# US 2014/0273508 A1 · Wafer Back Side Processing Structure and Apparatus

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2014/0273508 A1
- Document ID: US20140273508A1
- Status: Published application
- Kind: A1
- Application number: 13/924,993
- Filed: 2013-06-24
- Published: 2014-09-18
- Earliest claimed: 2013-03-12
- Assignees: Taiwan Semiconductor Manufacturing Company, Ltd.
- Applicants: Taiwan Semiconductor Manufacturing Company, Ltd.
- Inventors: Cheng-Chien Li; Wei-Chih Lin; Song-Bor Lee; Ching-Kun Huang
- Web page: https://patentgrep.com/patent/US20140273508A1

## CPC

- H10P 14/6506: {Formation of intermediate materials}
- H10P 14/6548: {by forming intermediate materials, e.g. capping layers or diffusion barriers}
- H10P 95/064: {the removal being chemical etching}
- H10P 95/90: Thermal treatments, e.g. annealing or sintering
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

Disclosed herein is a method of processing a device, comprising providing a substrate having a buffer layer disposed on a back side and forming an outer protection layer over the back side of the buffer layer, forming a thermal layer on the back side of the outer protection layer and heating the substrate through the thermal layer and the back side of the outer protective layer. A back side protection layer may be formed on the back side of the buffer layer. The thermal layer has a thermal emissivity coefficient of about 0.7 or greater and a thickness greater than a roughness of the back side of the outer protection layer. The back side protection layer is an oxide with a thickness between about 20 angstroms and about 50 angstroms. The outer protection layer is a nitride with a thickness between about 50 angstroms and about 300 angstroms.

## Claims

### Claim 1

A method of forming a device, comprising:
providing a substrate having a front side and a back side, the substrate having a buffer layer disposed on the back side;
forming an outer protection layer over the buffer layer;
polishing the outer protection layer; and
heating the substrate through the outer protective layer after the polishing the outer protection layer.

### Claim 2 (depends on 1)

The method of claim 1, further comprising forming a back side protection layer on the buffer layer prior to the forming the outer protection layer.

### Claim 3 (depends on 2)

The method of claim 2, wherein the back side protection layer is an oxide.

### Claim 4 (depends on 3)

The method of claim 3, wherein the outer protection layer is a nitride.

### Claim 5 (depends on 4)

The method of claim 4, wherein the buffer layer is polysilicon.

### Claim 6 (depends on 5)

The method of claim 5, wherein the polishing the outer protection layer comprises reducing a roughness of the back side of the outer protection layer to have an RMS of about 20 angstroms or less.

### Claim 7

A method of forming a device, comprising:
providing a substrate having a front side and a back side, the substrate having a buffer layer disposed on the back side;
forming an outer protection layer over the buffer layer;
forming a thermal layer on the outer protection layer; and
heating the substrate through the thermal layer and the outer protective layer.

### Claim 8 (depends on 7)

The method of claim 7, further comprising forming a back side protection layer on the buffer layer prior to the forming the outer protection layer.

### Claim 9 (depends on 8)

The method of claim 8, wherein the thermal layer has a thermal emissivity coefficient of about 0.7 or greater.

### Claim 10 (depends on 9)

The method of claim 9, wherein the thermal layer has a thickness greater than a roughness of the back side of the outer protection layer.

### Claim 11 (depends on 10)

The method of claim 10, wherein the back side protection layer is an oxide.

### Claim 12 (depends on 11)

The method of claim 11, wherein the back side protection layer is formed with a thickness between about 20 angstroms and about 50 angstroms.

### Claim 13 (depends on 11)

The method of claim 11, wherein the outer protection layer is a nitride.

### Claim 14 (depends on 13)

The method of claim 13, wherein the outer protection layer is formed with a thickness between about 50 angstroms and about 300 angstroms.

### Claim 15

A method of forming a device, comprising:
providing a substrate having a front side and a back side;
forming a buffer layer on the back side of the substrate;
forming a backside protection layer over the buffer layer;
forming an outer protection layer over the backside protection layer;
forming a thermal layer on the outer protection layer; and
heating the substrate through the thermal layer.

### Claim 16 (depends on 15)

The method of claim 15, wherein the buffer layer is polysilicon having a thickness between about 500 angstroms and about 1000 angstroms.

### Claim 17 (depends on 15)

The method of claim 15, wherein the thermal layer has a thermal emissivity coefficient of about 0.7 or greater and wherein the thermal layer has a thickness greater than a roughness of the back side of the outer protection layer.

### Claim 18 (depends on 15)

The method of claim 15, the thermal layer is formed in contact with the outer protection layer.

### Claim 19 (depends on 15)

The method of claim 15, wherein the thermal layer is a polymer or polyimide.

### Claim 20 (depends on 15)

The method of claim 15, wherein the thermal layer is silicon carbide, sapphire or an alumina ceramic.