# US 2014/0273434 A1 · Method of fabricating copper damascene

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2014/0273434 A1
- Document ID: US20140273434A1
- Status: Published application
- Kind: A1
- Application number: 13/834,448
- Filed: 2013-03-15
- Published: 2014-09-18
- Earliest claimed: 2013-03-12
- Assignees: Taiwan Semiconductor Manufacturing Company, Ltd.
- Applicants: Taiwan Semiconductor Manufacturing Company, Ltd.
- Inventors: Chao-Hsien Peng; Chi-Liang Kuo; Hsiang-Huan Lee; Shau-Lin Shue
- Web page: https://patentgrep.com/patent/US20140273434A1

## CPC

- H10W 20/057: {by selectively depositing, e.g. by using selective CVD or plating}
- H10W 20/032: {of conductive barrier, adhesion or liner layers}
- H10W 20/033: {in openings in dielectrics}
- H10W 20/044: {for electroless plating}
- H10W 20/0523: {by irradiating with ultraviolet or particle radiation}
- H10W 20/055: {by formation methods other than physical vapour deposition [PVD], chemical vapour deposition [CVD] or liquid deposition}
- H10W 20/0552: {by diffusing metallic dopants to react with dielectrics}
- H10W 20/056: {by filling conductive material into holes, grooves or trenches}
- H10W 20/074: {of dielectric parts comprising thin functional dielectric layers, e.g. dielectric etch-stop, barrier, capping or liner layers}
- H10W 20/076: {in via holes or trenches}
- H10W 20/094: {by transforming insulators into conductors}
- H10W 20/42: Vias, e.g. via plugs
- H10W 20/425: {Barrier, adhesion or liner layers}
- H10W 20/4424: {Copper alloys}
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

A method of fabricating a semiconductor device includes forming a non-conductive layer over a semiconductor substrate. A low-k dielectric layer is formed over the non-conductive layer. The low-k dielectric layer is etched and stopped at the non-conductive layer to form an opening. A plasma treatment is performed on the substrate to convert the non-conductive layer within the opening into a conductive layer. The opening is filled with a copper-containing material in an electroless copper bottom up fill process to form a copper-containing plug. The copper-containing plug is planarized so that the top of the copper-containing plug is co-planar with the top of the low-k dielectric layer. The substrate is heated to form a self-forming barrier layer on the sidewalls of the copper-containing plug.

## Claims

### Claim 1

A method of fabricating a semiconductor device, comprising:
forming a non-conductive layer over a semiconductor substrate;
forming a low-k dielectric layer over the non-conductive layer;
etching the low-k dielectric layer and stopping at the non-conductive layer to form an opening;
heating the substrate to convert the non-conductive layer within the opening into a conductive layer;
filling the opening with a copper-containing material to form a copper-containing plug;
planarizing the copper-containing plug so that a top of the copper-containing plug is co-planar with a top of the low-k dielectric layer; and
heating the substrate to form a self-forming barrier layer on sidewalls of the copper-containing plug.

### Claim 2 (depends on 1)

The method of claim 1, wherein the non-conductive layer includes a material selected from the group consisting of TaN, TaSiN, TaC, TiN, TiSiN, AlON, AlN, and AlO.

### Claim 3 (depends on 1)

The method of claim 1, wherein the non-conductive layer is formed over the substrate by CVD or ALD.

### Claim 4 (depends on 1)

The method of claim 1, wherein the opening is a dual damascene opening.

### Claim 5 (depends on 1)

The method of claim 1, wherein converting the non-conductive layer within the opening into a conductive layer comprises performing a plasma treatment on the substrate.

### Claim 6 (depends on 5)

The method of claim 5, wherein the plasma treatment is performed at a temperature ranging between about 20 Celsius and about 400 Celsius, at a pressure ranging between about 0.01 torr and about 100 torr at a power ranging between about 50 watts and about 500 watts, and a time of between 3 seconds and 30 seconds.

### Claim 7 (depends on 1)

The method of claim 1, wherein filling the opening with a copper-containing material comprises an electroless copper bottom up fill process.

### Claim 8 (depends on 5)

The method of claim 5, wherein the plasma treatment is performed with a gas selected from the group consisting of Ar, H2, He, Ne, and a combination thereof.

### Claim at position 9

9-15. (canceled)

### Claim 16

A method of fabricating a damascene layer, comprising:
forming a first non-conductive layer over a semiconductor substrate;
forming a first low-k dielectric layer over the first non-conductive layer;
forming a second non-conductive layer over the first low-k dielectric layer;
forming a second low-k dielectric layer over the second non-conductive layer;
etching the first low-k dielectric layer and stopping at the first non-conductive layer to form a first opening and etching the second low-k dielectric layer and stopping at the second non-conductive layer to form a second opening;
heating the substrate to convert the first non-conductive layer within the first opening into a first conductive layer and the second non-conductive layer within the second opening into a second conductive layer;
filling the first opening and the second opening with a copper-containing material to form a first copper-containing plug and a second copper-containing plug, respectively;
planarizing the first and second copper-containing plugs so that tops of the plugs are co-planar with a top of the second low-k dielectric layer; and
heating the substrate to form a self-forming barrier layer on sidewalls of the first and second copper-containing plugs.

### Claim 17 (depends on 16)

The method of claim 16, wherein the first and second non-conductive layers include a material selected from the group consisting of TaN, TaSiN, TaC, TiN, TiSiN, AlON, AlN, and AlO.

### Claim 18 (depends on 16)

The method of claim 16, wherein the first and second non-conductive layers are formed by CVD or ALD.

### Claim 19 (depends on 16)

The method of claim 16, wherein the step of heating the substrate to convert the first non-conductive layer within the first opening into a first conductive layer and the second non-conductive layer within the second opening into a second conductive layer includes performing a plasma treatment with a gas selected from the group consisting of Ar, H2, He, Ne, and a combination thereof.

### Claim 20 (depends on 19)

The method of claim 19, wherein the plasma treatment is performed at a temperature ranging between about 20 Celsius and about 400 Celsius, at a pressure ranging between about 0.01 torr and about 100 torr at a power ranging between about 50 watts and about 500 watts, and a time of between 3 seconds and 30 seconds.

### Claim 21

A method of fabricating a semiconductor device, comprising:
forming a first metallization layer over a semiconductor substrate;
forming a first non-conductive layer over the first metallization layer;
forming a first low-k dielectric layer over the non-conductive layer, a second non-conductive layer over the first low-k dielectric layer, and a second low-k dielectric layer over the second non-conductive layer;
etching a first opening, the first opening extending through the a second low-k dielectric layer, second non-conductive layer, and the first low-k dielectric layer, and exposing a portion of the first non-conductive layer;
etching a second opening, the second opening extending through the a second low-k dielectric layer and exposing a portion of the second non-conductive layer;
applying a heat treatment to convert the exposed portion of the first non-conductive layer to a first conductive portion and to convert the exposed portion of the second non-conductive layer to a second conductive portion;
filling the first opening with a conductive material and filling the second opening with conductive material; and
heating the device to form a self-forming barrier layer on sidewalls of the conductive material.

### Claim 22 (depends on 21)

The method of claim 21, wherein the conductive material includes an alloy of copper and an alloying metal and wherein the step of heating the device to form a self-forming barrier layer on sidewalls of the conductive material includes forming an oxide of the alloying metal on sidewalls of the conductive material.

### Claim 23 (depends on 21)

The method of claim 21, wherein the heat treatment is selected from the group consisting of a plasma treatment, an anneal, a pulsed energy beam, and combinations thereof.

### Claim 24 (depends on 21)

The method of claim 21, wherein the first non-conductive layer comprises a compound having a metallic component and a non-metallic component and wherein the step of applying a heat treatment converts the material from a first state in which the non-metallic component is greater than a stoichiometric level to a second state in which the metallic component is greater than the stoichiometric level.

### Claim 25 (depends on 24)

The method of claim 24, wherein the compound is selected from the group consisting of TaN, TaSiN, TaC, TiN, TiSiN, AlON, AlN, and AlO.

### Claim 26 (depends on 21)

The method of claim 21, wherein the conductive material includes a plug formed of copper and an alloying metal, and wherein the step of heating the device to form a self-forming barrier layer on sidewalls of the conductive material causes the alloying metal to segregate from the copper and migrate to surfaces of the plug.

### Claim 27 (depends on 26)

The method of claim 26, wherein the step of heating the device to form a self-forming barrier layer on sidewalls of the conductive material is performed in an oxygen containing environment, and wherein segregated alloying metal combines with oxygen in the oxygen containing environment.