Back to results
US 2014/0272552 A1Published application
Nonaqueous electrolyte battery
AssigneeKabushiki Kaisha Toshiba
InventorsMasanori TANAKA, Hidesato Saruwatari, Kazuya Kuriyama
Life of this patent
Estimating the term…
Abstract
In general, according to one embodiment, there is provided a nonaqueous electrolyte battery. The nonaqueous electrolyte battery includes an electrode group containing a positive electrode and a negative electrode, and a nonaqueous electrolyte held in the electrode group. The nonaqueous electrolyte battery satisfies the following relation (1): −0.07≦(DA−DC)×S/B≦0.05.
Claims4
A nonaqueous electrolyte battery comprising:
- an electrode group comprising a positive electrode comprising a positive electrode layer comprising nickel in a quantity of 12 wt % or more but 34 wt % or less and a negative electrode comprising a negative electrode layer comprising titanium in a quantity of 39 wt % or more but 51 wt % or less and a portion of which is opposed to the positive electrode layer;
- and
- a nonaqueous electrolyte held by the electrode group,
- wherein a following relation (1) is satisfied:
- −0.07≦(DA−DC)×S/B≦0.05 (1)
- wherein the B [Ah] is a discharge capacity of the nonaqueous electrolyte battery, the B being obtained by charging the nonaqueous electrolyte battery up to a maximum usage voltage with a constant current at a rate of 0.05 C and at 25° C., and then charging the nonaqueous electrolyte battery with a constant voltage until a current value becomes 0.01 C, and then discharging the nonaqueous electrolyte battery up to a final discharge voltage at a rate of 0.05 C;
- the S [cm2] is an area of the portion of the negative electrode layer opposed to the positive electrode layer;
- the DC [mAh/cm2] is a discharge capacity of the positive electrode, the DC being obtained by discharging the positive electrode from a fully charged state up to 3.0 V (vs. Li/Li+) at 25° C. and at a rate of 0.05 C;
- and
- the DA [mAh/cm2] is a discharge capacity of the negative electrode, the DA being obtained by discharging the negative electrode from a fully charged state up to 2.0 V (vs. Li/Li+) at 25° C. and at a rate of 0.05 C.
7 more elements