# US 2014/0273509 A1 · Method and Apparatus for Planarization of Substrate Coatings

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2014/0273509 A1
- Document ID: US20140273509A1
- Status: Published application
- Kind: A1
- Application number: 13/800,627
- Filed: 2013-03-13
- Published: 2014-09-18
- Earliest claimed: 2013-03-12
- Assignees: Taiwan Semiconductor Manufacturing Company, Ltd.
- Inventors: Wen-Yun Wang; Cheng-Han Wu; Yu-Chung Su; Ching-Yu Chang
- Web page: https://patentgrep.com/patent/US20140273509A1

## CPC

- H10P 72/0418: {for etching}
- B05B 12/02: for controlling time, or sequence, of delivery
- B05B 13/0228: {the movement of the objects being rotative (B05B13/0242 takes precedence)}
- G03F 7/162: {Coating on a rotating support, e.g. using a whirler or a spinner}
- H10P 14/6342: {Liquid deposition, e.g. spin-coating, sol-gel techniques or spray coating}
- H10P 72/0406: {for cleaning followed by drying, rinsing, stripping, blasting or the like}
- H10P 72/0448: {Apparatus for applying a liquid, a resin, an ink or the like}
- H10P 76/204: {of organic photoresist masks}
- H10P 95/064: {the removal being chemical etching}
- H10P 95/08: {Planarisation of organic insulating materials}
- B05D 1/005: {Spin coating}
- H10P 95/06: {Planarisation of inorganic insulating materials}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- B05B: SPRAYING APPARATUS; ATOMISING APPARATUS; NOZZLES (spray-mixers with nozzles B01F25/72; processes for applying liquids or other fluent materials to surfaces by spraying B05D)
- G03F: PHOTOMECHANICAL PRODUCTION OF TEXTURED OR PATTERNED SURFACES, e.g. FOR PRINTING, FOR PROCESSING OF SEMICONDUCTOR DEVICES; MATERIALS THEREFOR; ORIGINALS THEREFOR; APPARATUS SPECIALLY ADAPTED THEREFOR; (phototypographic composing devices B41B; photosensitive materials or processes for photographic purposes G03C; electrophotography, sensitive layers or processes therefor G03G)
- B05D: PROCESSES FOR APPLYING FLUENT MATERIALS TO SURFACES, IN GENERAL (conveying articles or workpieces through baths of liquid B65G, e.g. B65G49/02)

## Abstract

Disclosed herein is a method of forming a coating, comprising applying a first coating to a substrate having a plurality of topographical features, planarizing a top surface of the first coating, and drying the coating after planarizing the top surface of the first coating. The first coating may be applied over the plurality of topographical features, and substantially liquid during application. The first coating may optionally be a conformal coating over topographical features of the substrate. The conformal coating may be dried prior to planarizing the top surface of the first coating and a solvent applied to the conformal coating, with the top surface of the conformal coating being substantially planar after application of the solvent. The coating may have a planar surface prior to the drying the first coating and the first coating may be dried without substantial spin-drying by modifying an environment of the first coating.

## Claims

### Claim 1

A method of forming a coating, comprising:
applying a first coating to a substrate;
drying the first coating after the applying the first coating;
applying a solvent to the first coating after the drying the first coating after application of the first coating, the top surface of the first coating achieving a substantially planar state after application of the solvent; and
drying the first coating after application of the solvent, the first coating having a substantially planar top surface after drying;
wherein the top surface of the first coating is planarized before drying the first coating.

### Claim 2 (depends on 1)

The method of claim 1, wherein the first coating is applied as a conformal coating.

### Claim 3 (depends on 2)

The method of claim 2, wherein applying the solvent comprises reflowing at least a top portion of the first coating.

### Claim 4 (depends on 3)

The method of claim 3, further comprising spinning the substrate at a first speed during application of the first coating and spinning the substrate at a second speed lower than the first speed during the drying the first coating.

### Claim 5 (depends on 3)

The method of claim 3, wherein the drying the coating after application of the solvent comprises drying the first coating through modifying an environment of the first coating.

### Claim 6 (depends on 5)

The method of claim 5, wherein modifying the environment comprises modifying at least one of a gas pressure, a gas flow rate and a temperature.

### Claim 7 (depends on 1)

The method of claim 1, further comprising applying a second coating over the top surface of the first coating.

### Claim 8 (depends on 7)

The method of claim 7, wherein the second coating is spin coated and spin dried on the planar top surface of the first coating.

### Claim 9

A method of forming a coating, comprising:
applying a first coating to a substrate having a plurality of topographical features, the first coating applied over the plurality of topographical features, the first coating substantially liquid during application;
planarizing a top surface of the first coating prior to drying the first coating; and
drying the coating without substantial spin-drying after planarizing the top surface of the first coating.

### Claim 10 (depends on 9)

The method of claim 9, wherein the drying the coating comprises drying the first coating through modifying an environment of the first coating.

### Claim 11 (depends on 9)

The method of claim 9, further comprising spinning the substrate at a first speed during application of the first coating and spinning the substrate at a second speed lower than the first speed during the planarizing the top surface of the first coating.

### Claim 12 (depends on 9)

The method of claim 9, further comprising applying a second coating over the top surface of the first coating.

### Claim 13 (depends on 12)

The method of claim 12, wherein the second coating is spin coated and spin dried on the planar top surface of the first coating.

### Claim 14

A system for applying a coating, comprising:
a coating chamber comprising:
a platen configured to hold a wafer; and
a coating nozzle configured to deliver a first coating to the wafer
wherein the coating chamber is configured to dry the first coating on the wafer with a substantially planar top surface and without substantial spin drying; and
wherein the platen is configured to spin the wafer at a first speed during delivery of the first coating to the wafer, the platen further configured to spin the wafer at a second speed during drying of the first coating.

### Claim 15 (depends on 14)

The system of claim 14, wherein the first coating is a conformal coating, the first coating conforming to topographical features on the wafer, wherein the coating chamber is configured to dry the conformal coating prior to drying the conformal coating and further configured to planarize the top surface of the conformal coating after drying the conformal coating.

### Claim 16 (depends on 15)

The system of claim 15, wherein the coating chamber is further configured to planarize the top surface of the first coating by applying a solvent to the conformal coating, the solvent reflowing the coating, and wherein the coating chamber is further configured to dry the reflowed first coating.

### Claim 17 (depends on 14)

The system of claim 14, wherein the platen is further configured to vibrate the wafer during application of the first coating and during drying of the first coating.

### Claim 18 (depends on 14)

The system of claim 14, wherein the coating chamber is configured to dry the first coating by controlling an environment contained in the coating chamber.

### Claim 19 (depends on 18)

The system of claim 18, wherein the coating chamber is configured to control the environment by modifying at least one of a gas pressure, a gas flow rate and a temperature.

### Claim 20 (depends on 14)

The system of claim 14, further comprising a thickness monitor configured to measure a thickness of the first coating, and wherein the coating chamber is configured to apply a second coating on the planar top surface of the first coating, the second coating having a thickness depending on at least the thickness of the first coating measured by the thickness monitor.