# US 2014/0273477 A1 · Si PRECURSORS FOR DEPOSITION OF SiN AT LOW TEMPERATURES

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2014/0273477 A1
- Document ID: US20140273477A1
- Status: Published application
- Kind: A1
- Application number: 14/167,904
- Filed: 2014-01-29
- Published: 2014-09-18
- Earliest claimed: 2013-03-14
- Assignees: ASM IP Holding B.V.
- Applicants: Asm IP Holding B.V.
- Inventors: Antti J. Niskanen; Shang Chen; Viljami Pore; Atsuki Fukazawa; Hideaki Fukuda; Suvi P. Haukka
- Web page: https://patentgrep.com/patent/US20140273477A1

## CPC

- H10P 14/69433: {the material being a silicon nitride not containing oxygen, e.g. SixNy or SixByNz}
- H10P 14/6336: {in the presence of a plasma [PECVD]}
- H10P 14/6339: {deposition by cyclic CVD, e.g. ALD, ALE or pulsed CVD}
- H10P 14/6682: {the compound being a silane, e.g. disilane, methylsilane or chlorosilane}
- H10D 84/0158: {the components including FinFETs}
- H10D 84/038: {using silicon technology, e.g. SiGe}
- H10P 50/283: {by chemical means}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

Methods and precursors for depositing silicon nitride films by atomic layer deposition (ALD) are provided. In some embodiments the silicon precursors comprise an iodine ligand. The silicon nitride films may have a relatively uniform etch rate for both vertical and the horizontal portions when deposited onto three-dimensional structures such as FinFETS or other types of multiple gate FETs. In some embodiments, various silicon nitride films of the present disclosure have an etch rate of less than half the thermal oxide removal rate with diluted HF (0.5%).

## Claims

### Claim 1

A method of depositing a silicon nitride thin film on a substrate in a reaction space comprising:
(a) introducing a vapor-phase silicon reactant into the reaction space so that the silicon precursor is adsorbed to a surface of the substrate;
(b) removing excess silicon reactant and reaction byproducts;
(c) contacting the adsorbed silicon reactant with a reactive species generated by a plasma from a nitrogen precursor;
(d) removing excess reactive species and reaction byproducts;
wherein steps (a) through (d) are repeated until a silicon nitride film of a desired thickness is formed;
wherein the silicon reactant comprises a precursor having a formula of
H2n+2−y−z−wSinIyAzRw
wherein, n=1-10, y=1 or more (and up to 2n+2−z−w), z=0 or more (and up to 2n+2−y−w), w=0 or more (and up to 2n+2−y−z), A is a halogen other than I, R is an organic ligand and can be independently selected from the group consisting of alkoxides, alkylsilyls, alkyl, substituted alkyl, alkylamines, and unsaturated hydrocarbon.

### Claim 2 (depends on 1)

The method of claim 1, wherein the reactive species comprises hydrogen, hydrogen atoms, hydrogen plasma, hydrogen radicals, N*, NH* or NH2* radicals.

### Claim 3 (depends on 1)

The method of claim 1, wherein the reaction space is part of a showerhead reactor and comprises a showerhead and a susceptor.

### Claim 4 (depends on 3)

The method of claim 3, wherein there is a gap of about 0.5 cm to about 5 cm between the showerhead and susceptor.

### Claim 5 (depends on 3)

The method of claim 3, wherein there is a gap of about 0.8 cm to about 3.0 cm between the showerhead and susceptor.

### Claim 6 (depends on 1)

The method of claim 1, wherein the reactive species are generated directly above the substrate.

### Claim 7 (depends on 1)

The method of claim 1, wherein the silicon reactant is H2SiI2.

### Claim 8 (depends on 1)

The method of claim 1, wherein the method is performed at a temperature between about 200° C. and about 400° C.

### Claim 9 (depends on 1)

The method of claim 1, wherein the nitrogen precursor is selected from the group consisting of NH3, N2H4, an N2/H2 mixture, N2, and any mixtures thereof.

### Claim 10 (depends on 1)

The method of claim 1, wherein the silicon nitride thin film exhibits a step coverage and pattern loading effect of at least about 80%

### Claim 11 (depends on 1)

The method of claim 1, wherein the silicon nitride thin film is formed on a three-dimensional structure.

### Claim 12 (depends on 11)

The method of claim 11, wherein the structure comprises a sidewall and top regions and the sidewall wet etch rate (WER) of the silicon nitride film relative to the top region WER is about 1 in 0.5% dHF.

### Claim 13 (depends on 1)

The method of claim 1, wherein an etch rate of the silicon nitride thin film is less than about 4 nm/min in 0.5% aqueous HF.

### Claim 14 (depends on 1)

The method of claim 1, wherein nitrogen is used as a carrier gas.

### Claim 15 (depends on 1)

The method of claim 1, wherein nitrogen is flowed continuously to the reaction space throughout steps (a)-(d).

### Claim 16 (depends on 1)

The method of claim 1, wherein the silicon reactant comprises a precursor having the following formula:
H2n+2−y−z−wSinXyAz(NR1R2)w
wherein, n=1-10, y=1 or more (and up to 2n+2−z−w), z=0 or more (and up to 2n+2−y−w), w=1 or more (and up to 2n+2−y−z), X is I or Br, A is a halogen other an X, N is nitrogen, R1 can be independently selected from the group consisting of hydrogen, alkyl, substituted alkyl, silyl, alkylsilyl, and unsaturated hydrocarbon, and R2 can be independently selected from the group consisting of alkyl, substituted alkyl, silyl, alkylsilyl, and unsaturated hydrocarbon.

### Claim 17 (depends on 16)

The method of claim 16, wherein the silicon reactant comprises a precursor having one of the following formulas: (SiI2H)NHMe, (SiI2H)NHEt, (SiI2H)NMe2, (SiI2H)NMeEt, (SiI2H)NEt2, (SiI2)(NHMe)2, (SiI2)(NHEt)2, (SiI2)(NMe2)2, (SiI2)(NMeEt)2, and (SiI2)(NEt2)2.

### Claim 18

An atomic layer deposition (ALD) method for forming a silicon nitride thin film, the method comprising a plurality of cycles, each cycle comprising alternately and sequentially contacting a substrate in a reaction space with a vapor phase pulse of a silicon reactant and a second reactant, wherein the silicon reactant comprises a precursor having the following formula:
H2n+2−y−wSinly(NR1R2)w
wherein, n=1-10, y=1 or more (and up to 2n+2−w), w=1 or more (and up to 2n+2−y), N is nitrogen, and R1 and R2 can be independently selected from the group consisting of hydrogen, alkyl, substituted alkyl, silyl, alkylsilyl, and unsaturated hydrocarbon.

### Claim 19 (depends on 18)

The method of claim 18, wherein the silicon reactant comprises a precursor having one of the following formulas: (SiI2H)NH2, (SiI2H)NHMe, (SiI2H)NHEt, (SiI2H)NMe2, (SiI2H)NMeEt, (SiI2H)NEt2, (SiI2)(NH2)2, (SiI2)(NHMe)2, (SiI2)(NHEt)2, (SiI2)(NMe2)2, (SiI2)(NMeEt)2, and (SiI2)(NEt2)2.

### Claim 20 (depends on 18)

The method of claim 18, wherein the second reactant comprises a nitrogen precursor.

### Claim 21 (depends on 20)

The method of claim 20, wherein the nitrogen precursor comprises reactive species from a nitrogen containing plasma.

### Claim 22 (depends on 20)

The method of claim 20, wherein the nitrogen precursor comprises nitrogen radicals, nitrogen atoms and/or nitrogen plasma.