# US 2014/0272642 A1 · Catalysts for hydrocarbon reforming

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2014/0272642 A1
- Document ID: US20140272642A1
- Status: Published application
- Kind: A1
- Application number: 13/837,544
- Filed: 2013-03-15
- Published: 2014-09-18
- Earliest claimed: 2013-03-15
- Assignees: LG Fuel Cell Systems Inc.
- Applicants: LG Fuel Cell Systems, Inc.
- Inventors: John R. Budge
- Web page: https://patentgrep.com/patent/US20140272642A1

## CPC

- C01B 3/40: characterised by the catalyst
- B01J 23/40: of the platinum group metals
- B01J 23/464: {Rhodium}
- B01J 23/74: Iron group metals
- B01J 37/20: Sulfiding
- C01B 3/38: using catalysts
- H01M 8/0618: {Reforming processes, e.g. autothermal, partial oxidation or steam reforming}
- B01J 23/96: of catalysts comprising metals, oxides or hydroxides of the noble metals
- C01B 2203/0233: the reforming step being a steam reforming step
- C01B 2203/0238: the reforming step being a carbon dioxide reforming step
- C01B 2203/0244: the reforming step being an autothermal reforming step, e.g. secondary reforming processes
- C01B 2203/066: with fuel cells
- C01B 2203/1052: Nickel or cobalt catalysts
- C01B 2203/1235: Hydrocarbons
- C01B 2203/1258: Pre-treatment of the feed
- H01M 2008/1293: {Fuel cells with solid oxide electrolytes}
- Y02E 60/50: Fuel cells
- Y02P 20/141: Feedstock
- Y02P 20/52: using catalysts, e.g. selective catalysts
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

In some examples, a method for treating a reforming catalyst, the method comprising heating a catalyst metal used for reforming hydrocarbon in a reducing gas mixture environment. The reducing gas mixture comprises hydrogen and at least one sulfur-containing compound. The at least one sulfur-containing compound includes one or more of hydrogen sulfide, carbonyl sulfide, carbonyl disulfide and organic sulfur-containing compounds such as thiophenes, thiophanes, sulfides (RSH), disulfides (RS2R′), tri-sulfides (RS3R′) and mercaptans (RSR′).

## Claims

### Claim 1

A method for treating a reforming catalyst, the method comprising heating a catalyst metal used for reforming hydrocarbon in a reducing gas mixture environment, wherein the reducing gas mixture comprises hydrogen and at least one sulfur-containing compound, wherein the at least one sulfur-containing compound includes one or more of hydrogen sulfide, carbonyl sulfide, carbonyl disulfide and organic sulfur-containing compounds such as thiophenes, thiophanes, sulfides (RSH), disulfides (RS2R′), tri-sulfides (RS3R′) and mercaptans (RSR′).

### Claim 2 (depends on 1)

The method of claim 1, wherein the catalyst metal is treated with a dose of sulfur during treatment such that catalyst performance is stabilized without substantially negatively impacting activity of the catalyst metal.

### Claim 3 (depends on 1)

The method of claim 1, wherein the heating the catalyst metal comprises heating the catalyst metal to a temperature between approximately 350 to 1,200 degrees Celsius.

### Claim 4 (depends on 1)

The method of claim 1, further comprising reforming hydrocarbons via a reformer with the catalyst metal to produce hydrogen.

### Claim 5 (depends on 4)

The method of claim 4, wherein reforming hydrocarbons comprises steam reforming.

### Claim 6 (depends on 4)

The method of claim 4, further comprising supplying the hydrogen to the fuel side of a solid oxide fuel cell stack.

### Claim 7 (depends on 4)

The method of claim 4, wherein the at least one sulfur compound is periodically added to a feed stream of the reformer while reforming the hydrocarbons.

### Claim 8 (depends on 7)

The method of claim 7, wherein a frequency, amount, and duration of the periodic addition of the sulfur compounds is selected such that catalyst performance is stabilized without substantially negatively impacting activity of the catalyst metal.

### Claim 9 (depends on 1)

The method of claim 1, wherein the catalyst metal is supported by a catalyst carrier.

### Claim 10 (depends on 1)

The method of claim 1, wherein the catalyst metal comprises one or more of Ni, Co, Rh, Ru, Pd, Pt and Co.

### Claim 11

An article for reforming hydrocarbons, the article comprising a catalyst metal for reforming hydrocarbons, wherein the catalyst metal has been treated by heating the in a reducing gas mixture environment, wherein the reducing gas mixture comprises hydrogen and at least one sulfur-containing compound, wherein the at least one sulfur-containing compound includes one or more of hydrogen sulfide, carbonyl sulfide, carbonyl disulfide and organic sulfur-containing compounds such as thiophenes, thiophanes, sulfides (RSH), disulfides (RS2R′), tri-sulfides (RS3R′) and mercaptans (RSR′).

### Claim 12 (depends on 11)

The article of claim 11, wherein the catalyst metal has been treated with a dose of sulfur during treatment such that catalyst performance is stabilized without substantially negatively impacting activity of the catalyst metal.

### Claim 13 (depends on 11)

The article of claim 11, wherein, during treatment, the catalyst metal is heated to a temperature between approximately 350 to 1,200 degrees Celsius.

### Claim 14 (depends on 11)

The article of claim 11, further comprising a reformer for reforming hydrocarbons, wherein the treated catalyst metal is used by the reformer to produce hydrogen.

### Claim 15 (depends on 14)

The article of claim 14, wherein reformer comprises a steam reformer.

### Claim 16 (depends on 14)

The article of claim 14, further comprising a solid oxide fuel cell stack, wherein the hydrogen produced by the reformer is supplied to the fuel side of the solid oxide fuel cell stack.

### Claim 17 (depends on 14)

The article of claim 14, wherein the at least one sulfur compound is periodically added to a feed stream of the reformer while reforming the hydrocarbons.

### Claim 18 (depends on 17)

The article of claim 17, wherein a frequency, amount, and duration of the periodic addition of the sulfur compounds is selected such that catalyst performance is stabilized without substantially negatively impacting activity of the catalyst metal.

### Claim 19 (depends on 11)

The article of claim 11, wherein the catalyst metal is supported by a catalyst carrier.

### Claim 20 (depends on 11)

The article of claim 11, wherein the catalyst metal comprises one or more of Ni, Co, Rh, Ru, Pd, Pt and Co.