (TOR) and mixtures thereof.