# US 2014/0272703 A1 · Triboelectric charge control of toner through monomer ratio of shell latex

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2014/0272703 A1
- Document ID: US20140272703A1
- Status: Published application
- Kind: A1
- Application number: 13/840,877
- Filed: 2013-03-15
- Published: 2014-09-18
- Earliest claimed: 2013-03-15
- Assignees: Xerox Corporation
- Applicants: Xerox Corporation
- Inventors: Padam K. ANGRA; Christopher M. WOLFE
- Web page: https://patentgrep.com/patent/US20140272703A1

## CPC

- G03G 9/09392: {Preparation thereof}
- G03G 9/09321: {obtained by reactions only involving carbon-to-carbon unsaturated bonds}
- G03G: ELECTROGRAPHY; ELECTROPHOTOGRAPHY; MAGNETOGRAPHY

## Abstract

Core/shell toner particles are made to have a desired triboelectric charge through control of the glass transition temperature (Tg) of the shell polymer and/or the ratio of styrene and at least one monomer for forming the polymer of the shell. The polymer is introduced onto core particles to form a shell thereon via an aggregation process.

## Claims

### Claim 1

A method for preparing toner particles having a desired triboelectric charge, comprising:
selecting a triboelectric charge for the toner particles, the toner particles comprising a core and a shell;
selecting a styrene and at least one monomer selected from the group consisting of acrylates, butadienes, and methacrylates;
obtaining a ratio of the styrene to the at least one monomer for forming a polymer, the polymer forming the shell, the ratio corresponding to the selected triboelectric charge;
preparing a shell latex comprising the polymer derived from the styrene and the at least one monomer having the obtained ratio;
introducing the shell latex to core particles; and
aggregating to form toner particles having the shell comprised of the polymer on the core particles, and having the selected triboelectric charge.

### Claim 2 (depends on 1)

The method of claim 1, wherein the core comprises a binder and a colorant.

### Claim 3 (depends on 2)

The method of claim 2, wherein the colorant comprises a carbon black pigment.

### Claim 4 (depends on 1)

The method of claim 1, further comprising:
determining a jacket temperature for introducing the shell latex to the core particles based on the obtained ratio of the styrene to the at least one monomer.

### Claim 5 (depends on 1)

The method of claim 1, wherein the core further comprises a wax.

### Claim 6 (depends on 1)

The method of claim 1, wherein the at least one monomer comprises butyl acrylate.

### Claim 7 (depends on 1)

The method of claim 1, wherein the ratio of the styrene to the at least one monomer is obtained from stored data regarding the relationship between triboelectric charge and the ratio for the selected styrene and the at least one monomer.

### Claim 8 (depends on 1)

The method of claim 1, wherein the triboelectric charge of the toner particles is from −15 microcoulombs/gram to −80 microcoulombs/gram.

### Claim 9

A method for preparing aggregated toner particles having a desired triboelectric charge, comprising:
predetermining a triboelectric charge for the aggregated toner particles based upon an application of the aggregated toner particles, the toner particles comprising a core and a shell;
selecting a styrene and at least one monomer selected from the group consisting of acrylates, butadienes, and methacrylates for forming the shell;
determining a necessary glass transition temperature value for a polymer derived from the selected styrene and the at least one monomer based upon the predetermined triboelectric charge;
obtaining from predetermined information a ratio of the styrene to the at least one monomer necessary to form the polymer having the determined glass transition temperature value;
preparing a shell latex comprising the polymer derived from the selected styrene and the at least one monomer having the obtained ratio;
introducing the shell latex to aggregated core particles; and
aggregating to form toner particles having the shell comprised of the polymer on the aggregated core particles, the toner particles having the predetermined triboelectric charge.

### Claim 10 (depends on 9)

The method of claim 9, wherein the ratio of the styrene to the at least one monomer is obtained from stored data regarding the relationship between triboelectric charge and the ratio for the selected styrene and the at least one monomer.

### Claim 11 (depends on 9)

The method of claim 9, wherein the triboelectric charge of the aggregated toner particles is related to the glass transition temperature of the shell.

### Claim 12 (depends on 9)

The method of claim 9, wherein the ratio of the styrene to the at least one monomer is obtained by correlating the determined glass transition temperature value to the predetermined triboelectric charge from stored data, and subsequently obtaining the ratio of the styrene to the at least one monomer from stored data regarding the relationship between the glass transition temperature value and the ratio of the styrene to the at least one monomer for the selected styrene and the at least one monomer.

### Claim 13 (depends on 9)

The method of claim 9, wherein the shell polymer is selected from the group consisting of poly(styrene-alkyl acrylate), poly(styrene-1,3-diene), poly(styrene-alkyl methacrylate), poly(styrene-alkyl acrylate-acrylic acid), poly(styrene-1,3-diene-acrylic acid), poly(styrene-alkyl methacrylate-acrylic acid), poly(styrene-alkyl acrylate-acrylonitrile-acrylic acid), poly(styrene-1,3-diene-acrylonitrile-acrylic acid), poly(styrene-butadiene), poly(methylstyrene-butadiene), poly(styrene-isoprene), poly(methylstyrene-isoprene), poly(styrene-propyl acrylate), poly(styrene-butyl acrylate), poly(styrene-butadiene-acrylic acid), poly(styrene-butadiene-methacrylic acid), poly(styrene-butadiene-acrylonitrile-acrylic acid), poly(styrene-butyl acrylate-acrylic acid), poly(styrene-butyl acrylate-methacrylic acid), poly(styrene-butyl acrylate-acrylononitrile), poly(styrene-butyl acrylate-acrylonitrile-acrylic acid), poly(styrene-butadiene), poly(styrene-isoprene), poly(styrene-butyl methacrylate), poly(styrene-butyl acrylate-acrylic acid), poly(styrene-butyl methacrylate-acrylic acid), and combinations thereof.

### Claim 14 (depends on 9)

The method of claim 9, further comprising:
determining a jacket temperature for introducing the shell latex to aggregated core particles based on the obtained ratio of the styrene to the at least one monomer.

### Claim 15 (depends on 8)

The method of claim 8, wherein the at least one monomer comprises butyl acrylate.

### Claim 16 (depends on 9)

The method of claim 9, wherein the core comprises binder and a colorant.

### Claim 17 (depends on 16)

The method of claim 16, wherein the colorant comprises carbon black pigment.

### Claim 18 (depends on 9)

The method of claim 9, wherein the core further comprises a wax.

### Claim 19 (depends on 9)

The method of claim 9, wherein the triboelectric charge of the toner particles is from −15 microcoulombs/gram to −80 microcoulombs/gram.

### Claim 20 (depends on 9)

The method of claim 9, wherein the glass transition temperature value is from 30° C. to 80° C.

### Claim 21

A method of aggregating toner particles, comprising:
predetermining a triboelectric charge based upon an application of toner particles, the toner particles comprising a core and a shell;
selecting a styrene and at least one monomer selected from the group consisting of acrylates, butadienes, and methacrylates for forming the shell;
obtaining from predetermined information a ratio of the styrene to the at least one monomer necessary to achieve the toner particles having the predetermined triboelectric charge, the styrene and the at least one monomer forming a polymer;
aggregating a mixture comprising a binder resin and a colorant to form the cores of the toner particles;
adding a latex comprising the polymer derived from the styrene and the at least one monomer having the obtained ratio to the cores to form the shell over the cores and thereby obtain aggregated toner particles;
coalescing the aggregated toner particles; and
recovering the aggregated toner particles, wherein the toner particles have the predetermined triboelectric charge.

### Claim 22 (depends on 21)

The method of claim 21, wherein the shell polymer is selected from the group consisting of poly(styrene-alkyl acrylate), poly(styrene-1,3-diene), poly(styrene-alkyl methacrylate), poly(styrene-alkyl acrylate-acrylic acid), poly(styrene-1,3-diene-acrylic acid), poly(styrene-alkyl methacrylate-acrylic acid), poly(styrene-alkyl acrylate-acrylonitrile-acrylic acid), poly(styrene-1,3-diene-acrylonitrile-acrylic acid), poly(styrene-butadiene), poly(methylstyrene-butadiene), poly(styrene-isoprene), poly(methylstyrene-isoprene), poly(styrene-propyl acrylate), poly(styrene-butyl acrylate), poly(styrene-butadiene-acrylic acid), poly(styrene-butadiene-methacrylic acid), poly(styrene-butadiene-acrylonitrile-acrylic acid), poly(styrene-butyl acrylate-acrylic acid), poly(styrene-butyl acrylate-methacrylic acid), poly(styrene-butyl acrylate-acrylononitrile), poly(styrene-butyl acrylate-acrylonitrile-acrylic acid), poly(styrene-butadiene), poly(styrene-isoprene), poly(styrene-butyl methacrylate), poly(styrene-butyl acrylate-acrylic acid), poly(styrene-butyl methacrylate-acrylic acid), and combinations thereof.

### Claim 23 (depends on 21)

The method of claim 21, wherein the ratio of the styrene to the at least one monomer is obtained from stored data regarding the relationship between triboelectric charge and the ratio for the selected styrene and the at least one monomer.