# US 2014/0273414 A1 · Method for manufacturing graphene film and graphene channel of transistor

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2014/0273414 A1
- Document ID: US20140273414A1
- Status: Published application
- Kind: A1
- Application number: 14/028,760
- Filed: 2013-09-17
- Published: 2014-09-18
- Earliest claimed: 2013-03-13
- Assignees: Academia Sinica
- Applicants: Academia Sinica
- Inventors: SHIH-YEN LIN; MENG-YU LIN
- Web page: https://patentgrep.com/patent/US20140273414A1

## CPC

- H10P 14/3406: {Carbon, e.g. diamond-like carbon}
- H10D 30/01: Manufacture or treatment
- H10D 30/472: {having lower bandgap active layer formed on top of wider bandgap layer, e.g. inverted HEMT}
- H10D 62/8303: {Diamond}
- H10D 62/882: {Graphene}
- H10P 14/22: using physical deposition, e.g. vacuum deposition or sputtering
- H10P 14/2923: {being conductive materials, e.g. metallic silicides}
- H10P 14/38: {characterised by treatments done after the formation of the materials}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

The present invention provides a method for manufacturing a graphene film and a graphene channel of transistor. The graphene film is prepared at a low temperature by using molecular beam epitaxy technique, and the graphene channel is able to fit into a transistor. The excellent characteristic of current modulation within graphene transistors is observed.

## Claims

### Claim 1

A method for manufacturing a graphene film, comprising following steps:
(a) annealing a first substrate in a furnace filled with a mixed gas;
(b) moving the first substrate into a growing chamber of a molecular beam epitaxy system, wherein a temperature of the growing chamber is ranged from room temperature to 500° C.;
(c) heating a carbon source set in the molecular beam epitaxy system to evaporate carbon atoms onto a surface of the first substrate; and
(d) depositing the carbon atoms on the surface of the first substrate to grow the graphene film.

### Claim 2

A method for manufacturing a graphene channel within a transistor, comprising following steps:
(a) annealing a first substrate in a furnace filled with a mixed gas;
(b) moving the first substrate into a growing chamber of a molecular beam epitaxy system, wherein a temperature of the growing chamber is ranged from room temperature to 500° C.;
(c) heating a carbon source set in the molecular beam epitaxy system to evaporate carbon atoms onto a surface of the first substrate;
(d) depositing the carbon atoms on the surface of the first substrate to grow a graphene film;
(e) replacing the first substrate with a second substrate; and
(f) etching the graphene film by a photolithography process.

### Claim 3 (depends on 1)

The method of claim 1, wherein the mixed gas is H2/Ar.

### Claim 4 (depends on 1)

The method of claim 1, wherein the first substrate is a copper substrate.

### Claim 5 (depends on 1)

The method of claim 1, wherein the carbon source is heated to 2100-2200° C.

### Claim 6 (depends on 1)

The method of claim 1, wherein the carbon source is graphite.

### Claim 7 (depends on 2)

The method of claim 2, wherein the step (e) comprises following steps:
(e1) coating the graphene film on the side opposite to the first substrate with an organic polymer material, and heating the organic polymer material by a temperature of 150-200° C. to cure the organic polymer material;
(e2) removing the first substrate by a reagent to obtain the graphene film coated with the organic polymer material;
(e3) attaching the graphene film coated with the organic polymer material to the second substrate through a step of dredge up;
(e4) removing the organic polymer material to obtain the graphene film attached to the second substrate.

### Claim 8 (depends on 7)

The method of claim 7, wherein the organic polymer material is poly(methyl methacrylate).

### Claim 9 (depends on 7)

The method of claim 7, wherein the reagent is a ferric chloride solution.

### Claim 10 (depends on 7)

The method of claim 7, wherein the organic polymer material is removed by acetone.

### Claim 11 (depends on 2)

The method of claim 2, wherein the transistor is a back-gate transistor.

### Claim 12 (depends on 11)

The method of claim 11, wherein the second substrate is a Si substrate having a silicon dioxide layer.

### Claim 13 (depends on 12)

The method of claim 12, wherein the Si substrate is a p-type Si substrate having a boron doping concentration of 1×1015 cm−3.

### Claim 14 (depends on 2)

The method of claim 2, further comprising a following step:
(g) evaporating a metal to both terminals of the graphene film to form a source and a drain.

### Claim 15 (depends on 14)

The method of claim 14, wherein the metal is titanium or gold.

### Claim 16 (depends on 2)

The method of claim 2, wherein the mixed gas is H2/Ar.

### Claim 17 (depends on 2)

The method of claim 2, wherein the first substrate is a copper substrate.

### Claim 18 (depends on 2)

The method of claim 2, wherein the carbon source is heated to 2100-2200° C.

### Claim 19 (depends on 2)

The method of claim 2, wherein the carbon source is graphite.